# US 2021/0288322 A1 · Secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0288322 A1
- Document ID: US20210288322A1
- Status: Published application
- Kind: A1
- Application number: 17/307,661
- Filed: 2021-05-04
- Published: 2021-09-16
- Earliest claimed: 2018-11-30
- Assignees: Murata Manufacturing Co., Ltd.
- Applicants: Murata Manufacturing Co., Ltd.
- Inventors: Keitaro KITADA; Futoshi SATO; Takaaki MATSUI; Taichi KOGURE; Aya MASHIKO; Yoshifumi SHIMIZU; Kazuki HONDA; Yuta HIRANO; Shinji HATAKE; Naoko YAMAKAWA; Moriaki OKUNO; Masahiro MIYAMOTO
- Web page: https://patentgrep.com/patent/US20210288322A1

## CPC

- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C07D 319/06: not condensed with other rings
- C08F 214/22: Vinylidene fluoride
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/364: {as mixtures}
- H01M 4/366: {as layered products}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/623: {fluorinated polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0567: characterised by the additives
- H01M 10/0587: of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
- H01M 50/414: Synthetic resins, e.g. thermoplastics or thermosetting resins
- H01M 50/449: having a layered structure
- H01M 50/461: {with adhesive layers between electrodes and separators}
- H01M 50/105: Pouches or flexible bags
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2300/0025: Organic electrolyte
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C07D: HETEROCYCLIC COMPOUNDS (macromolecular compounds C08)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A secondary battery includes a positive electrode, a negative electrode, and an electrolytic solution. The positive electrode includes a lithium-cobalt composite oxide having a layered rock-salt crystal structure. The negative electrode includes graphite. An open circuit potential of the negative electrode measured in a full charge state is from 19 mV to 86 mV. A potential variation of the negative electrode is greater than or equal to 1 mV when the secondary battery is discharged from the full charge state by a capacity corresponding to 1% of a maximum discharge capacity. The maximum discharge capacity is obtained when the secondary battery is discharged with a constant current from the full charge state until the closed circuit voltage reaches 3.00 V, following which the secondary battery is discharged with a constant voltage of the closed circuit voltage of 3.00 V for 24 hours.

## Claims

### Claim 1

A secondary battery comprising:
a positive electrode including a lithium-cobalt composite oxide represented by Formula (1) and having a layered rock-salt crystal structure;
a negative electrode including graphite; and
an electrolytic solution, wherein
an open circuit potential, versus a lithium reference electrode, of the negative electrode measured in a full charge state is from 19 millivolts to 86 millivolts, the full charge state being a state in which the secondary battery is charged with a constant voltage of a closed circuit voltage of higher than or equal to 4.38 volts for 24 hours, and
a potential variation of the negative electrode represented by Formula (2) is greater than or equal to 1 millivolt when the secondary battery is discharged from the full charge state by a capacity corresponding to 1 percent of a maximum discharge capacity, the maximum discharge capacity being a discharge capacity obtained when the secondary battery is discharged with a constant current from the full charge state until the closed circuit voltage reaches 3.00 volts, following which the secondary battery is discharged with a constant voltage of the closed circuit voltage of 3.00 volts for 24 hours,
LixCo1-yMyO2-zXz (1)
wherein
M represents at least one of titanium (Ti), vanadium (V), chromium (Cr), manganese (Mn), iron (Fe), nickel (Ni), copper (Cu), sodium (Na), magnesium (Mg), aluminum (Al), silicon (Si), tin (Sn), potassium (K), calcium (Ca), zinc (Zn), gallium (Ga), strontium (Sr), yttrium (Y), zirconium (Zr), niobium (Nb), molybdenum (Mo), barium (Ba), lanthanum (La), tungsten (W), or boron (B),
X represents at least one of fluorine (F), chlorine (Cl), bromine (Br), iodine (I), or sulfur (S), and
x, y, and z satisfy 0.8<x<1.2, 0≤y<0.15, and 0≤z<0.05,
potential variation (millivolt(s)) of negative electrode=second negative electrode potential (millivolt(s))−first negative electrode potential (millivolt(s)) (2)
wherein
the first negative electrode potential is the open circuit potential, versus the lithium reference electrode, of the negative electrode measured in the full charge state, and
the second negative electrode potential is an open circuit potential, versus the lithium reference electrode, of the negative electrode measured in a state in which the secondary battery is discharged from the full charge state by the capacity corresponding to 1 percent of the maximum discharge capacity.

### Claim 2 (depends on 1)

The secondary battery according to claim 1, wherein a potential variation of the positive electrode represented by Formula (3) is greater than or equal to 2 millivolts when the secondary battery is discharged from the full charge state by the capacity corresponding to 1 percent of the maximum discharge capacity,
potential variation (millivolt(s)) of positive electrode=first positive electrode potential (millivolt(s))−second positive electrode potential (millivolt(s)) (3)
wherein
the first positive electrode potential is an open circuit potential, versus the lithium reference electrode, of the positive electrode measured in the full charge state, and
the second positive electrode potential is an open circuit potential, versus the lithium reference electrode, of the positive electrode measured in the state in which the secondary battery is discharged from the full charge state by the capacity corresponding to 1 percent of the maximum discharge capacity.

### Claim 3 (depends on 1)

The secondary battery according to claim 1, wherein
the positive electrode includes a positive electrode active material layer, the positive electrode active material layer including a positive electrode active material and a positive electrode binder,
the positive electrode active material includes the lithium-cobalt composite oxide,
the positive electrode binder includes at least one of a homopolymer or a copolymer, the homopolymer and the copolymer each including vinylidene fluoride as a polymerization unit,
the electrolytic solution includes a cyclic carbonate ester and at least one of a chain carbonate ester or a chain carboxylate ester,
an area density of the positive electrode active material layer is greater than or equal to 36 milligrams per square centimeter,
a volume density of the positive electrode active material layer is greater than or equal to 3.9 grams per cubic centimeter,
a ratio of a weight of the positive electrode binder to a weight of the positive electrode active material layer is from 0.8 weight percent to 2.5 weight percent,
a ratio of a weight of the cyclic carbonate ester to a sum of a weight of the chain carbonate ester and a weight of the chain carboxylate ester is greater than or equal to 0.2 and less than or equal to 1, and
a content of the electrolyte salt in the electrolytic solution is from 0.7 moles per kilogram to 1.5 moles per kilogram with respect to the solvent.

### Claim 4 (depends on 3)

The secondary battery according to claim 3, wherein the homopolymer and the copolymer each including the vinylidene fluoride as the polymerization unit include at least one of polyvinylidene difluoride, a copolymer of the vinylidene fluoride and tetrafluoroethylene, a copolymer of the vinylidene fluoride and hexafluoropropylene, or a copolymer of the vinylidene fluoride, the tetrafluoroethylene, and the hexafluoropropylene.

### Claim 5 (depends on 4)

The secondary battery according to claim 4, wherein
a copolymerization amount of the tetrafluoroethylene is from 0.1 weight percent to 20 weight percent, and
a copolymerization amount of the hexafluoropropylene is from 0.2 weight percent to 5 weight percent.

### Claim 6 (depends on 1)

The secondary battery according to claim 1, wherein
the negative electrode includes a negative electrode active material layer, the negative electrode active material layer including a plurality of first negative electrode active material particles,
the first negative electrode active material particles each include the graphite,
a median diameter D50 of the first negative electrode active material particles is less than or equal to 20 micrometers,
a volume density of the negative electrode active material layer is greater than or equal to 1.5 grams per cubic centimeter, and
an integrated intensity ratio represented by Formula (8) in a case where the negative electrode active material layer is analyzed by X-ray diffractometry is less than or equal to 500,
integrated intensity ratio=second integrated intensity/first integrated intensity (8)
wherein
the first integrated intensity is an integrated intensity of a peak derived from a (002) plane of the graphite, and
the second integrated intensity is an integrated intensity of a peak derived from a (110) plane of the graphite.

### Claim 7 (depends on 6)

The secondary battery according to claim 6, wherein
the negative electrode active material layer further includes a plurality of second negative electrode active material particles, and
the second negative electrode active material particles each include a material including silicon as a constituent element.

### Claim 8 (depends on 6)

The secondary battery according to claim 6, wherein a ratio of mass of the second negative electrode active material particles to mass of the first negative electrode active material particles is from 0.1 mass percent to 5 mass percent.

### Claim 9 (depends on 6)

The secondary battery according to claim 6, wherein a median diameter D50 of the second negative electrode active material particles is smaller than the median diameter D50 of the first negative electrode active material particles.

### Claim 10 (depends on 9)

The secondary battery according to claim 9, wherein the median diameter D50 of the second negative electrode active material particles is from 1 micrometer to 10 micrometers.

### Claim 11 (depends on 6)

The secondary battery according to claim 6, wherein at least a portion of a surface of each of the second negative electrode active material particles is covered with a carbon material.

### Claim 12 (depends on 11)

The secondary battery according to claim 11, wherein the carbon material includes at least one of amorphous carbon, graphite, graphene, a carbon nanotube, or a carbon nanofiber.

### Claim 13 (depends on 1)

The secondary battery according to claim 1, further comprising
a wound electrode body including the positive electrode and the negative electrode, the positive electrode and the negative electrode being wound while being separated away from each other, wherein
the wound electrode body has an elongated shape including a flat part and a pair of curved parts, the pair of curved parts opposing each other with the flat part interposed therebetween,
the positive electrode includes a positive electrode current collector and a positive electrode active material layer, the positive electrode active material layer being provided on the positive electrode current collector,
the positive electrode active material layer includes the lithium-cobalt composite oxide, and
a degree of durability of the positive electrode in the curved parts represented by Formula (12) is less than or equal to 200,
degree of durability=(area density (milligram(s) per square centimeter) of positive electrode active material layer×volume density (gram(s) per cubic centimeter) of positive electrode active material layer)/piercing strength (newton(s)) of positive electrode (12).

### Claim 14 (depends on 1)

The secondary battery according to claim 1, further comprising
a separator interposed between the positive electrode and the negative electrode, wherein
the negative electrode includes a negative electrode active material layer, the negative electrode active material layer including the graphite,
the separator is adhered to the negative electrode active material layer, and
an adhesive strength of the negative electrode active material layer to the separator is from 5 millinewtons per millimeter to 100 millinewtons per meter.

### Claim 15 (depends on 14)

The secondary battery according to claim 14, wherein
the separator includes
a base layer, and
a first polymer compound layer provided on the base layer and adhered to the negative electrode active material layer, and
the first polymer compound layer includes a plurality of insulating particles.

### Claim 16 (depends on 14)

The secondary battery according to claim 14, wherein
the positive electrode includes a positive electrode active material layer, the positive electrode active material layer including the lithium-cobalt composite oxide,
the separator is adhered to the positive electrode active material layer, and
an adhesive strength of the positive electrode active material layer to the separator is from 5 millinewtons per millimeter to 100 millinewtons per meter.

### Claim 17 (depends on 1)

The secondary battery according to claim 1, wherein
the electrolytic solution includes a chain carboxylate ester and at least one of a carbonate ester or a lactone, and
a ratio of a volume of the chain carboxylate ester to a sum of a volume of the carbonate ester, a volume of the lactone, and a volume of the chain carboxylate ester is from 10 volume percent to 80 volume percent.

### Claim 18 (depends on 17)

The secondary battery according to claim 17, wherein
the chain carboxylate ester includes at least one of an acetate ester, a propionate ester, or a butyrate ester, and
a molecular weight of the chain carboxylate ester is less than or equal to 119.

### Claim 19 (depends on 17)

The secondary battery according to claim 17, wherein
the electrolytic solution further includes a dinitrile compound, and
a content of the dinitrile compound in the electrolytic solution is from 1 weight percent to 20 weight percent.

### Claim 20 (depends on 17)

The secondary battery according to claim 17, wherein
the electrolytic solution further includes a halogenated carbonate ester and a dioxane compound, the dioxane compound being represented by Formula (17),
a content of the halogenated carbonate ester in the electrolytic solution is from 1 weight percent to 20 weight percent, and
a content of the dioxane compound in the electrolytic solution is from 0.1 weight percent to 2 weight percent,
wherein each of R1 to R8 represents one of a hydrogen group and a monovalent hydrocarbon group.