# US 2021/0304908 A1 · Method for process for producing fully ceramic microencapsulated fuels containing tristructural-isotropic particles with a coating layer having higher shrinkage than matrix

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0304908 A1
- Document ID: US20210304908A1
- Status: Published application
- Kind: A1
- Application number: 17/216,678
- Filed: 2021-03-30
- Published: 2021-09-30
- Earliest claimed: 2015-08-07
- Assignees: University of Seoul Industry Cooperation Foundation; Kepco Nuclear Fuel Co., Ltd.
- Applicants: University of Seoul Industry Cooperation Foundation; Kepco Nuclear Fuel Co., Ltd.
- Inventors: Young Wook KIM; Jung Hye EOM; Yu Kwang SEO; Seung Jae LEE
- Web page: https://patentgrep.com/patent/US20210304908A1

## CPC

- G21C 3/626: {Coated fuel particles}
- C04B 35/565: based on silicon carbide
- C04B 35/6261: {Milling}
- C04B 35/62655: {Drying, e.g. freeze-drying, spray-drying, microwave or supercritical drying}
- C04B 35/62886: {by wet chemical techniques}
- C04B 35/62894: {with more than one coating layer}
- C04B 35/632: Organic additives
- C04B 35/63472: {Condensation polymers of aldehydes or ketones}
- C04B 35/645: Pressure sintering
- C04B 38/0022: {obtained by a chemical conversion or reaction other than those relating to the setting or hardening of cement-like material or to the formation of a sol or a gel, e.g. by carbonising or pyrolysing preformed cellular materials based on polymers, organo-metallic or organo-silicon precursors}
- G21C 3/20: with coating on fuel or on inside of casing; with non-active interlayer between casing and active material {with multiple casings or multiple active layers}
- G21C 3/62: Ceramic fuel
- G21C 21/04: by vibrational compaction or tamping {of fuel in the jacket}
- C04B 35/62834: {Silicon carbide}
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3826: Silicon carbides
- C04B 2235/383: Alpha silicon carbide
- C04B 2235/3834: Beta silicon carbide
- C04B 2235/48: Organic compounds becoming part of a ceramic after heat treatment, e.g. carbonising phenol resins
- C04B 2235/483: Si-containing organic compounds, e.g. silicone resins, (poly)silanes, (poly)siloxanes or (poly)silazanes
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/604: Pressing at temperatures other than sintering temperatures
- C04B 2235/6562: Heating rate
- C04B 2235/6567: Treatment time
- C04B 2235/658: Atmosphere during thermal treatment
- C04B 2235/668: Pressureless sintering
- C04B 2235/77: Density
- Y02E 30/30: Nuclear fission reactors
- G21C: NUCLEAR REACTORS (fusion reactors, hybrid fission-fusion reactors G21B; nuclear explosives G21J)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to a method for preparing a fully ceramic capsulated nuclear fuel material containing three-layer-structured isotropic nuclear fuel particles coated with a ceramic having a composition which has a higher shrinkage than a matrix in order to prevent cracking of ceramic nuclear fuel, wherein the three-layer-structured nuclear fuel particles before coating is included in the range of between 5 and 40 fractions by volume based on after sintering. More specifically, the present invention provides a composition for preparing a fully ceramic capsulated nuclear fuel containing three-layer-structured isotropic particles coated with the substance which includes, as a main ingredient, a silicon carbine derived from a precursor of the silicon carbide wherein a condition of ΔLc>ΔLm at normal pressure sintering is created, where the sintering shrinkage of the coating layer of the three-layer-structured isotropic nuclear fuel particles is ΔLc and the sintering shrinkage of the silicon carbide matrix is ΔLm; material produced therefrom; and a method for manufacturing the material. The residual porosity of the fully ceramic capsulated nuclear fuel material is 4% or less.

## Claims

### Claim 1

A method for preparing a fully ceramic capsulated nuclear fuel material including three-layer-structured isotropic nuclear fuel particles with a coating layer having a shrinkage higher than a matrix phase, comprising:
(i) preparing a first mixture of a coating layer composition including a silicon carbide precursor;
(ii) coating the three-layer-structured isotropic nuclear fuel particles by using the first mixture;
(iii) preparing a second mixture of a silicon carbide matrix phase;
(iv) preparing a third mixture by mixing the three-layer-structured isotropic nuclear fuel particles having a coating layer including the silicon carbide precursor with the second mixture of the silicon carbide matrix phase;
(v) preparing a shaped body by using the third mixture;
(vi) preparing a partially sintered material by performing thermal decomposition of the silicon carbide precursor within the shaped body; and
(vii) performing normal pressure sintering of the pre-sintered body processed with thermal decomposition,
wherein, when shrinkage of the coating layer of the three-layer-structured isotropic nuclear fuel particles during a sintering process is given as ΔLc, and when the shrinkage of the silicon carbide matrix phase during the sintering process is given as ΔLm, a condition of ΔLc>ΔLm is satisfied when performing normal pressure sintering.

### Claim 2 (depends on 1)

The method of claim 1, wherein a sintering temperature range during the normal pressure sintering is 1700˜1800° C.

### Claim 3 (depends on 2)

The method of claim 2, wherein a holding time at a maximum temperature during the normal pressure sintering process corresponds to 0.5˜4 hours, and wherein the sintering atmosphere corresponds to argon.

### Claim 4 (depends on 1)

The method of claim 1, wherein, in the step of preparing a partially sintered material, the preparation is carried out at a heating speed within a range of 0.1° C./min˜1° C./min in order to control cracking in the shaped body caused by a discharge of gas, the discharged gas being a by-product of the thermal decompression of the silicon carbide precursor.

### Claim 5 (depends on 1)

The method of claim 1, wherein, in the step of preparing a partially sintered material, the atmosphere consists of ambient air starting from ambient temperature to 200° C. for cross-linking of the silicon carbide precursor, and wherein the atmosphere consists of argon gas starting from 200° C. to a temperature range of 800˜1400° C. in order to prevent oxidation of silicon carbide.