# US 2021/0280842 A1 · Method for producing lithium secondary battery thick film and method for producing lithium secondary battery by using electrostatic slurry spraying of slurry containing sulfide-based solid electrolyte

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0280842 A1
- Document ID: US20210280842A1
- Status: Published application
- Kind: A1
- Application number: 16/319,672
- Filed: 2017-07-19
- Published: 2021-09-09
- Earliest claimed: 2016-07-19
- Assignees: Industry-University Cooperation Foundation Hanyang University
- Applicants: Industry-University Cooperation Foundation Hanyang University
- Inventors: Dong Wook SHIN; Chan Hwi PARK; Se Wook LEE
- Web page: https://patentgrep.com/patent/US20210280842A1

## CPC

- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0419: {involving spraying}
- H01M 4/364: {as mixtures}
- H01M 4/623: {fluorinated polymers}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0562: Solid materials
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided are a method for producing a lithium secondary battery thick film and a method for producing a lithium secondary battery, by using electrostatic slurry spraying of slurry containing a sulfide-based solid electrolyte. Particularly, the method for producing a lithium secondary battery thick film comprises: a step of preparing slurry in which the powder of a sulfide-based solid electrolyte is mixed with at least one solvent selected between a dichloroethane and a dichlorobenzene, at the weight ratio of 1:10 to 1:100; and a step of depositing a lithium secondary battery thick film by electrostatically spraying the slurry on a current collector under a nitrogen atmosphere in the cone-jet mode.

## Claims

### Claim 1

A method of forming a lithium secondary battery thick film by electrostatically spraying a slurry including a sulfide-based solid electrolyte, the method comprising:
preparing a slurry in which a powder of a sulfide-based solid electrolyte is mixed into at least one solvent selected from dichloroethane and dichlorobenzene at a weight ratio of 1:10 to 1:100; and
electrostatically spraying the slurry on a current collector in a cone-jet mode in a nitrogen atmosphere to deposit a lithium secondary battery thick film.

### Claim 2

The method of claim, 1, wherein the sulfide-based solid electrolyte includes a compound of sulfur and at least two components selected from among lithium, phosphorus, boron, silicon, and aluminum.

### Claim 3 (depends on 1)

The method of claim 1, wherein, in the preparing of the slurry, at least one binder selected from among nitrile butadiene rubber (NBR), polyvinylpyrrolidone (PVP), and polyvinylidene fluoride (PVDF) is further mixed into the solvent.

### Claim 4 (depends on 1)

The method of claim 1, wherein, in the preparing of the slurry, a powder of an active material and a powder of a conductive material are further mixed into the solvent, and
the lithium secondary battery thick film is a composite electrode thick film in which the sulfide-based solid electrolyte, the active material, and the conductive material are mixed.

### Claim 5 (depends on 1)

The method of claim 1, wherein the deposition of the lithium secondary battery thick film includes heating the current collector during the electrostatic spraying of the slurry.

### Claim 6 (depends on 1)

The method of claim 1, wherein a ratio of an applied voltage to a spray distance to the current collector is in a range of 1.0 kV/cm to 1.5 kV/cm.

### Claim 7 (depends on 1)

The method of claim 1, wherein a spray flow rate of the slurry is in a range of 115 cm/h to 320 cm/h during the electrostatic spraying.

### Claim 8

A method of manufacturing a lithium secondary battery, the method comprising:
electrostatically spraying a first composite electrode slurry including a powder of a sulfide-based solid electrolyte, a powder of a first active material, and a powder of a conductive material to deposit a first lithium secondary battery composite electrode thick film;
electrostatically spraying a solid electrolyte slurry including a powder of a sulfide-based solid electrolyte on the first lithium secondary battery composite electrode thick film to deposit a lithium secondary battery solid electrolyte thick film; and
electrostatically spraying a second composite electrode slurry including a powder of a sulfide-based solid electrolyte, a powder of a second active material, and a powder of a conductive material on the lithium secondary battery solid electrolyte thick film to deposit a second lithium secondary battery composite electrode thick film,
wherein one of the first active material and the second active material is a positive active material and the other is a negative active material, and
the first composite electrode slurry, the solid electrolyte slurry, and the second composite electrode slurry each include at least one solvent selected from dichloroethane and dichlorobenzene and are electrostatically sprayed in a cone-jet mode in a nitrogen atmosphere.