# US 2021/0288227 A1 · Wavelength conversion material, method of manufacturing thereof and light emitting device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0288227 A1
- Document ID: US20210288227A1
- Status: Published application
- Kind: A1
- Application number: 17/033,699
- Filed: 2020-09-26
- Published: 2021-09-16
- Earliest claimed: 2020-03-11
- Assignees: Lextar Electronics Corporation
- Applicants: Lextar Electronics Corporation
- Inventors: Yi-Ting TSAI; Hung-Chia WANG; Chia-Chun HSIEH; Hung-Chun TONG; Yu-Chun LEE; Tzong-Liang TSAI
- Web page: https://patentgrep.com/patent/US20210288227A1

## CPC

- H10H 20/8512: {Wavelength conversion materials}
- C09K 11/77348: {Silicon Aluminium Nitrides or Silicon Aluminium Oxynitrides}
- H10H 20/818: within the light-emitting regions
- H10H 20/0361: {of wavelength conversion means}
- Y02B 20/00: Energy efficient lighting technologies, e.g. halogen lamps or gas discharge lamps
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y02B: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO BUILDINGS, e.g. HOUSING, HOUSE APPLIANCES OR RELATED END-USER APPLICATIONS

## Abstract

The wavelength conversion material includes a general formula (I) MmAaBbCcDdEe:ESxREy and satisfies a condition (II) that a proportion of D for the wavelength conversion material greater than or equal to 50%. M is selected from a group consisting of Ca, Sr and Ba. A is selected from a group consisting of elements Mg, Mn, Zn and Cd. B is selected from a group consisting of elements B, Al, Ga and In. C is selected from a group consisting of Si, Ge, Ti and Hf. D is selected from a group consisting of elements O, S and Se. E is selected from a group consisting of elements N and P. ES is selected from a group consisting of divalent Eu, Sm and Yb. RE is selected from a group consisting of trivalent Ce, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er and Tm.

## Claims

### Claim 1

A wavelength conversion material comprising a general formula (I) and satisfying a condition (II);
wherein the general formula (I) is MmAaBbCcDdEe:ESxREy, M is selected from a group consisting of Ca, Sr and Ba, 0.8≤m≤1.5; A is selected from at a group consisting of elements Mg, Mn, Zn and Cd, 0.1≤a≤1; B is selected from a group consisting of elements B, Al, Ga and In, 0.5≤b≤1.5; C is selected from a group consisting of Si, Ge, Ti and Hf, 5≤c≤40; D is selected from a group consisting of elements O, S and Se, 10≤d≤80; E is selected from a group consisting of elements N and P, 0.01≤e≤3; ES is selected from a group consisting of divalent Eu, Sm and Yb, 0≤x≤1; RE is selected from a group consisting of trivalent Ce, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er and Tm, 0≤y≤1, and 0<x+y≤1; and
wherein the condition (II) is that a proportion of the element D for the wavelength conversion material is greater than or equal to 50%.

### Claim 2 (depends on 1)

The wavelength conversion material of claim 1, wherein the wavelength conversion material is excited by a blue light source or an ultraviolet light source to emit a light, the light has a peak in a spectrum, and the peak corresponds to a wavelength ranging from 610 nm to 655 nm.

### Claim 3 (depends on 1)

The wavelength conversion material of claim 1, wherein the wavelength conversion material further satisfies a condition (III),
wherein the condition (III) is that the light has a maximum intensity, a difference between maximum and minimum wavelengths corresponding to 50% of the maximum intensity is p, a difference between maximum and minimum wavelengths corresponding to 10% of the maximum intensity is q, wherein 2p≤q≤5p.

### Claim 4 (depends on 1)

The wavelength conversion material of claim 1, further comprising polycrystalline crystal.

### Claim 5 (depends on 4)

The wavelength conversion material of claim 4, further comprising amorphous crystal.

### Claim 6 (depends on 1)

A light emitting device, comprising:
a light source; and
the wavelength conversion material of claim 1.

### Claim 7 (depends on 6)

The light emitting device of claim 6, wherein the light source comprises a blue light emitting diode or an ultraviolet light emitting diode.

### Claim 8 (depends on 7)

The light emitting device of claim 7, wherein the wavelength conversion material is excited by the blue light source or the ultraviolet light source to emit a light, the light has a peak in a spectrum, and the peak corresponds to a wavelength ranging from 610 nm to 655 nm.

### Claim 9 (depends on 6)

The light emitting device of claim 6, wherein the wavelength conversion material further satisfies a condition (III),
wherein the condition (III) is that the light has a maximum intensity, a difference between maximum and minimum wavelengths corresponding to 50% of the maximum intensity is p, a difference between maximum and minimum wavelengths corresponding to 10% of the maximum intensity is q, wherein 2p≤q≤5p.

### Claim 10 (depends on 6)

The light emitting device of claim 6, wherein the wavelength conversion material comprises polycrystalline crystal.

### Claim 11 (depends on 10)

The light emitting device of claim 10, wherein the wavelength conversion material further comprises amorphous crystal.

### Claim 12 (depends on 1)

A method of manufacturing the wavelength conversion material of claim 1, comprising:
configuring corresponding raw materials of selected elements M, A, B, C, D and E of the general formula (I) as a first mixture;
treating the first mixture under a first high-temperature process to have a first product;
configuring the first product and corresponding raw materials of at least one of selected elements ES and RE of the general formula (I) as a second mixture; and
treating the second mixture under a second high-temperature process in reducing atmosphere to have the wavelength conversion material.

### Claim 13 (depends on 12)

The method of claim 12, wherein in the operation of configuring corresponding raw materials of selected elements M, A, B, C, D and E of the general formula (I) as the first mixture, the corresponding raw materials of selected elements M, A, B, C, D and E of the general formula (I) comprise oxynitride, carbonate sulfide or salts, and the corresponding raw materials of selected elements M, A, B, C, D and E of the general formula (I) are dissolved in an acidic solution to form the first mixture.

### Claim 14 (depends on 12)

The method of claim 12, wherein the first high-temperature process is a sintering process between 200° C. and 600° C.

### Claim 15 (depends on 12)

The method of claim 12, wherein the second high-temperature process is a calcination process between 800° C. and 1500° C.