# US 2021/0280692 A1 · Reducing Metal Gate Overhang By Forming A Top-Wide Bottom-Narrow Dummy Gate Electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0280692 A1
- Document ID: US20210280692A1
- Status: Published application
- Kind: A1
- Application number: 17/323,557
- Filed: 2021-05-18
- Published: 2021-09-09
- Earliest claimed: 2016-10-07
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Shih Wei Bih; Han-Wen Liao; Xuan-You Yan; Yen-Yu Chen; Chun-Chih Lin
- Web page: https://patentgrep.com/patent/US20210280692A1

## CPC

- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 64/01324: {characterised by the sectional shape, e.g. T or inverted-T}
- H10D 64/518: {characterised by their lengths or sectional shapes}
- H10D 64/685: {being perpendicular to the channel plane}
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10D 84/85: Complementary IGFETs, e.g. CMOS
- H10P 50/266: {by vapour etching only}
- H10P 50/268: {of silicon-containing layers}
- H10D 64/667: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN workfunction layers (having lateral variation H10D64/671)}
- H10D 84/0172: {Manufacturing their gate conductors}
- H10D 84/0177: {the gate conductors having different materials or different implants}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A polysilicon layer is formed over a substrate. The polysilicon layer is etched to form a dummy gate electrode having a top portion with a first lateral dimension and a bottom portion with a second lateral dimension. The first lateral dimension is greater than, or equal to, the second lateral dimension. The dummy gate electrode is replaced with a metal gate electrode.

## Claims

### Claim 1

A method, comprising:
forming a dummy gate electrode layer over a gate dielectric layer;
forming a patterned mask layer over the dummy gate electrode layer;
patterning, using the patterned mask layer as a mask, the dummy gate electrode layer into a plurality of patterned dummy gate electrodes that are spaced apart from one another, such that each of the patterned dummy gate electrodes has a top-wide-bottom-narrow profile in a cross-sectional side view, wherein the patterning includes etching the dummy gate electrode layer with increasingly stronger lateral etching characteristics;
forming gate spacers on sidewalls of the patterned dummy gate electrodes; and
replacing the patterned dummy gate electrodes with metal-containing gate electrodes.

### Claim 2 (depends on 1)

The method of claim 1, wherein the etching the dummy gate electrode layer includes performing a plurality of etching steps, wherein each subsequent etching step etches the dummy gate electrode layer at a faster etching rate than a previous etching step.

### Claim 3 (depends on 1)

The method of claim 1, wherein the etching the dummy gate electrode layer includes etching the dummy gate electrode layer inside an etching chamber while an electronegativity etchant is applied.

### Claim 4 (depends on 3)

The method of claim 3, wherein the electronegativity etchant includes a fluorine-containing gas or plasma.

### Claim 5 (depends on 4)

The method of claim 4, wherein the fluorine-containing gas or plasma is applied with a flow rate in a range between about 80 standard cubic centimeters per minute (sccm) and about 120 sccm.

### Claim 6 (depends on 4)

The method of claim 4, wherein the etching the dummy gate electrode layer with increasingly stronger lateral etching characteristics includes increasing a flow rate of the fluorine-containing gas or plasma as deeper portions of the dummy gate electrode layer are reached.

### Claim 7 (depends on 1)

The method of claim 1, wherein the etching the dummy gate electrode layer includes etching the dummy gate electrode layer inside an etching chamber while a chlorine etchant is applied.

### Claim 8 (depends on 7)

The method of claim 7, wherein the chlorine etchant is applied with a flow rate in a range between about 30 standard cubic centimeters per minute (sccm) and about 36 sccm.

### Claim 9 (depends on 1)

The method of claim 1, wherein the patterning further includes applying a passivation gas during the patterning.

### Claim 10 (depends on 9)

The method of claim 9, wherein the applying the passivation gas is performed such that a passivation layer is formed on an upper portion, but not an entirety, of a side surface of each of the patterned dummy gate electrodes during the etching.

### Claim 11 (depends on 1)

The method of claim 1, wherein the forming the dummy gate electrode layer includes forming a polysilicon gate electrode layer over a high-k gate dielectric layer, and wherein the method further comprises:
forming a capping layer over the gate dielectric layer, wherein the dummy gate electrode layer is formed over the capping layer, and wherein the capping layer contains a rare earth material; and
forming an interlayer dielectric (ILD) after the forming of the gate spacers, wherein portions of the ILD are formed between the gate spacers.

### Claim 12 (depends on 11)

The method of claim 11, wherein the patterning the dummy gate electrode layer also patterns the capping layer and the gate dielectric layer, and wherein the patterned capping layer and the patterned gate dielectric layer have less tapered cross-sectional profiles than each of the patterned dummy gate electrodes.

### Claim 13

A method, comprising:
forming a gate dielectric layer over a substrate;
forming a dummy gate electrode layer over the gate dielectric layer;
patterning, via a plurality of etching processes, the dummy gate electrode layer into a plurality of patterned dummy gate electrodes, wherein the plurality of etching processes is performed with increasingly stronger lateral etching characteristics, such that the patterned dummy gate electrodes each have a tapered cross-sectional profile where an upper portion of the patterned dummy gate electrode is wider than a lower portion of the patterned dummy gate electrode;
forming gate spacers on sidewalls of the patterned dummy gate electrodes;
removing the patterned dummy gate electrodes, thereby forming a plurality of openings defined at least in part via the gate spacers; and
filling the plurality of openings with a metal-containing gate electrode layer.

### Claim 14 (depends on 13)

The method of claim 13, wherein the plurality of etching processes is performed inside an etching chamber while an electronegativity etchant and a chlorine etchant are simultaneously applied.

### Claim 15 (depends on 14)

The method of claim 14, wherein:
the electronegativity etchant includes a fluorine-containing gas or plasma; and
the plurality of etching processes is performed at least in part by increasing a flow rate of the fluorine-containing gas or plasma as the dummy gate electrode layer is etched more deeply.

### Claim 16 (depends on 15)

The method of claim 15, wherein:
the fluorine-containing gas or plasma is applied with a flow rate in a range between about 80 standard cubic centimeters per minute (sccm) and about 120 sccm; and
the chlorine etchant is applied with a flow rate in a range between about 30 sccm and about 36 sccm.

### Claim 17 (depends on 13)

The method of claim 13, wherein the patterning further includes forming a passivation layer partially on side surfaces of the dummy gate electrode layer during the etching.

### Claim 18

A method, comprising:
forming an un-patterned dummy gate structure over a substrate;
performing a first etching process on the un-patterned dummy gate structure, wherein the first etching process has a first lateral etching characteristic;
after the first etching process, performing a second etching process on the un-patterned dummy gate structure, wherein the second etching process has a second lateral etching characteristic that is greater than the first lateral etching characteristic;
after the second etching process, performing a third etching process on the un-patterned dummy gate structure, wherein the third etching process has a third lateral etching characteristic that is greater than the second lateral etching characteristic, and wherein the un-patterned dummy gate structure is etched into a plurality of patterned dummy gate structures that are separated from one another after the third etching process has been performed;
forming gate spacers on sidewalls of the patterned dummy gate structures; and
replacing the patterned dummy gate structures with metal-containing gate structures.

### Claim 19 (depends on 18)

The method of claim 18, wherein:
the first etching process is performed at a first etchant flow rate;
the second etching process is performed at a second etchant flow rate faster than the first etchant flow rate; and
the third etching process is performed at a third etchant flow rate faster than the second etchant flow rate.

### Claim 20 (depends on 18)

The method of claim 18, wherein the first etching process, the second etching process, and the third etching process are performed using at least a fluorine-containing gas or plasma as an etchant.