# US 2021/0287834 A1 · Grain-oriented magnetic steel sheets having chromium-free insulating tension coating, and methods for producing such steel sheets

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0287834 A1
- Document ID: US20210287834A1
- Status: Published application
- Kind: A1
- Application number: 16/324,211
- Filed: 2017-09-08
- Published: 2021-09-16
- Earliest claimed: 2016-09-13
- Assignees: Jfe Steel Corporation
- Applicants: JFE Steel Corporation
- Inventors: Souichiro Yoshizaki; Makoto Watanabe; Ryuichi Suehiro
- Web page: https://patentgrep.com/patent/US20210287834A1

## CPC

- H01F 1/18: with insulating coating
- C21D 8/1283: {Application of a separating or insulating coating}
- C21D 8/1288: {Application of a tension-inducing coating}
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C23C 22/08: Orthophosphates
- C23C 22/12: containing zinc cations
- C23C 22/13: containing also nitrate or nitrite anions
- C23C 22/18: containing manganese cations
- C23C 22/188: {containing also magnesium cations}
- C23C 22/20: containing aluminium cations
- C23C 22/22: containing alkaline earth metal cations
- C23C 22/74: for obtaining burned-in conversion coatings
- H01F 1/147: Alloys characterised by their composition {(treatment thereof for enhancing their electromagnetic properties C21D8/12)}
- C21D 2201/05: Grain orientation
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A grain-oriented magnetic steel sheet with chromium-free insulating tension coating includes a grain-oriented magnetic steel sheet and an insulating tension coating containing a phosphate salt and silica on a surface of the grain-oriented magnetic steel sheet, the coating further including a crystalline compound represented by the general formula (1): MII3MIII4(XVO4)6 . . . (1). A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating includes applying an insulating tension coating liquid to a surface of a finish annealed grain-oriented magnetic steel sheet, the coating liquid including colloidal silica, a phosphate salt and a metal element M-containing compound in a specific ratio, and heat treating the steel sheet at least one time at a temperature of not less than 900° C. in an atmosphere including a non-oxidizing gas and having a dew point of not more than 0° C.

## Claims

### Claim 1

A grain-oriented magnetic steel sheet with chromium-free insulating tension coating, comprising a grain-oriented magnetic steel sheet and an insulating tension coating containing a phosphate salt and silica on at least one side of the grain-oriented magnetic steel sheet, the coating further including a crystalline compound represented by the general formula (1) below:
MII3MIII4(XVO4)6 (1)
in the general formula (1), MII and MIII are each independently one, or two or more selected from Sc, Ti, V, Mn, Fe, Co, Ni, Cu and Mg, and XV is one, or two or more selected from P, V and Mo.

### Claim 2 (depends on 1)

The grain-oriented magnetic steel sheet with chromium-free insulating tension coating according to claim 1, wherein MIII is Fe and Xv is P in the general formula (1).

### Claim 3 (depends on 1)

The grain-oriented magnetic steel sheet with chromium-free insulating tension coating according to claim 1, wherein the crystalline compound represented by the general formula (1) is Fe7(PO4)6.

### Claim 4 (depends on 2)

The grain-oriented magnetic steel sheet with chromium-free insulating tension coating according to claim 2, wherein the crystalline compound represented by the general formula (1) is Fe7 (PO4)6.

### Claim 5 (depends on 1)

The grain-oriented magnetic steel sheet with chromium-free insulating tension coating according to claim 1, wherein the phosphate salt is one, or two or more selected from phosphate salts of Mg, Fe, Al, Ca, Mn and Zn.

### Claim 6 (depends on 2)

The grain-oriented magnetic steel sheet with chromium-free insulating tension coating according to claim 2, wherein the phosphate salt is one, or two or more selected from phosphate salts of Mg, Fe, Al, Ca, Mn and Zn.

### Claim 7 (depends on 3)

The grain-oriented magnetic steel sheet with chromium-free insulating tension coating according to claim 3, wherein the phosphate salt is one, or two or more selected from phosphate salts of Mg, Fe, Al, Ca, Mn and Zn.

### Claim 8 (depends on 4)

The grain-oriented magnetic steel sheet with chromium-free insulating tension coating according to claim 4, wherein the phosphate salt is one, or two or more selected from phosphate salts of Mg, Fe, Al, Ca, Mn and Zn.

### Claim 9 (depends on 1)

A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating described in claim 1, comprising:
applying an insulating tension coating liquid to at least one side of a finish annealed grain-oriented magnetic steel sheet, the coating liquid comprising 20 parts by mass in terms of solid of colloidal silica, 10 to 80 parts by mass of a phosphate salt and 5 to 10 parts by mass in terms of oxide of a metal element M-containing compound (the metal element M is one, or two or more selected from Sc, Ti, V, Mn, Fe, Co, Ni, Cu and Mg), and heat treating the steel sheet at least one time at a temperature of not less than 900° C. in an atmosphere including a non-oxidizing gas and having a dew point of not more than 0° C.

### Claim 10 (depends on 2)

A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating described in claim 2, comprising:
applying an insulating tension coating liquid to at least one side of a finish annealed grain-oriented magnetic steel sheet, the coating liquid comprising 20 parts by mass in terms of solid of colloidal silica, 10 to 80 parts by mass of a phosphate salt and 5 to 10 parts by mass in terms of oxide of a metal element M-containing compound (the metal element M is one, or two or more selected from Sc, Ti, V, Mn, Fe, Co, Ni, Cu and Mg), and heat treating the steel sheet at least one time at a temperature of not less than 900° C. in an atmosphere including a non-oxidizing gas and having a dew point of not more than 0° C.

### Claim 11 (depends on 3)

A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating described in claim 3, comprising:
applying an insulating tension coating liquid to at least one side of a finish annealed grain-oriented magnetic steel sheet, the coating liquid comprising 20 parts by mass in terms of solid of colloidal silica, 10 to 80 parts by mass of a phosphate salt and 5 to 10 parts by mass in terms of oxide of a metal element M-containing compound (the metal element M is one, or two or more selected from Sc, Ti, V, Mn, Fe, Co, Ni, Cu and Mg), and heat treating the steel sheet at least one time at a temperature of not less than 900° C. in an atmosphere including a non-oxidizing gas and having a dew point of not more than 0° C.

### Claim 12 (depends on 4)

A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating described in claim 4, comprising:
applying an insulating tension coating liquid to at least one side of a finish annealed grain-oriented magnetic steel sheet, the coating liquid comprising 20 parts by mass in terms of solid of colloidal silica, 10 to 80 parts by mass of a phosphate salt and 5 to 10 parts by mass in terms of oxide of a metal element M-containing compound (the metal element M is one, or two or more selected from Sc, Ti, V, Mn, Fe, Co, Ni, Cu and Mg), and heat treating the steel sheet at least one time at a temperature of not less than 900° C. in an atmosphere including a non-oxidizing gas and having a dew point of not more than 0° C.

### Claim 13 (depends on 5)

A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating described in claim 5, comprising:
applying an insulating tension coating liquid to at least one side of a finish annealed grain-oriented magnetic steel sheet, the coating liquid comprising 20 parts by mass in terms of solid of colloidal silica, 10 to 80 parts by mass of a phosphate salt and 5 to 10 parts by mass in terms of oxide of a metal element M-containing compound (the metal element M is one, or two or more selected from Sc, Ti, V, Mn, Fe, Co, Ni, Cu and Mg), and heat treating the steel sheet at least one time at a temperature of not less than 900° C. in an atmosphere including a non-oxidizing gas and having a dew point of not more than 0° C.

### Claim 14 (depends on 6)

A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating described in claim 6, comprising:
applying an insulating tension coating liquid to at least one side of a finish annealed grain-oriented magnetic steel sheet, the coating liquid comprising 20 parts by mass in terms of solid of colloidal silica, 10 to 80 parts by mass of a phosphate salt and 5 to 10 parts by mass in terms of oxide of a metal element M-containing compound (the metal element M is one, or two or more selected from Sc, Ti, V, Mn, Fe, Co, Ni, Cu and Mg), and heat treating the steel sheet at least one time at a temperature of not less than 900° C. in an atmosphere including a non-oxidizing gas and having a dew point of not more than 0° C.

### Claim 15 (depends on 7)

A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating described in claim 7, comprising:
applying an insulating tension coating liquid to at least one side of a finish annealed grain-oriented magnetic steel sheet, the coating liquid comprising 20 parts by mass in terms of solid of colloidal silica, 10 to 80 parts by mass of a phosphate salt and 5 to 10 parts by mass in terms of oxide of a metal element M-containing compound (the metal element M is one, or two or more selected from Sc, Ti, V, Mn, Fe, Co, Ni, Cu and Mg), and heat treating the steel sheet at least one time at a temperature of not less than 900° C. in an atmosphere including a non-oxidizing gas and having a dew point of not more than 0° C.

### Claim 16 (depends on 8)

A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating described in claim 8, comprising:
applying an insulating tension coating liquid to at least one side of a finish annealed grain-oriented magnetic steel sheet, the coating liquid comprising 20 parts by mass in terms of solid of colloidal silica, 10 to 80 parts by mass of a phosphate salt and 5 to 10 parts by mass in terms of oxide of a metal element M-containing compound (the metal element M is one, or two or more selected from Sc, Ti, V, Mn, Fe, Co, Ni, Cu and Mg), and heat treating the steel sheet at least one time at a temperature of not less than 900° C. in an atmosphere including a non-oxidizing gas and having a dew point of not more than 0° C.

### Claim 17 (depends on 1)

A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating described in claim 1, comprising:
applying an insulating tension coating liquid to at least one side of a finish annealed grain-oriented magnetic steel sheet, the coating liquid comprising 20 parts by mass in terms of solid of colloidal silica, 10 to 80 parts by mass of a phosphate salt, and an amount of a crystalline compound represented by the general formula (1), and heat treating the steel sheet at least one time in a non-oxidizing atmosphere.

### Claim 18 (depends on 2)

A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating described in claim 2, comprising:
applying an insulating tension coating liquid to at least one side of a finish annealed grain-oriented magnetic steel sheet, the coating liquid comprising 20 parts by mass in terms of solid of colloidal silica, 10 to 80 parts by mass of a phosphate salt, and an amount of a crystalline compound represented by the general formula (1), and heat treating the steel sheet at least one time in a non-oxidizing atmosphere.

### Claim 19 (depends on 3)

A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating described in claim 3, comprising:
applying an insulating tension coating liquid to at least one side of a finish annealed grain-oriented magnetic steel sheet, the coating liquid comprising 20 parts by mass in terms of solid of colloidal silica, 10 to 80 parts by mass of a phosphate salt, and an amount of a crystalline compound represented by the general formula (1), and heat treating the steel sheet at least one time in a non-oxidizing atmosphere.

### Claim 20 (depends on 4)

A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating described in claim 4, comprising:
applying an insulating tension coating liquid to at least one side of a finish annealed grain-oriented magnetic steel sheet, the coating liquid comprising 20 parts by mass in terms of solid of colloidal silica, 10 to 80 parts by mass of a phosphate salt, and an amount of a crystalline compound represented by the general formula (1), and heat treating the steel sheet at least one time in a non-oxidizing atmosphere.