# US 2021/0288304 A1 · Anisotropic expansion of silicon-dominant anodes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0288304 A1
- Document ID: US20210288304A1
- Status: Published application
- Kind: A1
- Application number: 17/242,169
- Filed: 2021-04-27
- Published: 2021-09-16
- Earliest claimed: 2019-11-05
- Assignees: Enevate Corporation
- Applicants: Enevate Corporation
- Inventors: Rahul Kamath; Fred Bonhomme; Ian Browne
- Web page: https://patentgrep.com/patent/US20210288304A1

## CPC

- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/622: {being polymers}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/44: Methods for charging or discharging (circuits for charging H02J7/00)
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Systems and methods for anisotropic expansion of silicon-dominant anodes may include forming an anode by pyrolyzing an active material layer comprising a binder and silicon particles in a temperature range of 600 to 800° C.; and forming a battery cell comprising a cathode, an electrolyte, and the anode, where the anode comprises the pyrolyzed active material layer on a current collector. A lateral expansion of the anode during operation may be less than 2%, less than 1%, or less than 0.6%. The active material layer may be pyrolyzed on the current collector or may be pyrolyzed on a substrate before laminating on the current collector. The anode active material layer may be pyrolyzed using a 1 hour dwell time or less or using a 2 hour dwell time or less. The active material layer may be pyrolyzed in a temperature range of 650 to 800° C.

## Claims

### Claim 1

A method of forming a battery cell, the method comprising:
forming an anode by pyrolyzing an active material layer comprising a binder and silicon particles in a temperature range of 600 to 800° C.;
forming a battery cell comprising a cathode, an electrolyte, and the anode, the anode comprising the pyrolyzed active material layer on a current collector, wherein a lateral expansion of the anode during operation is less than 2%.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the lateral expansion of the anode during operation is less than 1%.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the lateral expansion of the anode during operation is less than 0.6%.

### Claim 4 (depends on 1)

The method according to claim 1, comprising pyrolyzing the active material layer on the current collector.

### Claim 5 (depends on 1)

The method according to claim 1, comprising pyrolyzing the active material layer on a substrate before laminating on the current collector.

### Claim 6 (depends on 1)

The method according to claim 1, comprising pyrolyzing the anode active material layer using a 1 hour dwell time or less.

### Claim 7 (depends on 1)

The method according to claim 1, comprising pyrolyzing the anode active material layer using a 2 hour dwell time or less.

### Claim 8 (depends on 1)

The method according to claim 1, comprising pyrolyzing the active material layer in a temperature range of 650 to 800° C.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the current collector comprises copper.

### Claim 10

A method of forming a battery cell, the method comprising:
forming an anode by pyrolyzing an active material layer comprising a binder and silicon particles in a temperature range of 650 to 800° C.;
forming a battery cell comprising a cathode, an electrolyte, and the anode, the anode comprising the pyrolyzed active material layer on a copper current collector, wherein a lateral expansion of the anode during operation is less than 1%.