# US 2021/0289636 A1 · Apparatus and method relating to electrochemical migration

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0289636 A1
- Document ID: US20210289636A1
- Status: Published application
- Kind: A1
- Application number: 16/336,670
- Filed: 2017-10-23
- Published: 2021-09-16
- Earliest claimed: 2016-10-24
- Assignees: Jaguar Land Rover Limited
- Applicants: Jaguar Land Rover Limited
- Inventors: Thomas LIEDTKE
- Web page: https://patentgrep.com/patent/US20210289636A1

## CPC

- H05K 3/244: {Finish plating of conductors, especially of copper conductors, e.g. for pads or lands (selective plating methods H05K3/243; finish plating of conductors made by printing techniques H05K3/246; solder as finish H05K3/3465)}
- H05K 3/3473: Plating of solder
- B23K 35/262: {Sn as the principal constituent}
- B23K 35/302: {Cu as the principal constituent}
- G01R 31/2817: {Environmental-, stress-, or burn-in tests (of IC's G01R31/2855; of individual semiconductors G01R31/2642; of other circuits G01R31/2849)}
- H05K 1/09: Use of materials for the {conductive, e.g. } metallic pattern
- H05K 3/346: Solder materials or compositions specially adapted therefor
- H05K 2201/0305: Solder used for other purposes than connections between PCB or components, e.g. for filling vias or for programmable patterns
- H05K 2201/0338: Layered conductor, e.g. layered metal substrate, layered finish layer or layered thin film adhesion layer
- H05K 2201/0769: Anti metal-migration, e.g. avoiding tin whisker growth
- H05K 2203/1105: Heating or thermal processing not related to soldering, firing, curing or laminating, e.g. for shaping the substrate or during finish plating
- H05K 2203/162: Testing a finished product, e.g. heat cycle testing of solder joints
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- G01R: MEASURING ELECTRIC VARIABLES; MEASURING MAGNETIC VARIABLES (indicating correct tuning of resonant circuits H03J3/12)

## Abstract

Embodiments of the present invention provide a method (1000) of assembling an electrical circuit comprising one or more copper electrical conductors, the method comprising plating (1010) a surface of the one or more conductors with a layer comprising tin; annealing the plating; applying (1020) solder to at least a portion of the one or more electrical conductors, wherein said solder comprises tin and copper; and annealing the electrical circuit.

## Claims

### Claim at position 1

1-65. (canceled)

### Claim 66

A method of assembling an electrical circuit comprising one or more copper electrical conductors, the method comprising:
plating a surface of the one or more conductors with a layer comprising tin;
applying solder to at least a portion of the one or more electrical conductors, wherein said solder comprises tin and copper; and
annealing the electrical circuit having the solder applied to the at least a portion of the one or more electrical conductors at a temperature of up to around 150° C.

### Claim 67 (depends on 66)

The method of claim 66, wherein the annealing of the electrical circuit having the solder applied has a duration of between 45 minutes and 1.5 hours.

### Claim 68 (depends on 66)

The method of claim 66, comprising allowing the electrical circuit to cool following the annealing in an atmosphere at a temperature within a range of 10 to 40° C.

### Claim 69 (depends on 66)

The method of claim 66, comprising cooling the electrical circuit following the annealing at a rate within a range of 1.8° C./minute to 3° C./minute.

### Claim 70 (depends on 66)

The method of claim 66, wherein the solder comprises copper in a range from 0.5 wt % to 1 wt %.

### Claim 71 (depends on 66)

The method of claim 66, wherein the solder is at least 95 wt % tin.

### Claim 72 (depends on 66)

The method of claim 66, comprising applying a rosin-based flux to the electrical circuit.

### Claim 73 (depends on 72)

The method of claim 72, wherein a reflow temperature of the flux corresponds to the temperature of the annealing.

### Claim 74

An electrical circuit, comprising:
one or more copper electrical conductors having a tin plating; and
solder comprising tin and copper applied to at least a portion of the one or more electrical conductors and annealed at a temperature of up to around 150° C.

### Claim 75 (depends on 74)

The electrical circuit of claim 74, wherein the solder comprises copper in a range from 0.5 wt % to 1 wt %.

### Claim 76 (depends on 75)

The electrical circuit of claim 75, wherein the solder comprises around 0.7 wt % copper.

### Claim 77 (depends on 74)

The electrical circuit of claim 74, wherein the solder comprises nickel in a range of 0.1 to 0.05 wt %.

### Claim 78 (depends on 74)

The electrical circuit of claim 74, wherein the solder is at least 95 wt % tin.

### Claim 79 (depends on 74)

The electrical circuit of claim 74, wherein the solder is substantially free of silver.

### Claim 80 (depends on 74)

The electrical circuit of claim 74, wherein the solder comprises Germanium.

### Claim 81 (depends on 74)

The electrical circuit of claim 74, wherein the tin plating has a thickness of less than or equal to 5 μm.

### Claim 82 (depends on 81)

The electrical circuit of claim 81, wherein the tin plating thickness is less than or equal to 2 μm.

### Claim 83 (depends on 81)

The electrical circuit of claim 81, wherein the tin plating thickness is around 1 μm.

### Claim 84 (depends on 74)

The electrical circuit of claim 74, wherein the one or more copper conductors are without a conformal coating.

### Claim 85 (depends on 74)

A vehicle comprising the electrical circuit of claim 74.