# US 2021/0286257 A1 · Pellicle

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0286257 A1
- Document ID: US20210286257A1
- Status: Published application
- Kind: A1
- Application number: 17/332,463
- Filed: 2021-05-27
- Published: 2021-09-16
- Earliest claimed: 2018-12-03
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Applicants: Shin-Etsu Chemical Co., Ltd.
- Inventors: Yu YANASE
- Web page: https://patentgrep.com/patent/US20210286257A1

## CPC

- G03F 1/64: characterised by the frames, e.g. structure or material, including bonding means therefor
- G03F 1/62: Pellicles, e.g. pellicle assemblies, e.g. having membrane on support frame; Preparation thereof
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A pellicle characterized by having an amount of released aqueous gas of 1×10−3 Pa·L/s or less per pellicle, an amount of released hydrocarbon-based gas of 1×10−5 Pa·L/s or less per pellicle in a range of measured mass number of 45 to 100 amu, and an amount of released hydrocarbon-based gas of 4×10−7 Pa·L/s or less per pellicle in a range of measured mass number of 101 to 200 amu, under vacuum after the pellicle has been left to stand for 10 minutes in an atmosphere of 23° C. and 1×10−3 Pa or less.

## Claims

### Claim 1

A method for preventing a contamination formed from an outgas and deposited onto an inner wall surface of an exposure device, the method comprising a step of
performing exposure by using a pellicle in the exposure device, wherein the pellicle has an amount of released aqueous gas of 1×10−3 Pa·L/s or less per pellicle in a range of measured mass number of 1, 2, 17, and 18 amu, an amount of released hydrocarbon-based gas of 1×10−5 Pa·L/s or less per pellicle in a range of measured mass number of 45 to 100 amu, and an amount of released hydrocarbon-based gas of 4×10−7 Pa·L/s or less per pellicle in a range of measured mass number of 101 to 200 amu, under vacuum after the pellicle being left to stand for 10 minutes in an atmosphere of 23° C. and 1×10−3 Pa or less.

### Claim 2 (depends on 1)

The method of claim 1, wherein the amount of released aqueous gas in the range of measured mass number of 1, 2, 17, and 18 amu is 8.5×10−4 Pa·L/s or less per the pellicle.

### Claim 3 (depends on 1)

The method of claim 1, wherein the amount of released hydrocarbon-based gas in a range of measured mass number of 45 to 100 amu is 8.9×10−6 Pa·L/s or less per pellicle.

### Claim 4 (depends on 1)

The method of claim 1, wherein the amount of released hydrocarbon-based gas in a range of measured mass number of 101 to 200 amu is 3.5×10−6 Pa·L/s or less per pellicle.

### Claim 5 (depends on 1)

The method of claim 1, wherein the pellicle has a pellicle film and a pellicle frame, and the pellicle film is arranged on an upper end face of the pellicle frame with an adhesive agent or a pressure-sensitive adhesive agent interposed therebetween.

### Claim 6 (depends on 5)

The method of claim 5, wherein a pressure-sensitive adhesive agent is arranged on a lower end face of the pellicle frame.

### Claim 7 (depends on 5)

The method of claim 5, wherein the adhesive agent or the pressure-sensitive adhesive agent arranged on the upper end face of the pellicle frame is a silicone-based adhesive agent, a silicone-based pressure-sensitive adhesive agent, or an epoxy-based adhesive agent.

### Claim 8 (depends on 6)

The method of claim 6, wherein the pressure-sensitive adhesive agent arranged on the lower end face of the pellicle frame is an acrylic pressure-sensitive adhesive agent or a silicone-based pressure-sensitive adhesive agent.

### Claim 9 (depends on 6)

The method of claim 6, wherein the adhesive agent or the pressure-sensitive adhesive agent arranged on the upper end face of the pellicle frame is a silicone-based adhesive agent or a silicone-based pressure-sensitive adhesive agent, and the pressure-sensitive adhesive agent arranged on the lower end face of the pellicle frame is a silicone-based pressure-sensitive adhesive agent.

### Claim 10 (depends on 5)

The method of claim 5, wherein the pellicle film is a silicon film or a carbon film.

### Claim 11 (depends on 5)

The method of claim 5, wherein the material of the pellicle frame is selected from the group consisting of quartz, invar, titanium and ceramic.

### Claim 12 (depends on 1)

The method of claim 1, the exposure device is used for EUV lithography.

### Claim 13 (depends on 1)

The method of claim 1, the exposure device is the device using a reflection mirror.

### Claim 14

An exposure method, comprising a step of performing exposure by using a pellicle in an exposure device, while preventing a contamination formed from an outgas and deposited onto an inner wall surface of the exposure device, wherein the pellicle has an amount of released aqueous gas of 1×10−3 Pa·L/s or less per pellicle in a range of measured mass number of 1, 2, 17, and 18 amu, an amount of released hydrocarbon-based gas of 1×10−5 Pa·L/s or less per pellicle in a range of measured mass number of 45 to 100 amu, and an amount of released hydrocarbon-based gas of 4×10−7 Pa·L/s or less per pellicle in a range of measured mass number of 101 to 200 amu, under vacuum after the pellicle being left to stand for 10 minutes in an atmosphere of 23° C. and 1×10−3 Pa or less.

### Claim 15 (depends on 14)

The exposure method of claim 14, wherein the exposure is an exposure based on EUV lithography.

### Claim 16

A method for manufacturing a semiconductor comprising a step of performing exposure by using a pellicle in an exposure device, while preventing a contamination formed from an outgas and deposited onto an inner wall surface of the exposure device, wherein the pellicle has an amount of released aqueous gas of 1×10−3 Pa·L/s or less per pellicle in a range of measured mass number of 1, 2, 17, and 18 amu, an amount of released hydrocarbon-based gas of 1×10−5 Pa·L/s or less per pellicle in a range of measured mass number of 45 to 100 amu, and an amount of released hydrocarbon-based gas of 4×10−7 Pa·L/s or less per pellicle in a range of measured mass number of 101 to 200 amu, under vacuum after the pellicle being left to stand for 10 minutes in an atmosphere of 23° C. and 1×10−3 Pa or less.

### Claim 17 (depends on 16)

The method for manufacturing a semiconductor of claim 16, wherein the exposure is performed in an EUV lithography.

### Claim 18

A method for reducing an outgas generated from a pellicle during a lithography in an exposure device, the method comprising the steps of:
providing the pellicle in an exposure device; and
conducting exposure through the pellicle during a lithography in the exposure device, wherein the pellicle has an amount of released aqueous gas of 1×10−3 Pa·L/s or less per pellicle in a range of measured mass number of 1, 2, 17, and 18 amu, an amount of released hydrocarbon-based gas of 1×10−5 Pa·L/s or less per pellicle in a range of measured mass number of 45 to 100 amu, and an amount of released hydrocarbon-based gas of 4×10−7 Pa·L/s or less per pellicle in a range of measured mass number of 101 to 200 amu, under vacuum after the pellicle being left to stand for 10 minutes in an atmosphere of 23° C. and 1×10−3 Pa or less.