# US 2021/0288341 A1 · Substrate for composite membrane

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0288341 A1
- Document ID: US20210288341A1
- Status: Published application
- Kind: A1
- Application number: 16/319,661
- Filed: 2017-05-31
- Published: 2021-09-16
- Earliest claimed: 2016-07-25
- Assignees: Teijin Limited
- Applicants: Teijin Limited
- Inventors: Takeo YAMAGUCHI; Yuhei OSHIBA; Hidenori OHASHI; Jin TOMATSU; Koji FURUYA; Takao OHNO; Mami NANBU
- Web page: https://patentgrep.com/patent/US20210288341A1

## CPC

- H01M 8/1062: characterised by the physical properties of the porous support, e.g. its porosity or thickness
- B01D 69/106: {Membranes in the pores of a support, e.g. polymerized in the pores or voids}
- B01D 69/107: {Organic support material}
- B01D 71/261: {Polyethylene}
- B01D 71/262: {Polypropylene}
- C08J 9/26: by elimination of a solid phase from a macromolecular composition or article, e.g. leaching out
- C08J 9/28: by elimination of a liquid phase from a macromolecular composition or article, e.g. drying of coagulum
- C25B 13/08: based on organic materials
- H01M 8/106: characterised by the chemical composition of the porous support
- B01D 2323/02: Hydrophilization
- B01D 2323/12: Specific ratios of components used
- B01D 2325/0283: Pore size
- B01D 2325/04: Characteristic thickness
- B01D 2325/24: Mechanical properties, e.g. strength
- B01D 2325/341: At least two polymers of same structure but different molecular weight
- B01D 2325/36: Hydrophilic membranes
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A substrate for a composite membrane includes a microporous polyolefin membrane for carrying a hydrophilic resin compound within the pores of the microporous membrane wherein: the average pore diameter is 1 nm to 50 nm; the porosity is 50% to 78%; the membrane thickness is 1 μm to 12 μm; and, when a mixed solution of ethanol and water (volume ratio ½) is dripped onto a surface of the microporous polyolefin membrane which has not undergone hydrophilization treatment, the contact angle θ1 between the droplet and the surface is 0 to 90 degrees 1 second after the dripping, and the contact angle θ2 between the droplet and the surface is 0 to 70 degrees 10 minutes after the dripping, and the rate of change of the contact angle ((θ1−θ2)/θ1×100) is 10 to 50%.

## Claims

### Claim 1

A substrate for a composite membrane comprising a microporous polyolefin membrane for carrying a hydrophilic resin compound within pores of the microporous membrane wherein:
the average pore size is 1 nm to 50 nm;
the porosity is 50% to 78%;
the membrane thickness is 1 μm to 12 μm; and
when a mixed solution of ethanol and water (volume ratio ½) is dripped onto a surface of the microporous polyolefin membrane which has not undergone hydrophilization treatment, a contact angle θ1 between the droplet and the surface is 0 to 90 degrees 1 second after the dripping, and a contact angle θ2 between the droplet and the surface is 0 to 70 degrees 10 minutes after the dripping, and a rate of change of the contact angle ((θ1−θ2)/θ1×100) is 10 to 50%.

### Claim 2 (depends on 1)

The substrate for a composite membrane according to claim 1, wherein the rate of change of the contact angle ((θ1−θ2)/θ1×100) is 17 to 41%.

### Claim 3 (depends on 1)

The substrate for a composite membrane according to claim 1, wherein the polyolefin is a polyethylene composition comprising a high molecular weight polyethylene with a mass average molecular weight of 900,000 or more and a low molecular weight polyethylene with a mass average molecular weight of 200,000 to 800,000 mixed at a mass ratio of 20:80 to 80:20.

### Claim 4 (depends on 1)

The substrate for a composite membrane according to claim 1, wherein the substrate for a composite membrane can be impregnated with a liquid which is a solvent for the hydrophilic resin compound and has a surface free energy of 35 to 36.5 mJ/m2

### Claim 5 (depends on 4)

The substrate for a composite membrane according to claim 4, wherein the substrate for a composite membrane can be impregnated with a mixture of ethanol and water in which the water concentration is greater than 65.8% by volume to 70.6% by volume or less.

### Claim 6 (depends on 1)

The substrate for a composite membrane according to claim 1, wherein the Gurley value as measured according to JIS P8117 is 90 s/100 cc or less.

### Claim 7 (depends on 1)

The substrate for a composite membrane according to claim 1, wherein the tensile breaking strength (MD or TD) per unit cross sectional area of the polyolefin solid content is 50 MPa or more.

### Claim 8 (depends on 2)

The substrate for a composite membrane according to claim 2, wherein the polyolefin is a polyethylene composition comprising a high molecular weight polyethylene with a mass average molecular weight of 900,000 or more and a low molecular weight polyethylene with a mass average molecular weight of 200,000 to 800,000 mixed at a mass ratio of 20:80 to 80:20.