# US 2021/0287996 A1 · Method for making aluminum nitride wafer and aluminum nitride wafer made by the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0287996 A1
- Document ID: US20210287996A1
- Status: Published application
- Kind: A1
- Application number: 16/922,127
- Filed: 2020-07-07
- Published: 2021-09-16
- Earliest claimed: 2020-03-13
- Assignees: Hong Chuang Applied Technology Co., Ltd.
- Applicants: Hong Chuang Applied Technology Co., Ltd
- Inventors: Yan-Kai ZENG; Bai-Xuan JIANG
- Web page: https://patentgrep.com/patent/US20210287996A1

## CPC

- H10W 46/00: Marks applied to devices, e.g. for alignment or identification
- B24B 37/04: designed for working plane surfaces
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10P 90/12: {Preparing bulk and homogeneous wafers}
- H10P 90/123: {by grinding or lapping}
- H10P 90/128: {by edge treatment, e.g. chamfering}
- H10P 90/18: {by shaping}
- H10W 46/201: {located on the periphery of wafers, e.g. orientation notches or lot numbers}
- H10W 46/301: {for alignment}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides an aluminum nitride wafer and a method for making the same. The method includes forming at least one alignment notch in or at least one flat alignment edge on a periphery of the aluminum nitride wafer. The alignment notch and the flat alignment edge can prevent the aluminum nitride wafer from being in a poor state during the semiconductor manufacturing process and makes it possible to position the aluminum nitride wafer precisely so that the fraction defective can be lowered. The aluminum nitride wafer of the present invention has advantages of effective insulation, efficient heat dissipation, and a high dielectric constant, and can be used in semiconductor manufacturing processes, electronic products, and semiconductor equipment.

## Claims

### Claim 1

A method for making an aluminum nitride wafer, comprising the steps of:
(a) subjecting an aluminum nitride green-body block to a high-temperature treatment and thereby turning the aluminum nitride green-body block into an aluminum nitride wafer block;
(b) forming at least one alignment notch in or at least one flat alignment edge on a periphery of the aluminum nitride wafer block, and cutting the aluminum nitride wafer block into a plurality of aluminum nitride wafer slices; and
(c) lapping and polishing each of the aluminum nitride wafer slice.

### Claim 2 (depends on 1)

The method of claim 1, wherein the aluminum nitride green-body block is obtained by placing an aluminum nitride green body into a mold, shaping the aluminum nitride green body in a mechanical or hydraulic manner, and performing an iso static pressing process with water pressure, oil pressure, or gas pressure; wherein, the mechanical or hydraulic molding is performed at a molding force of 98066.50 to 9806650.00 N, a pressure in the mold is −0.063 to 100 atm, and the water, oil, or gas pressure-based isostatic pressing process uses a pressure of 100 to 8000 atm and a temperature of 10° C. to 100° C.

### Claim 3

A method for making an aluminum nitride wafer, comprising the steps of:
(a) providing an aluminum nitride green-body slice, which can be obtained either by subjecting an aluminum nitride green body to a tape-casting process, or by first subjecting the aluminum nitride green body to a tape-casting process to form an aluminum nitride green-body roll and then cutting the aluminum nitride green-body roll;
(b) subjecting the aluminum nitride green-body slice to a high-temperature treatment such that the aluminum nitride green-body slice is turned into an aluminum nitride wafer slice; and
(c) forming at least one alignment notch in or at least one flat alignment edge on a periphery of the aluminum nitride wafer slice, and then lapping and polishing the aluminum nitride wafer slice.

### Claim 4 (depends on 1)

The method of claim 1, wherein the high-temperature treatment includes a debinding process and a sintering process; wherein, the debinding process is performed at a temperature of 200° C. to 900° C. in an environment that contains hydrogen, nitrogen, oxygen, argon, or air; and the sintering process is conducted at a temperature of 1000° C. to 3000° C. under a vacuum-pressure, atmospheric-pressure, or a high-pressure, and in an environment that contains hydrogen, nitrogen, or argon.

### Claim 5 (depends on 3)

The method of claim 3, wherein the high-temperature treatment includes a debinding process and a sintering process; wherein, the debinding process is performed at a temperature of 200° C. to 900° C. in an environment that contains hydrogen, nitrogen, oxygen, argon, or air; and the sintering process is conducted at a temperature of 1000° C. to 3000° C. under a vacuum-pressure, atmospheric-pressure, or a high-pressure, and in an environment that contains hydrogen, nitrogen, or argon.

### Claim 6 (depends on 2)

The method of claim 2, wherein the aluminum nitride green body includes aluminum nitride granules; wherein, the aluminum nitride granules are obtained by mixing aluminum oxide and/or pure aluminum powder with an organic adhesive that contains nitrogen, carbon, and hydrogen atoms; subjecting the mixture to high-temperature carbothermic reduction in a gaseous environment containing nitrogen, carbon, and hydrogen atoms; performing high-temperature decarbonization in a nitrogen atmosphere, an oxygen atmosphere, or an atmospheric gaseous environment; and performing granulation.

### Claim 7 (depends on 3)

The method of claim 3, wherein the aluminum nitride green body includes aluminum nitride granules; wherein, the aluminum nitride granules are obtained by mixing aluminum oxide and/or pure aluminum powder with an organic adhesive that contains nitrogen, carbon, and hydrogen atoms; subjecting the mixture to high-temperature carbothermic reduction in a gaseous environment containing nitrogen, carbon, and hydrogen atoms; performing high-temperature decarbonization in a nitrogen atmosphere, an oxygen atmosphere, or an atmospheric gaseous environment; and performing granulation.

### Claim 8 (depends on 6)

The method of claim 6, wherein the high-temperature carbothermic reduction is completed at a temperature of 600° C. to 3000° C.

### Claim 9 (depends on 7)

The method of claim 7, wherein the high-temperature carbothermic reduction is completed at a temperature of 600° C. to 3000° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the step (c) further includes chamfering a periphery of the aluminum nitride wafer slice before or after the aluminum nitride wafer slice is lapped and polished; wherein, a shape of a chamfered periphery includes a rectangular shape, a semicircular shape, an asymmetric semicircular shape, a semielliptical shape, an asymmetric semielliptical shape, a symmetric trapezoidal shape, an asymmetric trapezoidal shape, a shape incorporating a semicircle into a symmetric trapezoid, and a shape incorporating a semicircle into an asymmetric trapezoid.

### Claim 11 (depends on 3)

The method of claim 3, wherein the step (c) further includes chamfering a periphery of the aluminum nitride wafer slice before or after the aluminum nitride wafer slice is lapped and polished; wherein, a shape of a chamfered periphery includes a rectangular shape, a semicircular shape, an asymmetric semicircular shape, a semielliptical shape, an asymmetric semielliptical shape, a symmetric trapezoidal shape, an asymmetric trapezoidal shape, a shape incorporating a semicircle into a symmetric trapezoid, and a shape incorporating a semicircle into an asymmetric trapezoid.

### Claim 12 (depends on 1)

The method of claim 1, wherein the alignment notch is a V-shaped groove, and its pointed V-shaped bottom as well as its left and right upper portions are curved.

### Claim 13 (depends on 3)

The method of claim 3, wherein the alignment notch is a V-shaped groove, and its pointed V-shaped bottom as well as its left and right upper portions are curved.

### Claim 14 (depends on 1)

The method of claim 1, wherein the flat alignment edge is formed by laser, a water jet cutter, or mechanical processing.

### Claim 15 (depends on 3)

The method of claim 3, wherein the flat alignment edge is formed by laser, a water jet cutter, or mechanical processing.

### Claim 16 (depends on 1)

An aluminum nitride wafer obtained using the method of claim 1, wherein a periphery of the aluminum nitride wafer includes at least one alignment notch or at least one flat alignment edge.

### Claim 17 (depends on 3)

An aluminum nitride wafer obtained using the method of claim 3, wherein a periphery of the aluminum nitride wafer includes at least one alignment notch or at least one flat alignment edge.