# US 2021/0287932 A1 · Trench isolation structure and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0287932 A1
- Document ID: US20210287932A1
- Status: Published application
- Kind: A1
- Application number: 16/483,081
- Filed: 2018-07-03
- Published: 2021-09-16
- Earliest claimed: 2017-07-03
- Assignees: Csmc Technologies Fab2 Co., Ltd.
- Applicants: CSMC Technologies FAB2 Co., Ltd.
- Inventors: Shukun Ql
- Web page: https://patentgrep.com/patent/US20210287932A1

## CPC

- H10W 10/0145: {of trenches having shapes other than rectangular or V-shape (H10W10/0143 takes precedence)}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10D 62/114: {PN junction isolations}
- H10D 62/115: {Dielectric isolations, e.g. air gaps}
- H10P 14/61: using masks
- H10P 14/6308: {of Group IV semiconductors}
- H10P 14/6322: {Formation by thermal treatments (formation by plasma treatment H10P14/6319)}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/21: {of electrically active species}
- H10P 50/283: {by chemical means}
- H10P 95/062: {involving a dielectric removal step}
- H10W 10/0147: {the shapes being altered by a local oxidation of silicon process, e.g. trench corner rounding by LOCOS}
- H10W 10/0148: {comprising introducing impurities in side walls or bottom walls of trenches, e.g. for forming channel stoppers}
- H10W 10/031: {of isolation regions comprising PN junctions}
- H10W 10/30: Isolation regions comprising PN junctions
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for manufacturing a trench isolation structure comprising forming a shallow trench having a wider upper section and a narrower lower section in a wafer surface, removing part of the silicon oxide by etching, forming a silicon oxide corner structure at a corner at a top corner of the shallow trench by thermal oxidation, depositing silicon nitride on the wafer surface to cover surfaces of the shallow trench silicon oxide and the silicon oxide corner structure, dry etching the silicon nitride on the shallow trench silicon oxide surface thereby forming masking silicon nitride residues extending into the trench, etching downwards to form a deep trench, forming silicon oxide layers on a side wall and the bottom of the deep trench, depositing polycrystalline silicon in the shallow and deep trenches, removing the silicon nitride, and forming silicon oxide in the shallow trench to cover the polycrystalline silicon.

## Claims

### Claim 1

A method of manufacturing a trench isolation structure, comprising:
forming a first trench having a wide top and a narrow bottom on a surface of a wafer;
filling silicon oxide into the first trench by depositing;
removing a portion of a surface of the silicon oxide in the first trench by etching;
forming a silicon oxide corner structure at a corner of the top of the First trench by thermal oxidation, the silicon oxide corner structure being a structure in which the silicon oxide in the first trench gradually becomes thicker from the corner downward;
depositing a nitrogen-containing compound on the surface of the wafer to cover the surface of the silicon oxide in the first trench and a surface of the silicon oxide corner structure;
dry-etching the nitrogen-containing compound, removing the nitrogen-containing compound on the surface of the silicon oxide in the first trench, and forming a nitrogen-containing compound sidewall residue extending into the trench on the surface of the silicon oxide corner structure;
continuing etching the silicon oxide and the wafer downwardly using the nitrogen-containing compound sidewall residue, as a mask and forming a second trench;
forming a silicon oxide layer on a sidewall and a bottom of the second trench;
depositing polysilicon into the first trench and the second trench;
removing the nitrogen-containing compound sidewall residue; and
forming silicon oxide in the first trench to cover the polysilicon.

### Claim 2 (depends on 1)

The method according to claim 1, wherein tine first trench has a depth of 1 to 2 μm, and the second trench has a depth of 10 μm or more.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the step of forming the silicon oxide layer on the sidewall and the bottom of the second trench is performed by a thermal oxidation process, and the formed silicon oxide layer has a thickness of at least 1000 angstroms.

### Claim 4 (depends on 1)

The method according to claim 1, wherein after the step of forming the silicon oxide layer on the sidewall and the bottom of the second trench, prior to the step of depositing polysilicon into the first trench and the second trench, the method further comprises a step of implanting N type ions and P type ions into the second trench, respectively, and forming an N type ring and a P type ring around the bottom of the second trench.

### Claim 5 (depends on 1)

The method according to claim 1, wherein prior to the step of removing the nitrogen-containing compound sidewall residue, the method further comprises a step of etching the polysilicon to a position below the nitrogen-containing compound sidewall residue.

### Claim 6 (depends on 1)

The method according to claim 1, wherein prior to the step of filling silicon oxide into the first trench by depositing, the method further comprises a step of oxidizing a sidewall of the first trench.

### Claim 7 (depends on 1)

The method according to claim 1, wherein prior to the step of forming the first trench having the wide top and the narrow bottom on the surface of the wafer, the method further comprises a step of forming a silicon nitride layer on the surface of the wafer, and the step of forming the first trench having the wide top and the narrow bottom on the surface of the wafer is to etch through the silicon nitride layer to form the first trench.

### Claim 8 (depends on 1)

The method according to claim 1, wherein in the step of forming the silicon oxide corner structure at the corner of the top of the first trench by thermal oxidation, an oxidation temperature is from 800° C. to 950° C.

### Claim 9 (depends on 1)

The method according to claim 1, further comprising a step of epitaxially glowing of an epitaxial layer on a substrate by an epitaxial process, the epitaxial layer having a higher doping concentration than that of the substrate, wherein the step of forming the first trench on the surface of the, wafer is to form the first trench in the epitaxial layer.

### Claim 10 (depends on 1)

The method according to claim 1, wherein in the step of filling the silicon oxide into the first trench by depositing, the deposition of silicon oxide is performed by using a high-density plasma chemical vapor deposition process.

### Claim 11 (depends on 1)

The method according to claim 1, wherein after the step of filling the silicon oxide into the first trench by depositing, prior to the step of removing the portion of the surface of the silicon oxide in the first trench by etching, the method further comprises a step of removing the silicon oxide layer exposed outside the first trench by chemical mechanical polishing.

### Claim 12 (depends on 7)

The method according to claim 7, wherein after the step of filling the silicon oxide into the first trench by depositing, prior to the step of removing the portion of the surface of silicon oxide in the first trench by etching, the method further comprises a step of polishing the silicon oxide layer to the silicon nitride layer.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the step of removing the sidewall residue of the nitrogen-containing compound is performed by using concentrated phosphoric acid as an etchant.

### Claim 14 (depends on 1)

The method according to claim 1, wherein in the step of forming the silicon oxide in the first trench to cover the polysilicon, the deposition of silicon oxide is performed using a high-density plasma chemical, vapor deposition process.

### Claim 15 (depends on 1)

The method according to claim 1, wherein after the step of forming the silicon oxide in the first trench to cover the polysilicon, the method further comprises a step of flattening the silicon oxide exposed outside the first trench by chemical mechanical polishing.

### Claim 16 (depends on 1)

The method accord ng to claim 1, wherein the step of forming the first trench having the wide top and the narrow bottom on the surface of the wafer is to dry etch using CHCl3 and/or CH2Cl2 as an etchant.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the step of removing the portion of the surface of the silicon oxide in the first trench by etching is by dry-etching.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the step of removing the portion of the surface of the silicon oxide in the first trench by etching is performed using a high-density plasma etching process.

### Claim 19

A trench isolation structure, comprising:
a trench including a bottle mouth structure with a wide top and a narrow bottom and a bottle body structure extending downwardly from the bottle mouth structure;
silicon oxide filled in the trench; and
polysilicon located in the trench and surrounded by the silicon oxide.

### Claim 20 (depends on 19)

The trench isolation structure according to claim 19, further comprising an N type ring and a P type ring around a bottom of the bottle body structure, the P type ring being located above the N type ring.