# US 2021/0288352 A1 · Li/garnet electrolyte interface with low interfacial resistance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0288352 A1
- Document ID: US20210288352A1
- Status: Published application
- Kind: A1
- Application number: 17/196,355
- Filed: 2021-03-09
- Published: 2021-09-16
- Earliest claimed: 2020-03-10
- Assignees: Corning Incorporated; Shanghai Institute of Ceramics, Chinese Academy of Sciences
- Applicants: Corning Incorporated; Shanghai Institute of Ceramics, Chinese Academy of Sciences
- Inventors: Michael Edward Badding; Jun Jin; Zhen Song; Jianmeng Su; Zhaoyin Wen; Tongping Xiu
- Web page: https://patentgrep.com/patent/US20210288352A1

## CPC

- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/366: {as layered products}
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/052: Li-accumulators
- H01M 10/0562: Solid materials
- H01M 2004/027: {Negative electrodes}
- H01M 2300/0071: Oxides
- H01M 2300/0094: in the form of layered products, e.g. coatings
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A lithium-metal battery, includes: a substrate; a cathode disposed on the substrate; a garnet solid-state electrolyte disposed on the cathode; and a lithium anode disposed on the garnet solid-state electrolyte, such that a discoloration layer is disposed at an interface of the lithium anode and garnet solid-state electrolyte, the discoloration layer includes: a first portion; and a second portion, such that the first portion has a lithium component and the second portion has a garnet component. A method of forming a lithium-metal battery, includes: stacking a garnet source with at least one lithium source; and heating the stack at a temperature of at least 300° C. for a time in a range of 1 sec to 20 min to form a discoloration layer, such that the discoloration layer is disposed at an interface of the garnet source and the lithium source.

## Claims

### Claim 1

A lithium-metal battery, comprising:
a substrate;
a cathode disposed on the substrate;
a garnet solid-state electrolyte disposed on the cathode; and
a lithium anode disposed on the garnet solid-state electrolyte,
wherein a discoloration layer is disposed at an interface of the lithium anode and garnet solid-state electrolyte, the discoloration layer comprising:
a first portion; and
a second portion,
wherein the first portion including a lithium component and the second portion including a garnet component.

### Claim 2 (depends on 1)

The battery of claim 1, wherein an interfacial resistance at the interface is less than 1 Ω·cm2.

### Claim 3 (depends on 1)

The battery of claim 1, wherein a thickness of the discoloration layer is 1 nm to 50 nm.

### Claim 4 (depends on 1)

The battery on claim 1, further comprising:
a modification coating layer disposed between the garnet solid-state electrolyte and the lithium anode.

### Claim 5 (depends on 4)

The battery of claim 4, wherein the modification coating layer comprises at least one of: Au, Ag, Al, Si, C, Zn, Mg, Sn, Ti, B, Pb, Ge, or combinations thereof; and has a thickness of 1 nm to 50 nm.

### Claim 6 (depends on 1)

The battery of claim 1, wherein the first portion is positioned (A) in pores of the second portion; (B) atop a surface of the second portion; or (C) a combination thereof.

### Claim 7

A method of forming a lithium-metal battery, comprising:
stacking a garnet source with at least one lithium source; and
heating the stack at a temperature of at least 300° C. for a time in a range of 1 sec to 20 min to form a discoloration layer,
wherein the discoloration layer is disposed at an interface of the garnet source and the lithium source.

### Claim 8 (depends on 7)

The method of claim 7, wherein the heating is conducted at a temperature of at least 320° C.

### Claim 9 (depends on 7)

The method of claim 7, further comprising:
prior to stacking the garnet source with the at least one lithium source, sputtering the garnet source with a modification coating source.

### Claim 10 (depends on 9)

The method of claim 9, wherein the modification coating layer comprises at least one of: Au, Ag, Al, Si, C, Zn, Mg, Sn, Ti, B, Pb, Ge, or combinations thereof

### Claim 11 (depends on 9)

The method of claim 9, wherein:
a thickness of the discoloration layer is 1 nm to 50 nm; and
a thickness of the modification coating layer is 1 nm to 50 nm.

### Claim 12 (depends on 7)

The method of claim 7, the discoloration layer comprises:
a first portion; and
a second portion,
wherein the first portion includes a lithium component and the second portion includes a garnet component.

### Claim 13 (depends on 12)

The method of claim 12, wherein the first portion is positioned (A) in pores of the second portion; (B) atop a surface of the second portion; or (C) a combination thereof.

### Claim 14 (depends on 1)

The method of claim 1, wherein the interface is configured to have an interfacial resistance of less than 1 Ω·cm2.