# US 2021/0280634 A1 · Methods of forming films including scandium at low temperatures using chemical vapor deposition to provide piezoelectric resonator devices and/or high electron mobility transistor devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0280634 A1
- Document ID: US20210280634A1
- Status: Published application
- Kind: A1
- Application number: 17/193,623
- Filed: 2021-03-05
- Published: 2021-09-09
- Earliest claimed: 2020-03-05
- Assignees: Akoustis, Inc.
- Applicants: Akoustis, Inc.
- Inventors: Craig Moe; Jeffrey M. Leathersich
- Web page: https://patentgrep.com/patent/US20210280634A1

## CPC

- H10N 39/00: Integrated devices, or assemblies of multiple devices, comprising at least one piezoelectric, electrostrictive or magnetostrictive element covered by groups H10N30/00 – H10N35/00
- H10P 14/3216: {Nitrides}
- C23C 16/0272: {Deposition of sub-layers, e.g. to promote the adhesion of the main coating}
- C23C 16/34: Nitrides {(C23C16/303 takes precedence)}
- H03H 3/02: for the manufacture of piezoelectric or electrostrictive resonators or networks (H03H3/08 takes precedence)
- H03H 9/02031: {consisting of ceramic}
- H03H 9/173: {Air-gaps}
- H03H 9/176: {consisting of ceramic material (H03H9/177, H03H9/178 take precedence)}
- H10D 30/015: {of FETs having heterojunction interface channels or heterojunction gate electrodes, e.g. HEMT}
- H10D 30/475: {having wider bandgap layer formed on top of lower bandgap active layer, e.g. undoped barrier HEMTs such as i-AlGaN/GaN HEMTs}
- H10D 62/824: comprising only Group III-V materials heterojunctions, e.g. GaN/AlGaN heterojunctions
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10N 30/03: Assembling devices that include piezoelectric or electrostrictive parts
- H10N 30/076: by vapour phase deposition
- H10N 30/079: using intermediate layers, e.g. for growth control
- H10N 30/093: Forming inorganic materials
- H10N 30/708: {Intermediate layers, e.g. barrier, adhesion or growth control buffer layers}
- H10N 30/853: Ceramic compositions
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3248: {consisting of two layers}
- H10P 14/3254: {Graded layers}
- H10P 14/3416: {Nitrides}
- H03H 2003/021: {the resonators or networks being of the air-gap type}
- H10D 62/852: being Group III-V materials comprising three or more elements, e.g. AlGaN or InAsSbP
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H03H: IMPEDANCE NETWORKS, e.g. RESONANT CIRCUITS; RESONATORS (waveguides, resonators, lines or other devices of the waveguide type H01P)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of forming a film can include heating a CVD reactor chamber containing a substrate to a temperature range between about 750 degrees Centigrade and about 950 degrees Centigrade, providing a first precursor comprising Al to the CVD reactor chamber in the temperature range, providing a second precursor comprising Sc to the CVD reactor chamber in the temperature range, providing a third precursor comprising nitrogen to the CVD reactor chamber in the temperature range, and forming the film comprising ScAlN on the substrate.

## Claims

### Claim 1

A method of forming a film, the method comprising:
heating a CVD reactor chamber containing a substrate to a temperature range;
providing a first precursor comprising Al to the CVD reactor chamber in the temperature range;
providing to the CVD reactor chamber in the temperature range a second precursor of general formula (2):
Sc(R1Cp)x(R2—NC—C(R3)═N—R2)y (2)
wherein R1 is H or a C1-C5 alkyl chain, R2 is H or a C1-C5 alkyl chain, R3 is H or Me, x is 0, 1, or 2, y is 1, 2, or 3, with the proviso that x+y=3, and wherein there is one N atom for each outer shell electron of the Sc when x=0;
providing a third precursor comprising NITROGEN to the CVD reactor chamber in the temperature range; and
forming the film comprising ScAlN on the substrate.

### Claim 2 (depends on 1)

The method of claim 1 wherein the temperature range is between about 750 degrees Centigrade and about 950 degrees Centigrade.

### Claim 3 (depends on 1)

The method of claim 1 wherein a ratio of an amount of the N included in the third precursor to an amount of the Al and Sc in the first and second precursors, respectively, is in a range between about 500 and about 20,000.

### Claim 4 (depends on 1)

The method of claim 1 wherein a ratio of an amount of the N included in the third precursor to an amount of the Al and Sc in the first and second precursors, respectively, is in a range between about 500 and about 3000.

### Claim 5 (depends on 1)

The method of claim 1 wherein the substrate comprises Si, SiC, Al2O3, AlN, or GaN.

### Claim 6 (depends on 1)

The method of claim 1 wherein forming the film comprises forming a compositionally uniform single crystal piezoelectric ScAlN acoustic resonator film.

### Claim 7 (depends on 1)

The method of claim 1 further comprising:
before forming the film comprising ScAlN, forming an AlN nucleation layer on the substrate.

### Claim 8 (depends on 7)

The method of claim 7 further comprising:
before forming the film comprising ScAlN, forming a buffer layer comprising AlN on the substrate including a graded amount of Sc therein as a function of a thickness of the buffer layer to provide the film comprising ScAlN having a percentage of Sc in a range between about 18% and about 42%.

### Claim 9 (depends on 8)

The method of claim 8 wherein the film comprising ScAlN has a stress relative to the substrate in a range between about +200 MPa and about −200 MPa.

### Claim 10 (depends on 7)

The method of claim 7 further comprising:
before forming the film comprising ScAlN, forming a plurality of buffer layers comprising AlN on the substrate, wherein each successive one of the plurality of buffer layers has an increased percentage of Sc to provide the film comprising ScAlN having a percentage of Sc in a range between about 18% and about 42%.

### Claim 11 (depends on 10)

The method of claim 10 wherein the film comprising ScAlN has a stress relative to the substrate in a range between about +200 MPa and about −200 MPa.

### Claim 12 (depends on 7)

The method of claim 7 further comprising:
before forming the film comprising ScAlN, forming a buffer layer comprising AlxGa1-xN on the substrate including a graded decreasing amount of Al as a function of thickness of the buffer layer, to provide the film comprising ScAlN having a percentage of Sc in a range between about 18% and about 42%.

### Claim 13 (depends on 12)

The method of claim 12 wherein the film comprising ScAlN has a stress relative to the substrate in a range between about +200 MPa and about −200 MPa.

### Claim 14 (depends on 7)

The method of claim 7 further comprising:
before forming the film comprising ScAlN, forming a plurality of buffer layers comprising AlxGa1-xN on the substrate, wherein each successive one of the plurality of buffer layers has decreased amount of Al to provide the film comprising ScAlN having a percentage of Sc in a range between about 18% and about 42%.

### Claim 15 (depends on 13)

The method of claim 13 wherein the film comprising ScAlN has a stress relative to the substrate in a range between about +200 MPa and about −200 MPa.

### Claim 16 (depends on 1)

The method of claim 1 wherein the film comprising ScAlN provides a barrier layer of a High Electron Mobility Transistor (HEMT) device configured to confine formation of a 2DEG channel region of the HEMT device.

### Claim 17 (depends on 16)

The method of claim 16 wherein forming the film comprising ScAlN is preceded by:
forming a GaN channel layer including a GaN channel region on a buffer layer.

### Claim at position 18

-20. (canceled)

### Claim 21 (depends on 1)

The method of claim 1 wherein the film comprising ScAlN forms a substantially uniform composition of wurtzite crystalline structure ScAlN, as measured by a variation of less than ±0.5 atomic % over 50 nm of scan distance.

### Claim 22 (depends on 21)

The method of claim 21 wherein the substantially uniform composition of wurtzite crystalline structure ScAlN is substantially free of segregated ScN crystal structures.

### Claim 23 (depends on 21)

The method of claim 21 wherein the substantially free of segregated ScN crystal structures is indicated by a Sc peak count at about 34.5 degrees in an XRD 2Theta scan that is less than 5% of the Sc peak count at about 36 degrees taken relative to the 110 crystal plane.

### Claim 24 (depends on 21)

The method of claim 21 wherein the substantially uniform composition of wurtzite crystalline structure ScAlN is substantially free of segregated ScN crystal structures as illustrated in FIG. 4.

### Claim at position 23

-31. (canceled)

### Claim 32

A method of forming a film, the method comprising:
heating a CVD reactor chamber containing a substrate to a temperature range providing a first precursor comprising Al to the CVD reactor chamber in the temperature range;
providing a second precursor comprising Sc to the CVD reactor chamber in the temperature range,
providing a third precursor comprising NITROGEN to the CVD reactor chamber in the temperature range; and
forming the film comprising ScAlN a concentration of C that is less than 1019/cm3 on the substrate.

### Claim at position 25

-34. (canceled)

### Claim 35

An RF integrated circuit device comprising:
a substrate; and
a High Electron Mobility Transistor (HEMT) device on the substrate including a ScAlN layer including a concentration of C that is less than 1019/cm3 and configured to provide a barrier layer of the HEMT device to confine formation of a 2DEG channel region of the HEMT device.

### Claim at position 27

-39. (canceled)

### Claim 40 (depends on 37)

The RF integrated circuit device of claim 37 wherein the substantially uniform composition of wurtzite crystalline structure ScAlN is substantially free of segregated ScN crystal structures as illustrated in FIG. 4.

### Claim at position 29

-47. (canceled)

### Claim 48

A piezoelectric acoustic resonator layer comprising:
a substrate;
an MOCVD formed single crystal piezoelectric ScxAl1-xN layer on the substrate, where x is in a range between about 0.04 and about 0.41.

### Claim 49 (depends on 48)

The piezoelectric acoustic resonator layer of claim 48 wherein the MOCVD formed single crystal piezoelectric ScxAl1-xN layer has a crystalline structure characterized by an XRD rocking curve FWHM value in a range between about less than 1.0 degrees to about 0.001 degrees as measured about an omega scan angle.

### Claim 50 (depends on 49)

The piezoelectric acoustic resonator layer of claim 49 wherein the single crystal piezoelectric ScxAl1-xN layer has a thickness in a range between about 10 nm and about 2 um.

### Claim 51 (depends on 48)

The piezoelectric acoustic resonator layer of claim 48 wherein the substrate comprises SiC, Al2O3, Si, or GaN.

### Claim 52

A method of forming a piezoelectric acoustic resonator layer, the method comprising:
providing a substrate in a MOCVD reactor chamber;
forming an MOCVD single crystal piezoelectric ScxAl1-xN layer on the substrate, where x is in a range between about 0.04 and about 0.41.

### Claim 53 (depends on 52)

The method of claim 52 wherein forming the MOCVD single crystal piezoelectric ScxAl1-xN layer on the substrate comprises:
providing a heated Sc precursor material to the reactor chamber at a temperature in a range between about 100 degrees Centigrade and about 250 degrees Centigrade to grow the MOCVD single crystal piezoelectric ScxAl1-xN layer.

### Claim 54 (depends on 53)

The method of claim 53 further comprising:
Maintaining a surface of the substrate at a growth temperature in a range between about 1200 degrees Centigrade to about 800 degrees Centigrade while forming the MOCVD single crystal piezoelectric ScxAl1-xN layer, wherein the growth temperature is measured using pyrometry.

### Claim 55 (depends on 53)

The method of claim 53 further comprising:
maintaining a surface of the substrate at a growth temperature in a range between about 1050 degrees Centigrade to about 800 degrees Centigrade while forming the MOCVD single crystal piezoelectric ScxAl1-xN layer, wherein the growth temperature is measured using pyrometry.

### Claim 56 (depends on 53)

The method of claim 53 wherein the heated Sc precursor material comprises (DIPA)3Sc.

### Claim 57 (depends on 53)

The method of claim 53 wherein the heated Sc precursor material comprises (MeCp)3Sc.