# US 2021/0288207 A1 · High temperature acid etch for silicon

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0288207 A1
- Document ID: US20210288207A1
- Status: Published application
- Kind: A1
- Application number: 17/202,023
- Filed: 2021-03-15
- Published: 2021-09-16
- Earliest claimed: 2020-03-16
- Assignees: 1366 Technologies, Inc.
- Applicants: 1366 Technologies Inc.
- Inventors: Ralf JONCZYK; Patrick MCMAHON
- Web page: https://patentgrep.com/patent/US20210288207A1

## CPC

- H10F 71/1221: {comprising polycrystalline silicon}
- H10F 77/703: {of the semiconductor bodies, e.g. textured active layers}
- C09K 13/08: containing a fluorine compound
- H10P 50/642: {Chemical etching}
- H10P 50/667: {by liquid etching only}
- Y02E 10/546: Polycrystalline silicon PV cells
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method includes etching silicon using a mixture of nitric acid and hydrofluoric acid in which less than 6 mols of hydrofluoric acid is used to etch one mol of silicon. The etching may be conducted at an elevated temperature, such as a temperature of at least 70 degrees Celsius.

## Claims

### Claim 1

A method comprising etching silicon using a mixture of nitric acid and hydrofluoric acid in which less than 6 mols of hydrofluoric acid is used to etch one mol of silicon at a temperature above room temperature.

### Claim 2 (depends on 1)

The method of claim 1, wherein about 4 mols of hydrofluoric acid are used to etch one mol of silicon.

### Claim 3 (depends on 1)

The method of claim 1, wherein the etching is conducted at a temperature of at least 70 degrees Celsius.

### Claim 4 (depends on 1)

The method of claim 1, wherein the etching is conducted at a temperature of 70 to 130 degrees Celsius.

### Claim 5 (depends on 1)

The method of claim 1, wherein the etching is conducted at a temperature of at least 90 degrees Celsius.

### Claim 6 (depends on 1)

The method of claim 1, wherein the etching is conducted at a temperature of 90 to 110 degrees Celsius.

### Claim 7 (depends on 1)

The method of claim 1, wherein the mixture further comprises a metal catalyst to form cup-like texture in surface of the silicon by metal catalyzed chemical etching.

### Claim 8 (depends on 1)

The method of claim 1, wherein during the etching, the nitric acid oxidizes the silicon to silicon dioxide, and the hydrofluoric acid dissolves the silicon dioxide.

### Claim 9 (depends on 8)

The method of claim 8, wherein:
the nitric acid oxidizes the silicon to the silicon dioxide by forming nitrogen dioxide which oxidizes the silicon according to equation (I):
Si+2HNO3→SiO2+2NO2+H2O (I); and
the hydrofluoric acid dissolves the silicon dioxide according to equation (II):
SiO2+4HF→SiF4+2H2O (II).

### Claim 10 (depends on 8)

The method of claim 8, wherein reaction products of the etching comprise silicon tetrafluoride gas and water vapor.

### Claim 11 (depends on 10)

The method of claim 10, wherein the reaction products of the etching consist essentially of the silicon tetrafluoride gas and the water vapor, and include less than 1 mol percent of H2SiF6.

### Claim 12 (depends on 1)

The method of claim 1, wherein 2 moles of less of the nitric acid are used to etch one mol of the silicon.

### Claim 13 (depends on 1)

The method of claim 1, wherein the mixture further comprises a diluent comprising sulfuric acid.

### Claim 14 (depends on 13)

The method of claim 13, wherein:
the diluent comprises at least 50 volume percent of the sulfuric acid and up to 50 volume percent water;
the etching is started when the mixture contacts the silicon in a vessel; and
there is no liquid bleed from the vessel during the etching.

### Claim 15 (depends on 1)

The method of claim 1, wherein the silicon comprises polycrystalline silicon.

### Claim 16 (depends on 1)

The method of claim 1, wherein the silicon comprises a polycrystalline silicon wafer.

### Claim 17 (depends on 16)

The method of claim 16, further comprising forming a solar cell on the polycrystalline silicon wafer after the etching.

### Claim 18

A method comprising etching silicon using a mixture of nitric acid and hydrofluoric acid at a temperature of at least 70 degrees Celsius.

### Claim 19 (depends on 1)

The method of claim 1, wherein the etching is conducted at a temperature of 70 to 130 degrees Celsius, and the mixture further comprises a diluent comprising sulfuric acid.

### Claim 20

A method comprising etching silicon using a mixture of nitric acid, hydrofluoric acid and sulfuric acid at above room temperature.