# US 2021/0282253 A1 · Manufacturing method of esd protection device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0282253 A1
- Document ID: US20210282253A1
- Status: Published application
- Kind: A1
- Application number: 17/327,783
- Filed: 2021-05-24
- Published: 2021-09-09
- Earliest claimed: 2018-05-25
- Assignees: Industrial Technology Research Institute
- Applicants: Industrial Technology Research Institute
- Inventors: Ding-Shiang Wang; Jia-Jen Chang; Ming-Sheng Leu; Tai-Sheng Chen; Chin-Te Shih
- Web page: https://patentgrep.com/patent/US20210282253A1

## CPC

- H10P 72/1902: {specially adapted for a single substrate}
- B65G 47/74: Feeding, transfer, or discharging devices of particular kinds or types
- C23C 14/0021: {Reactive sputtering or evaporation}
- C23C 14/022: {by means of bombardment with energetic particles or radiation}
- C23C 14/024: {Deposition of sublayers, e.g. to promote adhesion of the coating (C23C14/027 takes precedence)}
- C23C 14/083: {of refractory metals or yttrium}
- C23C 14/14: Metallic material, boron or silicon
- C23C 14/325: {Electric arc evaporation}
- H10P 72/1911: {characterised by materials, roughness, coatings or the like}
- H10P 72/1928: {characterised by the presence of antistatic elements}
- H05F 3/04: by means of spark gaps or other discharge devices (devices providing for corona discharge per se H01T19/00)
- H10P 72/123: {characterised by a material, a roughness, a coating or the like}
- H10P 72/135: {characterised by a material, a roughness, a coating or the like}
- H10P 72/145: {characterised by a material, a roughness, a coating or the like}
- H10P 72/155: {characterised by a material, a roughness, a coating or the like}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B65G: TRANSPORT OR STORAGE DEVICES, e.g. CONVEYORS FOR LOADING OR TIPPING, SHOP CONVEYOR SYSTEMS OR PNEUMATIC TUBE CONVEYORS (packaging B65B; handling thin or filamentary materials, e.g. paper sheets or thread, B65H; cranes B66C; portable mobile or lifting or hauling appliances, e.g. hoists, B66D; devices for lifting or lowering goods for loading or unloading purposes, e.g. fork-lift trucks, B66F9/00; emptying bottles, jars, casks, barrels or similar containers, not otherwise provided for, B67C9/00; delivering or transferring liquids B67D; filling or discharging vessels for liquefied, solidified or compressed gases F17C; pipe-line systems for fluids F17D)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H05F: STATIC ELECTRICITY; NATURALLY-OCCURRING ELECTRICITY

## Abstract

A manufacturing method of the ESD protection device includes the following steps. A surface treatment is performed on the substrate. A link layer is formed on the substrate after the surface treatment, wherein a material of the link layer includes a metal material. A progressive layer is formed on the link layer, wherein a material of the progressive layer includes a non-stoichiometric metal oxide material, and an oxygen concentration in the non-stoichiometric metal oxide material is increased gradually away from the substrate in a thickness direction of the progressive layer. A composite layer is formed on the progressive layer, wherein the composite layer includes a stoichiometric metal oxide material and a non-stoichiometric metal oxide material, and a ratio of the non-stoichiometric metal oxide material and the stoichiometric metal oxide material in the composite layer may make a sheet resistance value of the composite layer 1×107 to 1×108 Ω/sq.

## Claims

### Claim 1

A manufacturing method of an ESD protection device comprising the following steps:
A. performing a surface treatment on a substrate;
B. forming a link layer on the substrate after the surface treatment, wherein a material of the link layer comprises a metal material;
C. forming a progressive layer on the link layer, wherein a material of the progressive layer comprises a non-stoichiometric metal oxide material, and an oxygen concentration in the non-stoichiometric metal oxide material is increased gradually away from the substrate in a thickness direction of the progressive layer; and
D. forming a composite layer on the progressive layer, wherein the composite layer comprises a stoichiometric metal oxide material and a non-stoichiometric metal oxide material, and a ratio of the non-stoichiometric metal oxide material and the stoichiometric metal oxide material in the composite layer may make a sheet resistance value of the composite layer 1×107 Ω/sq to 1×108 Ω/sq.

### Claim 2 (depends on 1)

The manufacturing method of the ESD protection device of claim 1, wherein a ratio of the non-stoichiometric metal oxide material and the stoichiometric metal oxide material in the composite layer is 0.005:1 to 0.01:1.

### Claim 3 (depends on 1)

The manufacturing method of the ESD protection device of claim 1, wherein:
step A comprises performing the surface treatment on the substrate using a plasma;
step B comprises providing a metal source and depositing a metal ion produced by the metal source on the substrate;
step C comprises providing an oxygen as a reaction gas at the same time the metal ion is provided by the metal source to deposit the resulting non-stoichiometric metal oxide material on the link layer, wherein a supply of the oxygen is gradually increased with a process time; and
step D comprises providing an oxygen as a reaction gas at the same time the metal ion is provided by the metal source to deposit the resulting stoichiometric metal oxide material and non-stoichiometric metal oxide material on the progressive layer, wherein a supply of the oxygen is configured such that the ratio of the non-stoichiometric metal oxide material and the stoichiometric metal oxide material in the resulting composite layer may make a sheet resistance of the composite layer 1×107 Ω/sq to 1×108 Ω/sq.

### Claim 4 (depends on 3)

The manufacturing method of the ESD protection device of claim 3, wherein step A to step D are performed using a same deposition equipment, and a same metal source is used in step B to step D.

### Claim 5 (depends on 3)

The manufacturing method of the ESD protection device of claim 3, wherein the plasma used in step A comprises an oxygen/argon plasma.

### Claim 6 (depends on 3)

The manufacturing method of the ESD protection device of claim 3, wherein the metal source comprises a metal target, and the metal target comprises a Ti target, an Al target, a Cu target, a Ni target, a Cr target, a Ta target, or a V target.

### Claim 7 (depends on 3)