# US 2021/0280859 A1 · Method for manufacturing negative electrode for lithium secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0280859 A1
- Document ID: US20210280859A1
- Status: Published application
- Kind: A1
- Application number: 17/331,293
- Filed: 2021-05-26
- Published: 2021-09-09
- Earliest claimed: 2018-12-04
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Gui Long JIN; Seung He WOO; Hyo Sik KIM
- Web page: https://patentgrep.com/patent/US20210280859A1

## CPC

- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/043: {involving compressing or compaction}
- H01M 4/139: Processes of manufacture
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 10/052: Li-accumulators
- H01M 10/0562: Solid materials
- H01M 10/0565: Polymeric materials, e.g. gel-type or solid-type
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 2004/027: {Negative electrodes}
- H01M 2220/30: Batteries in portable systems, e.g. mobile phone, laptop
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for manufacturing a negative electrode for a lithium secondary battery is provided in which the method is capable of effectively performing pre-lithiation. While a negative electrode is compressed with a press, a lithium alloy layer is formed on a portion in contact with a negative electrode active material layer of upper and lower plates of the press, and a negative electrode tab is electrically connected to the press through a connection part respectively disposed on the upper and lower plates of the press, and thus, it is possible to manufacture a negative electrode for a lithium secondary battery in which the pre-lithiation of the negative electrode may be performed at time of compression even without a separate pre-lithiation process.

## Claims

### Claim 1

A method for manufacturing a negative electrode for a lithium secondary battery, the method comprising:
forming a negative electrode active material layer on opposite sides of a negative electrode current collector to form a structure; and
placing the structure between upper and lower plates of a press and compressing the structure, wherein
a lithium alloy layer is formed on a portion of each of the upper and lower plates of the press which are in contact with respective negative electrode active material layers of the structure, and
a negative electrode tap protruding from one side of the negative electrode current collector and having no negative electrode active material is electrically connected to the press through a connection part respectively disposed on the upper and lower plates of the press, whereby pre-lithiation is performed at time of compression.

### Claim 2 (depends on 1)

The method of claim 1, wherein the negative electrode active material layer comprises a solid electrolyte together with the negative electrode active material when the negative electrode is used in the manufacturing of an all-solid lithium secondary battery.

### Claim 3 (depends on 2)

The method of claim 2, wherein the solid electrolyte is at least one of an inorganic solid electrolyte film or an organic solid electrolyte film.

### Claim 4 (depends on 1)

The method of claim 1, wherein a lithium alloy constituting the lithium alloy layer is an alloy of lithium and one or more metals selected from the group consisting of aluminum, silicon, tin, and indium.

### Claim 5 (depends on 1)

The method of claim 1, wherein, when a negative electrode active material constituting the negative electrode active material layer contains graphite, a lithium alloy constituting the lithium alloy layer is an alloy of lithium and aluminum.

### Claim 6 (depends on 1)

The method of claim 1, wherein the compressing is performed at a temperature of 25° C. to 200° C. and a surface pressure of 25 MPa to 500 MPa for 10 seconds to 60 minutes.

### Claim 7 (depends on 1)

The method of claim 1, wherein the connection part is made of a copper material.

### Claim 8 (depends on 1)

The method of claim 1, wherein the connection part is a spring.

### Claim 9

A method for manufacturing an all-solid lithium secondary battery, the method comprising:
forming a negative electrode active material layer on opposite sides of a negative electrode current collector to form a structure, the negative electrode active material layer including a negative electrode active material and a first solid electrolyte;
placing the structure between upper and lower plates of a press and compressing the structure to manufacture a negative electrode;
applying a second solid electrolyte on at least one surface of the manufactured negative electrode to form a solid electrolyte film;
laminating a positive electrode including a third solid electrolyte on an upper portion of the solid electrolyte film to form a laminate body; and
casing the laminate body, wherein
a lithium alloy layer is formed on a portion of each of the upper and lower plates of the press which are in contact with respective negative electrode active material layers of the structure, and
a negative electrode tap protruding from one side of the negative electrode current collector and having no negative electrode active material is electrically connected to the press through a connection part respectively disposed on the upper and lower plates of the press, whereby pre-lithiation is performed at time of compression.

### Claim 10 (depends on 9)

The method of claim 9, wherein the first, second, and third solid electrolytes are the same.

### Claim 11 (depends on 9)

The method of claim 9, wherein the first, second, and third solid electrolytes each independently comprise at least one selected from an inorganic solid electrolyte and an organic solid electrolyte.

### Claim 12

A method for manufacturing a lithium secondary battery, the method comprising:
forming a negative electrode active material layer on opposite sides of a negative electrode current collector to form a structure;
placing the structure between upper and lower plates of a press and compressing the structure to manufacture a negative electrode;
laminating a separator on at least one surface of the manufactured negative electrode;
laminating a positive electrode on an upper portion of the separator to form a laminate body; and
receiving the laminate body in a battery container and injecting a liquid electrolyte into the battery container, wherein
a lithium alloy layer is formed on a portion of each of the upper and lower plates of the press which are in contact with respective negative electrode active material layers of the structure, and
a negative electrode tap protruding from one side of the negative electrode current collector and having no negative electrode active material is electrically connected to the press through a connection part respectively disposed on the upper and lower plates of the press, whereby pre-lithiation is performed at time of compression.