# US 2021/0280864 A1 · Positive electrode active material for nonaqueous electrolyte secondary batteries, method for producing same, and nonaqueous electrolyte secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0280864 A1
- Document ID: US20210280864A1
- Status: Published application
- Kind: A1
- Application number: 16/328,386
- Filed: 2017-08-31
- Published: 2021-09-09
- Earliest claimed: 2016-08-31
- Assignees: Sumitomo Metal Mining Co., Ltd.
- Applicants: Sumitomo Metal Mining Co., Ltd.
- Inventors: Haruki KANEDA; Yuki KOSHIKA
- Web page: https://patentgrep.com/patent/US20210280864A1

## CPC

- C01G 53/82: Compounds containing nickel, with or without oxygen or hydrogen, and containing two or more other elements
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 53/502: containing lithium and cobalt
- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- H01M 4/366: {as layered products}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/52: containing elements as dopants
- C01P 2002/54: one element only
- C01P 2004/03: obtained by SEM
- C01P 2004/50: Agglomerated particles
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Provided is a positive electrode active material with which a nonaqueous electrolyte secondary battery can be obtained that achieves both high energy density and output characteristics and thermal stability at the time of short-circuit owing to low conductivity. A positive electrode active material for a nonaqueous electrolyte secondary battery contains a lithium-nickel-manganese composite oxide containing a secondary particle formed of a plurality of flocculated primary particles. The lithium-nickel-manganese composite oxide is represented by General Formula (1): LidNi1-a-b-cMnaMbNbcO2-γ, at least part of niobium is solid-solved in the primary particles, and a maximum niobium concentration within the primary particles is at least one time and up to three times an average niobium concentration within the primary particles.

## Claims

### Claim 1

A positive electrode active material for a nonaqueous electrolyte secondary battery, the positive electrode active material comprising:
a lithium-nickel-manganese composite oxide containing a secondary particle formed of a plurality of flocculated primary particles, wherein
the lithium-nickel-manganese composite oxide is represented by General Formula (I): LidNi1-a-b-cMnaMbNbcO2+γ (in General Formula (1), M is at least one element selected from Co, W, Mo, V, Mg, Ca, Al, Ti, Cr, Zr, and Ta; and 0.05≤a≤0.60, 0≤b≤0.60, 0.0003≤c≤0.03, 0.95≤d≤1.20, and 0≤γ≤0.5), at least part of niobium in the lithium-nickel-manganese composite oxide is solid-solved in the primary particles, and a maximum niobium concentration within the primary particles is at least one time and up to three times an average niobium concentration within the primary particles.

### Claim 2 (depends on 1)

The positive electrode active material for a nonaqueous electrolyte secondary battery according to claim 1, wherein a minimum niobium concentration within the primary particles is at least 50% of the average niobium concentration within the primary particles.

### Claim 3 (depends on 1)

The positive electrode active material for a nonaqueous electrolyte secondary battery according to claim 1, wherein a compound containing lithium and niobium is present at least on part of surfaces of the primary particles.

### Claim 4 (depends on 1)

The positive electrode active material for a nonaqueous electrolyte secondary battery according to claim 1, wherein the secondary particle has a volume average particle diameter MV of at least 5 μm and up to 20 μm.

### Claim 5 (depends on 1)

The positive electrode active material for a nonaqueous electrolyte secondary battery according to claim 1, wherein the secondary particle has an average degree of circularity E of at least 0.60 and up to 0.98, the degree being determined by the following expression:
E=4πS/L2 (Expression)
(in the above expression, S is a projected area of the secondary particle, L is a circumferential length of the secondary particle, and π is the ratio of the circumference of a circle to its diameter).

### Claim 6 (depends on 1)

The positive electrode active material for a nonaqueous electrolyte secondary battery according to claim 1, wherein conductivity determined by pressed powder resistance measurement is within a range of at least 1.0×10−5 S/cm and up to 1.0×10−2 S/cm.

### Claim 7

A method for producing a positive electrode, active material for a nonaqueous electrolyte secondary battery, the positive electrode active material comprising a lithium-nickel-manganese composite oxide represented by General Formula (1): LidNi1-a-b-cMnaMbNbcO2+γ (in Formula (1), M is at least one element selected from Co, W, Mo, V, Mg, Ca, Al, Ti, Cr, Zr, and Ta; and 0.05≤a≤0.60, 0≤b≤0.60, 0.0003≤c≤0.03, 0.95≤d≤1.20, and 0≤γ≤0.5) and containing a secondary particle formed of a plurality of flocculated primary particles, at least part of niobium being solid-solved in the primary particles,
the method comprising:
preparing a lithium-niobium mixture containing one or more selected from nickel-manganese composite hydroxide particles represented by General Formula (2): Ni1-a-b-cMnaMb(OH)2+α (in Formula (2), M is at least one element selected from Co, W, Mo, V, Mg, Ca, Al, Ti, Cr, Zr, and Ta; and 0.05≤a≤0.60, 0≤b≤0.60, and 0≤a≤0.4) and nickel-manganese composite oxide particles represented by General Formula (3): Ni1-a-b-cMnaMbO1+β (in Formula (3), M is at least one element selected from Co, W, Mo, V, Mg, Ca, Al, Ti, Cr, Zr, and Ta; and 0.05≤a≤0.60, 0≤b≤0.60, and 0≤β≤0.41, a niobium compound, and a lithium compound; and
firing the lithium-niobium mixture in an oxidative atmosphere at at least 750° C. and up to 1,000° C. to obtain the lithium-nickel-manganese composite oxide.

### Claim 8 (depends on 7)

The method for producing a positive electrode active material for a nonaqueous electrolyte secondary battery according to claim 7, wherein the preparing comprises:
obtaining the nickel-manganese composite hydroxide particles by crystallization; and
mixing the lithium compound and the niobium compound having an average particle diameter of at least 0.01 μm and up to 10 am with the nickel-manganese composite hydroxide particles to prepare the lithium-niobium mixture.

### Claim 9 (depends on 7)

The method for producing a positive electrode active material for a nonaqueous electrolyte secondary battery according to claim 7, wherein the niobium compound is either one or both of niobic acid and niobium oxide.

### Claim 10 (depends on 7)

The method for producing a positive electrode active material for a nonaqueous electrolyte secondary battery according to claim 7, wherein the preparing comprises:
obtaining the nickel-manganese composite hydroxide particles by crystallization;
adding a niobium salt solution and an acid to slurry obtained by mixing the nickel-manganese composite hydroxide particles and water together to obtain nickel-manganese composite hydroxide particles covered with a niobium compound; and
mixing the nickel-manganese composite hydroxide particles covered with a niobium compound and the lithium compound together to prepare the lithium-niobium mixture.

### Claim 11 (depends on 7)

The method for producing a positive electrode active material for a nonaqueous electrolyte secondary battery according to claim 7, comprising thermally treating the nickel-manganese composite hydroxide particles at a temperature of at least 105° C. and up to 700° C. before preparing the lithium-niobium mixture, wherein
the preparing prepares a lithium-niobium mixture containing either one or both, of nickel-manganese composite hydroxide particles and nickel-manganese composite oxide particles obtained by the thermally treating, a niobium compound, and a lithium compound.

### Claim 12

(canceled)

### Claim 13 (depends on 1)

A nonaqueous electrolyte secondary battery comprising:
a positive electrode;
a negative electrode;
a separator; and
a nonaqueous electrolyte solution,
the positive electrode containing the positive electrode active material for a nonaqueous electrolyte secondary battery according to claim 1.