# US 2021/0287949 A1 · In Situ Monitoring of Field-Effect Transistors During Atomic Layer Deposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0287949 A1
- Document ID: US20210287949A1
- Status: Published application
- Kind: A1
- Application number: 17/197,654
- Filed: 2021-03-10
- Published: 2021-09-16
- Earliest claimed: 2020-03-10
- Assignees: Northwestern University
- Applicants: Northwestern University
- Inventors: Michael J. Moody; Lincoln J. Lauhon; Ju Ying Shang
- Web page: https://patentgrep.com/patent/US20210287949A1

## CPC

- H10P 74/207: {Electrical properties, e.g. testing or measuring of resistance, deep levels or capacitance-voltage characteristics}
- C23C 16/305: {Sulfides, selenides, or tellurides}
- C23C 16/45544: {characterized by the apparatus}
- C23C 16/52: Controlling or regulating the coating process {(C23C16/45557, C23C16/279 take precedence)}
- G01R 31/2621: {for testing field effect transistors, i.e. FET's}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/3436: {being chalcogenide semiconductor materials not being oxides, e.g. ternary compounds}
- H10P 72/0604: {Process monitoring, e.g. flow or thickness monitoring}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- G01R: MEASURING ELECTRIC VARIABLES; MEASURING MAGNETIC VARIABLES (indicating correct tuning of resonant circuits H03J3/12)

## Abstract

A system and method for performing in-situ measurements of semiconductor devices during chemical vapor deposition (CVD) includes disposing a chip carrier within a sealed chamber of a reactor for carrying out in-situ monitoring of partially fabricated semiconductor devices. The chip carrier includes a plurality of metallized bonding pads disposed along both peripheral edges on a same surface of the base for making electrical connections to metallized pads or contacts on the semiconductor device through bonding wires. Each of the plurality of metallized bonding pads disposed along both peripheral edges is electrically connected to each other as a pair through electrically connecting to a corresponding pair of ports which are disposed along both peripheral edges of the chip carrier. In-situ monitoring of the partially fabricated semiconductor device is performed through connecting the plurality of ports on the chip carrier to an external source-measure unit through a connector and wire harness.

## Claims

### Claim 1

A system for in-situ monitoring of semiconductor devices during chemical vapor deposition, comprising:
a reactor having a sealed chamber for carrying out chemical vapor deposition (CVD) on semiconductor devices, wherein the reactor is configured with a plurality of openings for passaging of reactive gases and for in-situ monitoring of the semiconductor devices within the sealed chamber during the CVD; and
a chip carrier configured to be disposed within the sealed chamber, wherein the chip carrier is configured for mounting at least one partially fabricated semiconductor device on a base, wherein the chip carrier comprises a plurality of metallized bonding pads disposed along both peripheral edges on a same surface of the base for making electrical connections to one or more metallized pads or contacts on the at least one partially fabricated semiconductor device through bonding wires, such that each of the plurality of metallized bonding pads is individually and electrically connected to a respective port on the chip carrier for in-situ monitoring of electrical parameters of the at least one partially fabricated semiconductor device during the CVD, wherein electrical currents or electrical signals are exchanged between the at least one partially fabricated semiconductor device and a source-measure unit (SMU) disposed external to the sealed chamber through a connector and wire harness that is electrically coupled to a plurality of ports on one peripheral edge of the chip carrier within the sealed chamber,
wherein the SMU comprises a plurality of measurement equipment configured to perform in-situ measurements of the electrical parameters of the at least one partially fabricated semiconductor device during the CVD.

### Claim 2 (depends on 1)

The system according to claim 1, wherein the chip carrier is made from a high melting point polymer comprising PolyTetraFluoroEthylene (PTFE).

### Claim 3 (depends on 1)

The system according to claim 1, wherein each of the metallized source pad and the metallized drain pad of one of the plurality of partially fabricated back-gated FETs is electrically connected through a respective bond wire to a corresponding metallized bonding pad disposed along the one peripheral edge of the base of the chip carrier, wherein each metallized bonding pad is electrically connected to a respective port on the chip carrier for mating to a respective jack or plug of the connector and wire harness.

### Claim 4 (depends on 3)

The system according to claim 3, wherein each of the metallized drain pad, the metallized source pad and a gate remains being shorted together on another peripheral edge of the chip carrier through connecting to a shorting piece during transport and when being connected to the connector and wire harness on the one peripheral edge of the chip carrier prior to electrical parameters measurements, wherein the shorting piece on the another peripheral edge of the chip carrier is to be first removed prior to proceeding with the electrical parameters measurements by the SMU.

### Claim 5 (depends on 1)

The system according to claim 1, wherein each of the plurality of metallized bonding pads disposed along both peripheral edges is electrically connected to each other as a pair through electrically connecting to a corresponding pair of ports which are disposed along both peripheral edges of the chip carrier.

### Claim 6 (depends on 1)

The system according to claim 1, wherein the at least one partially fabricated semiconductor devices comprise a plurality of partially fabricated back-gated Field-Effect Transistors (FETs) fabricated on a portion of a wafer, wherein each of the plurality of partially fabricated back-gated FETs having at least a metallized source pad and a metallized drain pad on a topside surface separated by a semiconductor channel, wherein a gate is disposed on a backside surface facing oppositely away from the source pad and the drain pad.

### Claim 7 (depends on 6)

The system according to claim 6, wherein when the CVD performs an atomic layer deposition (ALD), the channel that separates the source pad and the drain pad comprising at least one mono-layer crystal structure of MX2 of transition metal dichalcogenides (TMDs), wherein the mono-layer crystal structure of MX2 is formed by a layer of transition metal atom M sandwiched between two layers of chalcogen atom X, and the at least one mono-layer crystal structure of MX2, wherein the transition metal atom M is selected from one of: molybdenum (Mo) and Tungsten (W), and the chalcogen atom X is selected from one of: Sulfur (S), Selenium (Se) and Tellurium (Te).

### Claim 8 (depends on 7)

The system according to claim 7, wherein the at least one mono-layer crystal structure of MX2 comprises one of: MoS2 (molybdenum disulfide) and MoTe2 (molybdenum ditelluride).

### Claim 9 (depends on 8)

The system according to claim 8, wherein the ALD uses the reactive gases comprising water (H2O) and oxygen (O2) to form an oxide encapsulation as a dielectric layer to improve field effect mobility of the TMDs on unmasked area, wherein the oxide encapsulation comprises MoOx (molybdenum oxide).

### Claim 10 (depends on 1)

The system according to claim 1, wherein the in-situ measurements of the electrical parameters of the at least one partially fabricated semiconductor device during the CVD comprising measurements over a defined time period of: channel currents, transconductance, bias voltage, carrier mobility, oxide encapsulation thickness, chamber temperature, chamber pressure and flow rate of reactant gases.

### Claim 11

A method for in-situ monitoring of semiconductor devices during chemical vapor deposition, comprising:
disposing a chip carrier within a sealed chamber of a reactor for carrying out in-situ monitoring of semiconductor devices within the sealed chamber during chemical vapor deposition (CVD), wherein the reactor is configured with a plurality of openings for passaging of reactive gases and for in-situ monitoring of the semiconductor devices during the CVD,
wherein the chip carrier is configured for mounting at least one partially fabricated semiconductor device on a base, and
the chip carrier comprises a plurality of metallized bonding pads disposed along both peripheral edges on a same surface of the base for making electrical connections to one or more metallized pads or contacts on the at least one partially fabricated semiconductor device through bonding wires, such that each of the plurality of metallized bonding pads is individually and electrically connected to a respective port on the chip carrier for in-situ monitoring of electrical parameters of the at least one partially fabricated semiconductor device during the CVD, wherein electrical currents or electrical signals are exchanged between the at least one partially fabricated semiconductor device and a source-measure unit (SMU) disposed external to the sealed chamber through a connector and wire harness that is electrically coupled to a plurality of ports on one peripheral edge of the chip carrier within the sealed chamber; and
performing by a plurality of measurement equipment of the SMU, in-situ measurements of the electrical parameters of the at least one partially fabricated semiconductor device during the CVD.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the chip carrier is made from a high melting point polymer comprising PolyTetraFluoroEthylene (PTFE).

### Claim 13 (depends on 11)

The method according to claim 11, wherein each of the metallized source pad and the metallized drain pad of one of the plurality of partially fabricated back-gated FETs is electrically connected through a respective bond wire to a corresponding metallized bonding pad disposed along the one peripheral edge of the base of the chip carrier, wherein each metallized bonding pad is electrically connected to a respective port on the chip carrier for mating to a respective jack or plug of the connector and wire harness.

### Claim 14 (depends on 13)

The method according to claim 13, comprising:
shorting each of the metallized drain pad, the metallized source pad and a gate on another peripheral edge of the chip carrier through connecting to a shorting piece during transport and when being connected to the connector and wire harness on the one peripheral edge of the chip carrier prior to electrical parameters measurements; and
removing the shorting piece on the another peripheral edge of the chip carrier prior to proceeding with the electrical parameters measurements by the SMU.

### Claim 15 (depends on 11)

The method according to claim 11, wherein each of the plurality of metallized bonding pads disposed along both peripheral edges is electrically connected to each other as a pair through electrically connecting to a corresponding pair of ports which are disposed along both peripheral edges of the chip carrier.

### Claim 16 (depends on 11)

The method according to claim 11, wherein the at least one partially fabricated semiconductor devices comprise a plurality of partially fabricated back-gated Field-Effect Transistors (FETs) fabricated on a portion of a wafer, wherein each of the plurality of partially fabricated back-gated FETs having at least a metallized source pad and a metallized drain pad on a topside surface separated by a semiconductor channel, wherein a gate is disposed on a backside surface facing oppositely away from the source pad and the drain pad.

### Claim 17 (depends on 16)

The method according to claim 16, wherein when the CVD performs an atomic layer deposition (ALD), the channel that separates the source pad and the drain pad comprising at least one mono-layer crystal structure of MX2 of transition metal dichalcogenides (TMDs), wherein the mono-layer crystal structure of MX2 is formed by a layer of transition metal atom M sandwiched between two layers of chalcogen atom X, and the at least one mono-layer crystal structure of MX2, wherein the transition metal atom M is selected from one of: molybdenum (Mo) and Tungsten (W), and the chalcogen atom X is selected from one of: Sulfur (S), Selenium (Se) and Tellurium (Te).

### Claim 18 (depends on 17)

The method according to claim 17 wherein the at least one mono-layer crystal structure of MX2 comprises one of: MoS2 (molybdenum disulfide) and MoTe2 (molybdenum ditelluride).

### Claim 19 (depends on 18)

The method according to claim 18, wherein the ALD uses the reactive gases comprising water (H2O) and oxygen (O2) to form an oxide encapsulation as a dielectric layer to improve field effect mobility of the TMDs on unmasked area, wherein the oxide encapsulation comprises MoOx (molybdenum oxide).

### Claim 20 (depends on 11)

The method according to claim 11, wherein the in-situ measurements of the electrical parameters of the at least one partially fabricated semiconductor device during the CVD comprising measurements over a defined time period of: channel currents, transconductance, bias voltage, carrier mobility, oxide encapsulation thickness, chamber temperature, chamber pressure and flow rate of reactant gases.