# US 2021/0285876 A1 · Method for determining the anionic charge density of a polymer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0285876 A1
- Document ID: US20210285876A1
- Status: Published application
- Kind: A1
- Application number: 16/477,058
- Filed: 2017-12-15
- Published: 2021-09-16
- Earliest claimed: 2017-01-31
- Assignees: S.P.C.M. SA
- Applicants: S.P.C.M. SA
- Inventors: Cédrick FAVERO; Olivier BRAUN; Renaud SOUZY; Arthur MARAIS; Thomas BRICHART
- Web page: https://patentgrep.com/patent/US20210285876A1

## CPC

- C09K 8/528: inorganic depositions, e.g. sulfates or carbonates
- G01N 21/6408: {with measurement of decay time, time resolved fluorescence}
- G01N 21/643: {non-biological material}
- G01N 33/2835: {Specific substances contained in the oils or fuels}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

The present invention relates to a method for determining the anionic charge density of at least one polymer present in a sample, according to the following steps: bringing the at least one polymer present in the sample into contact with, and enabling the interaction thereof with, a developer solution comprising lanthanide (III) ions, exciting the sample at an excitation wavelength λexc and detecting, by time-resolved photoluminescence, a signal originating from the lanthanide (III) ions that have interacted with the at least one polymer at an emission wavelength λem, and determining the anionic charge density of the at least one polymer of the sample using the signal detected at the emission wavelength λem.

## Claims

### Claim 1

A method for determining the anionic charge density of at least one polymer present in a sample, the method comprising the following steps:
bringing the at least one polymer present in the sample into contact with, and enabling its interaction with, a developer solution comprising lanthanide (III) ions,
exciting the sample at an excitation wavelength of λexc and detecting, by time-resolved photoluminescence, a signal originating from the lanthanide (III) ions that have interacted with the at least one polymer at an emission wavelength λem, and
determining the anionic charge density of the at least one polymer in the sample using the signal detected at the emission wavelength λem.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the sample comes from production water from an oil or gas recovery process.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the time-resolved photoluminescence is time-resolved fluorescence.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the at least one polymer present in the sample is a polymer of at least one water-soluble anionic monomer and at least one non-ionic monomer (A) and, optionally, of at least one cationic or zwitterionic monomer.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the lanthanide ions are chosen from europium, terbium, samarium and dysprosium ions.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the lanthanide ions are europium or terbium ions.

### Claim 7 (depends on 1)

The method according to claim 1, wherein an amount of lanthanide (III) ions between 1 ppm and 10,000 ppm is added to the sample by weight based on the weight of the sample before the sample comes into contact with the developer solution.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the excitation wavelength λexc lies between 200 nm and 600 nm and the emission signal wavelength λem lies between 300 nm and 800 nm.

### Claim 9 (depends on 1)

The method according to claim 1, wherein a signal modifier comprising a cationic compound is added to the sample before the sample is excited.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the method comprises a sample purification step prior to adding the developer solution comprising the lanthanide (III) ions.

### Claim 11 (depends on 10)

The method according to claim 10, wherein an amount of lanthanide (III) ions between 1 ppm and 10,000 ppm is added to the sample by weight based on the weight of the sample before the sample comes into contact with the developer solution.

### Claim 12 (depends on 3)

The method according to claim 3, wherein the at least one polymer present in the sample is a polymer of at least one water-soluble anionic monomer and at least one non-ionic monomer (A) and, optionally, of at least one cationic or zwitterionic monomer.

### Claim 13 (depends on 4)

The method according to claim 4, wherein the lanthanide ions are chosen from europium, terbium, samarium and dysprosium ions.

### Claim 14 (depends on 4)

The method according to claim 4, wherein the lanthanide ions are europium or terbium ions.

### Claim 15 (depends on 4)

The method according to claim 4, wherein the excitation wavelength λexc lies between 200 nm and 600 nm and the emission signal wavelength λem lies between 300 nm and 800 nm.

### Claim 16 (depends on 4)

The method according to claim 4, wherein an amount of lanthanide (III) ions between 1 ppm and 10,000 ppm is added to the sample by weight based on the weight of the sample before the sample comes into contact with the developer solution.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the excitation wavelength λexc lies between 200 nm and 600 nm and the emission signal wavelength λem lies between 300 nm and 800 nm.

### Claim 18 (depends on 4)

The method according to claim 4, wherein the method comprises a sample purification step prior to adding the developer solution comprising the lanthanide (III) ions.

### Claim 19 (depends on 4)

The method according to claim 4, wherein a signal modifier comprising a cationic compound is added to the sample before the sample is excited.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the method comprises a sample purification step prior to adding the developer solution comprising the lanthanide (III) ions.