# US 2021/0288246 A1 · Inverted wide base double magnetic tunnel junction device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0288246 A1
- Document ID: US20210288246A1
- Status: Published application
- Kind: A1
- Application number: 16/817,744
- Filed: 2020-03-13
- Published: 2021-09-16
- Earliest claimed: 2020-03-13
- Assignees: International Business Machines Corporation
- Applicants: International Business Machines Corporation
- Inventors: Pouya Hashemi; Bruce B. Doris; Janusz Jozef Nowak; Jonathan Zanhong Sun
- Web page: https://patentgrep.com/patent/US20210288246A1

## CPC

- H10N 50/01: Manufacture or treatment
- H10N 50/10: Magnetoresistive devices
- H10B 61/00: Magnetic memory devices, e.g. magnetoresistive RAM [MRAM] devices
- H10N 50/80: Constructional details
- H10N 50/85: Materials of the active region
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A method of manufacturing a double magnetic tunnel junction device is provided. The method includes forming a first magnetic tunnel junction stack, forming a spin conducting layer on the first magnetic tunnel junction stack, and forming a second magnetic tunnel junction stack on the spin conducting layer. The second magnetic tunnel junction stack has a width that is greater than a width of the first magnetic tunnel junction stack.

## Claims

### Claim 1

A method of manufacturing a double magnetic tunnel junction device, the method comprising:
forming a first magnetic tunnel junction stack;
forming a spin conducting layer on the first magnetic tunnel junction stack; and
forming a second magnetic tunnel junction stack on the spin conducting layer, the second magnetic tunnel junction stack having a width that is greater than a width of the first magnetic tunnel junction stack.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the first magnetic tunnel junction stack is formed on a back end of line base layer.

### Claim 3 (depends on 1)

The method according to claim 1,
wherein the first magnetic tunnel junction stack includes a first reference layer, a first tunnel barrier layer, and a first magnetic free layer, and
wherein the second magnetic tunnel junction stack includes a second reference layer, a second tunnel barrier layer, and a second magnetic free layer.

### Claim 4 (depends on 1)

The method according to claim 1, wherein, after forming the spin conducting layer, the method further comprises:
forming a first dielectric layer on sides of the first magnetic tunnel junction stack and on sides of the spin conducting layer; and
forming a second spin conducting layer on the spin conducting layer, the second spin conducting layer having a width that is greater than a width of the spin conducting layer and greater than the width of the first magnetic tunnel junction stack.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the second spin conducting layer is formed in direct contact with the spin conducting layer, and wherein the second spin conducting layer has a same material composition as the spin conducting layer.

### Claim 6 (depends on 4)

The method according to claim 4, wherein, after forming the spin conducting layer, the method further comprises:
forming a first dielectric layer on the sides of the first magnetic tunnel junction stack and on the sides of the spin conducting layer;
forming a second spin conducting layer on the spin conducting layer and the first dielectric layer,
forming the second magnetic tunnel junction stack on the second spin conducting layer;
forming a metal etch-stop layer on the second magnetic tunnel junction stack;
forming a metal hardmask layer on the metal etch-stop layer; and
etching through the metal etch-stop layer, the second magnetic tunnel junction stack, the second spin conducting layer, and a portion of a thickness of the first dielectric layer,
wherein the second spin conducting layer has a width that is the same as the width of the second magnetic tunnel junction stack.

### Claim 7 (depends on 4)

The method according to claim 4, further comprising pre-treating exposed surfaces with at least one selected from the group consisting of plasma O2, H2, N2 and NH3 prior to forming the second spin conducting layer.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the spin conducting layer comprises at least one non-magnetic material selected from the group consisting of Cu, CuN, Ag and AgSn.

### Claim 9 (depends on 1)

The method according to claim 1, further comprising forming a dielectric encapsulation layer on the second magnetic tunnel junction stack.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the dielectric encapsulation layer comprises at least one selected from the group consisting of PVD, ALD, PECVD, AlOx, TiOx, BN, SiN and SiBCN.

### Claim 11

A double magnetic tunnel junction device comprising:
a first magnetic tunnel junction stack;
a spin conducting layer on the first magnetic tunnel junction stack; and
a second magnetic tunnel junction stack on the spin conducting layer, the second magnetic tunnel junction stack having a width that is greater than a width of the first magnetic tunnel junction stack.

### Claim 12 (depends on 11)

The double magnetic tunnel junction device according to claim 11, wherein the first magnetic tunnel junction stack is on a back end of line base layer.

### Claim 13 (depends on 12)

The double magnetic tunnel junction device according to claim 12, further comprising a seed layer between the back end of line base layer and the first magnetic tunnel junction stack.

### Claim 14 (depends on 11)

The double magnetic tunnel junction device according to claim 11,
wherein the first magnetic tunnel junction stack includes a first reference layer, a first tunnel barrier layer, and a first magnetic free layer, and
wherein the second magnetic tunnel junction stack includes a second reference layer, a second tunnel barrier layer, and a second magnetic free layer.

### Claim 15 (depends on 11)

The double magnetic tunnel junction device according to claim 11, further comprising:
a first dielectric layer on sides of the first magnetic tunnel junction stack and on sides of the spin conducting layer; and
a second spin conducting layer on the spin conducting layer, the second spin conducting layer having a width that is greater than a width of the spin conducting layer and greater than the width of the first magnetic tunnel junction stack.

### Claim 16 (depends on 15)

The double magnetic tunnel junction device according to claim 15, wherein the second spin conducting layer is in direct contact with the spin conducting layer, and wherein the second spin conducting layer has a same material composition as the spin conducting layer.

### Claim 17 (depends on 15)

The double magnetic tunnel junction device according to claim 15, further comprising:
a first dielectric layer on the sides of the first magnetic tunnel junction stack and on the sides of the spin conducting layer;
a second spin conducting layer on the spin conducting layer, the second magnetic tunnel junction stack formed on the second spin conducting layer;
a metal etch stop layer on the second magnetic tunnel junction stack; and
a metal hardmask layer on the metal etch stop layer,
wherein the second spin conducting layer has a width that is the same as the width of the second magnetic tunnel junction stack.

### Claim 18 (depends on 11)

The double magnetic tunnel junction device according to claim 11, wherein the spin conducting layer comprises at least one non-magnetic material selected from the group consisting of Cu, CuN, Ag and AgSn.

### Claim 19 (depends on 11)

The double magnetic tunnel junction device according to claim 11, further comprising a dielectric encapsulation layer on the second magnetic tunnel junction stack.

### Claim 20 (depends on 19)

The double magnetic tunnel junction device according to claim 19, wherein the dielectric encapsulation layer comprises at least one selected from the group consisting of PVD, ALD, PECVD, AlOx, TiOx, BN, SiN and SiBCN.