# US 2021/0288185 A1 · Array substrate and method of preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0288185 A1
- Document ID: US20210288185A1
- Status: Published application
- Kind: A1
- Application number: 16/644,254
- Filed: 2019-11-22
- Published: 2021-09-16
- Earliest claimed: 2019-08-13
- Assignees: Wuhan China Star Optoelectronics Semiconductor Display Technology Co., Ltd.
- Applicants: Wuhan China Star Optoelectronics Semiconductor Display Technology Co., Ltd.
- Inventors: Chengjun FAN
- Web page: https://patentgrep.com/patent/US20210288185A1

## CPC

- H10D 30/6732: {Bottom-gate only TFTs}
- H10D 30/0316: {of lateral bottom-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D 30/6737: {characterised by the electrode materials}
- H10D 30/6743: {Silicon}
- H10D 30/6745: {Polycrystalline or microcrystalline silicon}
- H10D 62/116: {adjoining the input or output regions of field-effect devices, e.g. adjoining source or drain regions}
- H10P 14/3802: {Crystallisation or recrystallisation of non-monocrystalline semiconductor materials, e.g. regrowth}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present disclosure provides an array substrate and a method of preparing the same. The array substrate includes a substrate, a gate, a gate insulation layer, an active layer, a crystallization layer, an oxide layer, a source/drain metal layer, and a passivation layer. After the crystallization layer is prepared, a mask plate is not removed and is used to protect an upper surface of the crystallization layer from oxidation reaction. Then, an oxide layer is formed on sidewalls of the crystallization layer and the active layer. The oxide layer is used to obstruct the source/drain metal layer from contacting the active layer. The source/drain metal layer is only in contact with the crystallization layer, thereby reducing a path of leakage current and achieving a purpose of reducing the leakage current.

## Claims

### Claim 1

An array substrate, comprising:
a substrate;
a gate disposed on the substrate;
a gate insulation layer disposed on the gate and the substrate;
an active layer disposed on a side of the gate insulation layer away from the gate;
a crystallization layer disposed on a side of the active layer away from the gate insulation layer;
an oxide layer disposed on two sides of each of the active layer and the crystallization layer;
a source/drain metal layer disposed over the gate and the crystallization layer, wherein the source/drain metal layer covers the oxide layer and is provided with a through hole passing through the source/drain metal layer, the crystallization layer, and a part of the active layer; and
a passivation layer disposed over the source/drain metal layer and the gate and provided in the through hole.

### Claim 2 (depends on 1)

The array substrate as claimed in claim 1, wherein material of the oxide layer comprises silicon oxide.

### Claim 3 (depends on 1)

The array substrate as claimed in claim 1, wherein material of the crystallization layer comprises polysilicon and boron; and
material of the active layer comprises polysilicon.

### Claim 4 (depends on 1)

The array substrate as claimed in claim 1, wherein the source/drain metal layer is composed of three stacked metal layers, and specifically comprises:
a first metal layer;
a second metal layer disposed on the first metal layer; and
a third metal layer disposed on a side of the second metal layer away from the first metal layer.

### Claim 5 (depends on 1)

The array substrate as claimed in claim 1, wherein the through hole is formed into a groove that is located at the active layer and the crystallization layer.

### Claim 6 (depends on 1)

The array substrate as claimed in claim 1, wherein material of the passivation layer comprises silicon oxide.

### Claim 7 (depends on 4)

The array substrate as claimed in claim 4, wherein material of each of the first metal layer and the third metal layer comprises molybdenum; and
material of the second metal layer comprises aluminum and copper.

### Claim 8 (depends on 1)

The array substrate as claimed in claim 1, wherein the source/drain metal layer has a source wiring structure and a drain wiring structure, and the source wiring structure and the drain wiring structure are connected to the crystallization layer.

### Claim 9

A method of preparing an array substrate, comprising steps of:
providing a substrate;
depositing a gate on the substrate;
depositing a gate insulation layer on the substrate and the gate;
depositing an amorphous silicon material that is formed as an active layer provided with amorphous silicon over the gate, implanting boron into a surface of the amorphous silicon material, and rapidly heating the amorphous silicon material to crystallize a crystallization layer;
disposing a mask plate on the crystallization layer and forming a corresponding pattern by exposure and development;
performing a plasma process on sidewalls of the active layer and the crystallization layer to form an oxide layer;
removing the mask plate and depositing a source/drain metal layer over the gate and the crystallization layer;
patterning the source/drain metal layer to form a source wiring structure and a drain wiring structure, wherein a gap is between the source wiring structure and the drain wiring structure;
etching the crystallization layer at the gap to form a groove; and
depositing a passivation layer over the gate insulation layer and the source/drain metal layer, wherein the passivation layer fills the groove.

### Claim 10 (depends on 9)

The method of preparing the array substrate as claimed in claim 9, wherein in the step of rapidly heating the amorphous silicon material to crystallize the crystallization layer, temperature of heating ranges from 600 to 650 degrees Celsius and time of heating ranges from 10 to 20 minutes.