# US 2021/0286254 A1 · Mask blank, transfer mask, and method for manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0286254 A1
- Document ID: US20210286254A1
- Status: Published application
- Kind: A1
- Application number: 17/331,955
- Filed: 2021-05-27
- Published: 2021-09-16
- Earliest claimed: 2017-06-14
- Assignees: Hoya Corporation
- Applicants: Hoya Corporation
- Inventors: Masahiro HASHIMOTO; Hiroaki SHISHIDO
- Web page: https://patentgrep.com/patent/US20210286254A1

## CPC

- G03F 1/32: Attenuating PSM [att-PSM], e.g. halftone PSM or PSM having semi-transparent phase shift portion,; Preparation thereof
- G03F 1/58: having two or more different absorber layers, e.g. stacked multilayer absorbers
- G03F 7/20: Exposure; Apparatus therefor (photographic printing apparatus for making copies G03B27/00)
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- H10P 76/4085: {characterised by the processes involved to create the masks}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

This mask blank has a structure wherein a phase shift film and a light shielding film are sequentially formed as layers in this order on a transparent substrate. The optical density of the layered structure composed of the phase shift film and the light shielding film with respect to exposure light, which is an ArF excimer laser, is 3.5 or more; and the light shielding film has a structure wherein a lower layer and an upper layer are formed as layers sequentially from the transparent substrate side. The lower layer is formed from a material wherein the total content of chromium, oxygen, nitrogen and carbon is 90 atomic % or more; and the upper layer is formed from a material wherein the total content of metals and silicon is 80 atomic % or more. The extinction coefficient kU of the upper layer for the exposure light is higher than the extinction coefficient kL of the lower layer for the exposure light.

## Claims

### Claim 1

A mask blank comprising:
a substrate; and
first and second films formed on the substrate;
wherein the first film is closer to the substrate than the second film is, and
wherein a total content of chromium, oxygen, nitrogen, and carbon in the first film is at least 90 atomic %, and
wherein a content of chromium in the first film is at least 50 atomic %, and
wherein the second film contains metal and silicon, and a total content of metal and silicon is at least 80 atomic %, and
wherein an extinction coefficient kU of the second film with respect to light having a wavelength of 193 nm is greater than an extinction coefficient kL of the first film with respect to light having a wavelength of 193 nm.

### Claim 2 (depends on 1)

The mask blank according to claim 1, wherein the extinction coefficient kL of the first film is at most 2.0, and
wherein the extinction coefficient kU of the second film is greater than 2.0.

### Claim 3 (depends on 1)

The mask blank according to claim 1, wherein a refractive index nu of the second film with respect to light having a wavelength of 193 nm is less than a refractive index nL of the first film with respect to light having a wavelength of 193 nm, and
wherein a ratio nU/nL of the refractive index nU of the second film to the refractive index nL of the first film is at least 0.8.

### Claim 4 (depends on 3)

The mask blank according to claim 3, wherein the refractive index nL of the first film is at most 2.0, and
wherein the refractive index nU of the second film is less than 2.0.

### Claim 5 (depends on 1)

The mask blank according to claim 1, wherein a total content of chromium, oxygen, and carbon in the first film is at least 90 atomic %.

### Claim 6 (depends on 1)

The mask blank according to claim 1, wherein a content [atomic %] of metal in the second film is at least five percent of the total content [atomic %] of metal and silicon in the second film.

### Claim 7 (depends on 1)

The mask blank according to claim 1, wherein the second film contains tantalum as the metal, and
wherein a total content of tantalum and silicon in the second film is at least 80 atomic %.

### Claim 8

A transfer mask comprising:
a substrate; and
first and second films formed on the substrate, each of the first and second films having a transfer pattern;
wherein the first film is closer to the substrate than the second film is, and
wherein a total content of chromium, oxygen, nitrogen, and carbon in the first film is at least 90 atomic %, and
wherein a content of chromium in the first film is at least 50 atomic %, and
wherein the second film contains metal and silicon, and a total content of metal and silicon is at least 80 atomic %, and
wherein an extinction coefficient kU of the second film with respect to light having a wavelength of 193 nm is greater than an extinction coefficient kL of the first film with respect to light having a wavelength of 193 nm.

### Claim 9 (depends on 8)

The transfer mask according to claim 8, wherein the extinction coefficient kL of the first film is at most 2.0; and
wherein the extinction coefficient kU of the second film is greater than 2.0.

### Claim 10 (depends on 8)

The transfer mask according to claim 8, wherein a refractive index nU of the second film with respect to light having a wavelength of 193 nm is less than a refractive index nL of the first film with respect to light having a wavelength of 193 nm, and
wherein a ratio nU/nL of the refractive index nU of the second film to the refractive index nL of the first film is at least 0.8.

### Claim 11 (depends on 8)

The transfer mask according to claim 8, wherein the refractive index nL of the first film is at most 2.0, and
wherein the refractive index nU of the second film is less than 2.0.

### Claim 12 (depends on 8)

The transfer mask according to claim 8, wherein a total content of chromium, oxygen, and carbon in the first film is at least 90 atomic %.

### Claim 13 (depends on 8)

The transfer mask according to claim 8, wherein a content [atomic %] of metal in the second film is at least five percent of the total content [atomic %] of metal and silicon in the second film.

### Claim 14 (depends on 8)

The transfer mask according to claim 8, wherein the second film contains tantalum as the metal, and
wherein a total content of tantalum and silicon in the second film is at least 80 atomic %.

### Claim 15

A method for manufacturing a semiconductor device, comprising transferring a transfer pattern by exposure to a resist film on a semiconductor substrate using a transfer mask comprising:
a substrate; and
first and second films formed on the substrate, each of the first and second films having a transfer pattern;
wherein the first film is closer to the substrate than the second film is, and
wherein a total content of chromium, oxygen, nitrogen, and carbon in the first film is at least 90 atomic %, and
wherein a content of chromium in the first film is at least 50 atomic %, and
wherein the second film contains metal and silicon, and a total content of metal and silicon is at least 80 atomic %, and
wherein an extinction coefficient kU of the second film with respect to light having a wavelength of 193 nm is greater than an extinction coefficient kL of the first film with respect to light having a wavelength of 193 nm.