# US 2021/0280860 A1 · Lithium-ion battery anode material and preparation method thereof, anode, and lithium-ion battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0280860 A1
- Document ID: US20210280860A1
- Status: Published application
- Kind: A1
- Application number: 17/255,188
- Filed: 2019-06-19
- Published: 2021-09-09
- Earliest claimed: 2018-06-22
- Assignees: BYD Company Limited
- Applicants: BYD Company Limited
- Inventors: Zhengfu JIANG; Shicai LI; Xiaopeng JIAO; Yongqing GAN; Xiao SHI
- Web page: https://patentgrep.com/patent/US20210280860A1

## CPC

- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/366: {as layered products}
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/483: {for non-aqueous cells (H01M4/485 takes precedence)}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An anode material includes a core-shell structured composite material. The core-shell structured composite material includes a core material, an inner shell material, and an outer shell material. The core material includes graphite particles. The inner shell material includes a continuous phase and a dispersing phase. The dispersing phase includes nano silicon particles, the continuous phase includes carbon, and the outer shell material includes lithium metal. A chemical formula of the nano silicon-based particles is SiOx, 0<x<2.

## Claims

### Claim 1

A lithium-ion battery anode material, comprising:
a core-shell structured composite material, comprising:
a core material, an inner shell material, and an outer shell material, wherein:
the core material comprises graphite particles; and
the inner shell material comprises a continuous phase and a dispersing phase, wherein:
the dispersing phase comprises nano silicon-based particles,
wherein a chemical formula of the nano silicon-based particles is SiOx, 0<x<2; and
the continuous phase comprises carbon; and
the outer shell material comprises lithium metal.

### Claim 2 (depends on 1)

The anode material according to claim 1, wherein an average particle size of the core-shell structured composite material is 5.6-32 μm.

### Claim 3 (depends on 1)

The anode material according to claim 1, wherein:
an inner shell thickness of the core-shell structured composite material is 0.5-2 μm; and
an outer shell thickness of the core-shell structured composite material is 0.1-5 μm.

### Claim 4 (depends on 3)

The anode material according to claim 3, wherein:
the inner shell thickness of the core-shell structured composite material is 1-1.5 μm; and
the outer shell thickness of the core-shell structured composite material is 1-2 μm.

### Claim 5 (depends on 1)

The anode material according to claim 1, wherein:
an average particle size of the graphite particles is 5-25 μm; and
an average particle size of the nano silicon particles is 10-100 nm.

### Claim 6 (depends on 5)

The anode material according to claim 5, wherein:
the average particle size of the graphite particles is 15-20 μm; and
the average particle size of the nano silicon particles is 30-50 nm.

### Claim 7 (depends on 1)

The anode material according to claim 1, wherein:
a weight ratio of the graphite particles to the nano silicon particles is 1:(0.02-0.2);
a weight ratio of the graphite particles to the carbon is 1:(0.03-0.3); and
a weight ratio of the graphite particles to the lithium metal is 1:(0.01-0.2).

### Claim 8 (depends on 7)

The anode material according to claim 7, wherein:
the weight ratio of the graphite particles to the nano silicon particles is 1:(0.1-0.15);
the weight ratio of the graphite particles to the carbon is 1:(0.1-0.15); and
the weight ratio of the graphite particles to the lithium metal is 1:(0.01-0.2).

### Claim 9 (depends on 1)

The anode material according to claim 1, wherein the carbon in the inner shell material is pyrolytic carbon.

### Claim 10 (depends on 1)

The anode material according to claim 1, wherein: the core-shell structured composite material further comprises:
an inert material layer coated on the surface of the outer shell material,
wherein a material of the inert material layer comprises at least one of: Al2O3, LiF, Li3PO4, TiO2, Li3N or LiNO3.

### Claim 11

A method for preparing a lithium-ion battery anode material, comprising:
performing first ball-milling of nano silicon and a carbon source material, and adding graphite and performing second ball-milling to obtain a ball-milled mixture;
sintering the ball-milled mixture under an inert gas atmosphere to obtain a silicon-carbon material; and
depositing lithium metal on a surface of the silicon-carbon material to obtain the anode material.

### Claim 12 (depends on 11)

The method according to claim 11, wherein:
conditions of the first ball-milling comprise:
a rotating speed of 150-600 r/min and a ball-milling time of 12-60 h; and
conditions of the second ball-milling comprise:
a rotating speed of 150-400 r/min and a ball-milling time of 3-18 h.

### Claim 13 (depends on 11)

The method according to claim 11, wherein the carbon source material is at least one material selected from the group consisting of: pitch, glucose, sucrose, citric acid and epoxy resin.

### Claim 14 (depends on 11)

The method according to claim 11, wherein:
a weight ratio of the graphite particles to the nano silicon particles is 1:(0.02-0.2); and
a weight ratio of the graphite particles to the carbon source material is 1:(0.03-0.5).

### Claim 15 (depends on 11)

The method according to claim 11, wherein a weight ratio of the graphite particles to the lithium metal is 1:(0.01-0.2).

### Claim 16 (depends on 11)

The method according to claim 11, wherein:
after depositing lithium metal on the surface of the silicon-carbon material to obtain the anode material, the method further comprises:
depositing an inert material layer on the surface of the lithium metal,
wherein a material of the inert material layer comprises at least one of: Al2O3, LiF, Li3PO4, TiO2, Li3N or LiNO3.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the inert material layer is formed by one of: atomic deposition, chemical deposition, vacuum evaporation deposition, or magnetron sputtering.

### Claim 18

(canceled)

### Claim 19

A lithium-ion battery, comprising a lithium-ion battery anode, the lithium-ion battery anode comprises:
a lithium-ion battery anode material, comprising:
a core-shell structured composite material, comprising:
a core material, an inner shell material, and an outer shell material, wherein:
the core material comprises graphite particles;
the inner shell material comprises:
a continuous phase, and
a dispersing phase, wherein:
the dispersing phase comprises nano silicon-based particles,
wherein a chemical formula of the nano silicon-based particles is SiOx, 0<x<2; and
the continuous phase comprises carbon; and
the outer shell material comprises lithium metal.