# US 2021/0287905 A1 · Gate Structure Passivating Species Drive-In Method and Structure Formed Thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0287905 A1
- Document ID: US20210287905A1
- Status: Published application
- Kind: A1
- Application number: 17/334,255
- Filed: 2021-05-28
- Published: 2021-09-16
- Earliest claimed: 2017-09-28
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Hsiao-Kuan Wei; Hsien-Ming Lee; Chin-You Hsu; Hsin-Yun Hsu; Pin-Hsuan Yeh
- Web page: https://patentgrep.com/patent/US20210287905A1

## CPC

- H10D 64/0134: {with a treatment, e.g. annealing, after the formation of the insulator and before the formation of the conductor}
- H10D 64/01: Manufacture or treatment
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 64/667: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN workfunction layers (having lateral variation H10D64/671)}
- H10D 64/669: {the conductor further comprising additional layers of alloy material, compound material or organic material, e.g. TaN/TiAlN}
- H10D 64/683: {being parallel to the channel plane}
- H10D 64/685: {being perpendicular to the channel plane}
- H10P 14/43: Chemical deposition, e.g. chemical vapour deposition [CVD]
- H10P 14/6518: {by introduction of substances into an already-existing insulating layer}
- H10P 50/667: {by liquid etching only}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/62: Fin field-effect transistors [FinFET]
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 64/01318: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN (comprising a layer of alloys of Si, Ge or C H10D64/01314)}
- H10D 64/0132: {the conductor being a metallic silicide}
- H10P 14/418: {the conductive layers comprising transition metals}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Generally, the present disclosure provides example embodiments relating to formation of a gate structure of a device, such as in a replacement gate process, and the device formed thereby. In an example method, a gate dielectric layer is formed over an active area on a substrate. A dummy layer that contains a passivating species (such as fluorine) is formed over the gate dielectric layer. A thermal process is performed to drive the passivating species from the dummy layer into the gate dielectric layer. The dummy layer is removed. A metal gate electrode is formed over the gate dielectric layer. The gate dielectric layer includes the passivating species before the metal gate electrode is formed.

## Claims

### Claim 1

A method comprising:
forming a high-k gate dielectric layer over an active area on a substrate;
implanting the high-k gate dielectric layer with fluorine, the implanting the high-k gate dielectric layer comprising, in order:
forming a capping layer;
forming a barrier layer;
forming a dummy fluorine-containing layer, wherein the dummy fluorine-containing layer is formed by an atomic layer deposition process which utilizes a fluorine-containing precursor followed by a second precursor;
forming a capping layer;
performing a thermal process to drive fluorine from the dummy fluorine-containing layer into the high-k gate dielectric layer and from the dummy fluorine-containing layer into the capping layer, wherein the performing the thermal process reduces a concentration of fluorine within the barrier layer; and
removing the dummy fluorine-containing layer; and
forming a metal gate electrode over the high-k gate dielectric layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the forming the dummy fluorine-containing layer is performed at a temperature of about 300° C. for a duration of about 97 seconds.

### Claim 3 (depends on 1)

The method of claim 1, wherein the forming the capping layer is performed at a temperature of about 450° C. for a duration of about 175 seconds.

### Claim 4 (depends on 1)

The method of claim 1, wherein the performing the thermal process performs a rapid thermal anneal.

### Claim 5 (depends on 4)

The method of claim 4, wherein the rapid thermal anneal is performed at a temperature of about 575° C. for about 15 seconds.

### Claim 6 (depends on 1)

The method of claim 1, wherein the removing the dummy fluorine-containing layer is performed using a wet etch process with phosphoric acid (H3PO4).

### Claim 7

A method comprising:
conformally forming a high-k gate dielectric layer between gate spacers;
after the conformally forming the high-k gate dielectric layer, forming a barrier layer over the high-k gate dielectric layer;
after the forming the barrier layer, conformally depositing a dummy layer over the barrier layer;
after the conformally depositing the dummy layer, forming a dummy capping layer over the dummy layer;
after the forming the dummy capping layer, driving fluorine from the dummy layer into the high-k gate dielectric layer and also driving fluorine from the dummy layer into the dummy capping layer, wherein the driving the fluorine from the dummy layer into the high-k gate dielectric layer also reduces a concentration of fluorine in the barrier layer; and
after the driving the fluorine from the dummy layer into the high-k gate dielectric layer, removing the dummy layer.

### Claim 8 (depends on 7)

The method of claim 7, wherein the driving the fluorine from the dummy layer into the high-k gate dielectric layer is performed at least in part with a thermal process.

### Claim 9 (depends on 8)

The method of claim 8, wherein the thermal process is a rapid thermal anneal.

### Claim 10 (depends on 8)

The method of claim 8, wherein the thermal process is performed at least in part at a temperature between about 300° C. to about 600° C. for a duration between about 15 seconds to about 180 seconds.

### Claim 11 (depends on 7)

The method of claim 7, wherein the conformally depositing the dummy layer deposits fluorine-doped tungsten.

### Claim 12 (depends on 11)

The method of claim 11, wherein the conformally depositing the dummy layer utilizes a tungsten fluoride precursor and a diborane (B2H6) precursor.

### Claim 13 (depends on 11)

The method of claim 11, wherein the conformally depositing the dummy layer utilizes a tungsten fluoride precursor and an ethane (C2H6) precursor.

### Claim 14 (depends on 11)

The method of claim 11, wherein the conformally depositing the dummy layer utilizes a tungsten fluoride precursor and a silane (SiH4) precursor.

### Claim 15

A method comprising:
forming a gate dielectric layer over a substrate;
depositing a first capping layer over the gate dielectric layer;
depositing a dummy fluorine-containing layer with an atomic layer deposition process over the first capping layer, wherein the dummy fluorine-containing layer comprises a first material and fluorine, wherein the fluorine is deposited with the first material, and wherein during the depositing the dummy fluorine-containing layer fluorine diffuses into the gate dielectric layer;
depositing a dummy capping layer over the dummy fluorine-containing layer, wherein during the depositing the dummy capping layer fluorine diffuses from the dummy fluorine-containing layer into the gate dielectric layer;
performing an anneal, the performing the anneal reducing a concentration of fluorine in a portion of the first capping layer, the performing the anneal further diffusing fluorine from the dummy fluorine-containing layer into the dummy capping layer;
removing the dummy fluorine-containing layer; and
forming a metal gate electrode over the gate dielectric layer, wherein each of the steps recited herein is performed in the recited order.

### Claim 16 (depends on 15)

The method of claim 15, wherein the depositing the dummy fluorine-containing layer deposits the dummy fluorine-containing layer to a thickness in a range from about 5 Å to about 50 Å.

### Claim 17 (depends on 15)

The method of claim 15, wherein the depositing the dummy fluorine-containing layer deposits the dummy fluorine-containing layer with a fluorine concentration of less than about 1 percent.

### Claim 18 (depends on 15)

The method of claim 15, wherein the depositing the dummy capping layer deposits titanium nitride.

### Claim 19 (depends on 15)

The method of claim 15, wherein the depositing the dummy capping layer deposits the dummy capping layer to a thickness of between about 5 Å and about 30 Å.

### Claim 20 (depends on 15)

The method of claim 15, wherein the depositing the dummy fluorine-containing layer deposits fluorine-doped tungsten.