# US 2021/0280553 A1 · Palladium-coated copper bonding wire and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0280553 A1
- Document ID: US20210280553A1
- Status: Published application
- Kind: A1
- Application number: 17/328,622
- Filed: 2021-05-24
- Published: 2021-09-09
- Earliest claimed: 2018-11-26
- Assignees: Tanaka Denshi Kogyo K. K.
- Applicants: Tanaka Denshi Kogyo K. K.
- Inventors: Hiroyuki AMANO; Yuki ANTOKU; Takeshi KUWAHARA
- Web page: https://patentgrep.com/patent/US20210280553A1

## CPC

- H10W 72/50: Bond wires
- C22C 9/00: Alloys based on copper
- C22C 9/06: with nickel or cobalt as the next major constituent
- H10W 72/015: {of bond wires}
- H10W 72/01515: {Forming coatings}
- H10W 72/01551: {Changing the shapes of bond wires}
- H10W 72/01565: {Thermally treating}
- H10W 72/07141: {Means for applying energy, e.g. ovens or lasers}
- H10W 72/075: {of bond wires}
- H10W 72/07511: {Treating the bonding area before connecting, e.g. by applying flux or cleaning}
- H10W 72/07532: {Compression bonding, e.g. thermocompression bonding}
- H10W 72/07533: {Ultrasonic bonding, e.g. thermosonic bonding}
- H10W 72/521: {Structures or relative sizes of bond wires}
- H10W 72/522: {Multilayered bond wires, e.g. having a coating concentric around a core}
- H10W 72/523: {characterised by the structures of the outermost layers, e.g. multilayered coatings}
- H10W 72/536: {the connected ends being ball-shaped}
- H10W 72/5449: {not being orthogonal to a side surface of the chip, e.g. fan-out arrangements}
- H10W 72/552: {comprising metals or metalloids, e.g. silver}
- H10W 72/5522: {comprising gold [Au]}
- H10W 72/5525: {comprising copper [Cu]}
- H10W 72/555: {of outermost layers of multilayered bond wires, e.g. material of a coating}
- H10W 72/59: Bond pads specially adapted therefor
- H10W 72/90: Bond pads, in general
- H10W 72/932: {Plan-view shape, i.e. in top view}
- H10W 72/9445: {Top-view layouts, e.g. mirror arrays}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 90/755: {between a chip and a laterally-adjacent insulating package substrate, interpose or RDL}
- H10W 90/756: {between a chip and a stacked lead frame, conducting package substrate or heat sink}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

There is provided a palladium-coated copper bonding wire that does not cause a shrinkage cavity during first bonding, has high bonding reliability, and is capable of maintaining excellent bonding reliability for a long period of time even in high-temperature and high-humidity environments. A palladium-coated copper bonding wire in which a concentration of palladium is 1.0 mass % or more and 4.0 mass % or less relative to the total of copper, palladium, and a sulfur group element, a total concentration of the sulfur group element is 50 mass ppm or less, and a concentration of sulfur is 5 mass ppm or more and 12 mass ppm or less, a concentration of selenium is 5 mass ppm or more and 20 mass ppm or less, or a concentration of tellurium is 15 mass ppm or more and 50 mass ppm or less, and the palladium-coated copper bonding wire including a palladium-concentrated region with the average concentration of palladium of 6.5 atom % or more and 30.0 atom % or less relative to the total of copper and palladium within a range from a surface of a tip portion of a free air ball formed at a tip of the wire to 5.0 nm or more and 100.0 nm or less.

## Claims

### Claim 1

A palladium-coated copper bonding wire containing 50 mass ppm or less of sulfur group element in total, the palladium-coated copper bonding wire comprising:
a core material containing copper as a main component; and
a palladium layer on the core material, wherein
the sulfur group element includes at least one of:
5 mass ppm or more and 12 mass ppm or less of sulfur (S);
5 mass ppm or more and 20 mass ppm or less of selenium (Se); and
15 mass ppm or more and 50 mass ppm or less of tellurium (Te),
a concentration of palladium is 1.0 mass % or more and 4.0 mass % or less relative to the total of copper, palladium, and the sulfur group element of the palladium-coated copper bonding wire, and,
the palladium-coated copper bonding wire includes a palladium-concentrated region with the average concentration of palladium of 6.5 atom % or more and 30.0 atom % or less relative to the total of copper and palladium within a range from a surface of a tip portion of a free air ball formed at a tip of the wire to 5.0 nm or more and 100.0 nm or less.

### Claim 2 (depends on 1)

The palladium-coated copper bonding wire according to claim 1,
wherein
a concentration of palladium derived from the palladium layer is 1.0 mass % or more and 2.5 mass % or less relative to the total of copper, palladium, and the sulfur group element of the palladium-coated copper bonding wire.

### Claim 3 (depends on 1)

The palladium-coated copper bonding wire according to claim 1, wherein
a diameter of the palladium-coated copper bonding wire is 10 μm or more and 30 μm or less.

### Claim 4 (depends on 1)

The palladium-coated copper bonding wire according to claim 1, wherein
free air ball forming conditions when detecting the palladium-concentrated region are that a discharge current value is 65 mA and a diameter of a ball is 1.8 times the diameter of the wire, in the presence of a mixed gas of nitrogen and hydrogen.

### Claim 5 (depends on 1)

The palladium-coated copper bonding wire according to claim 1, wherein
the concentration of palladium of the palladium-concentrated region is a concentration measured under Auger electron spectroscopy analysis conditions where an acceleration voltage of a primary electron beam is 10 kV, a measurement region calculated from a set value is 15 μm2 or more and 20 μm2 or less, an acceleration voltage of argon ion sputtering is 1 kV, and a sputtering rate is 2.5 nm/min (in terms of SiO2) as setting conditions of a device.

### Claim 6 (depends on 1)

The palladium-coated copper bonding wire according to claim 1, wherein 50.0% or more of the sulfur group element is contained in the palladium layer.

### Claim 7 (depends on 1)

The palladium-coated copper bonding wire according to claim 1, wherein
50.0% or more of the sulfur group element is contained between the surface of the palladium-coated copper bonding wire and a place with 50.0 atom % of palladium relative to the total of palladium and copper.

### Claim 8 (depends on 1)

The palladium-coated copper bonding wire according to claim 1, further comprising:
a gold layer on a surface of the palladium layer.

### Claim 9 (depends on 1)

The palladium-coated copper bonding wire according to claim 1, wherein
the concentration of sulfur (S) in the entire palladium-coated copper bonding wire is 6 mass ppm or more and 10 mass ppm or less.

### Claim 10 (depends on 1)

The palladium-coated copper bonding wire according to claim 1, wherein
the concentration of selenium (Se) in the entire palladium-coated copper bonding wire is 6 mass ppm or more and 15 mass ppm or less.

### Claim 11 (depends on 1)

The palladium-coated copper bonding wire according to claim 1, wherein
the concentration of tellurium (Te) in the entire palladium-coated copper bonding wire is 16 mass ppm or more and 45 mass ppm or less.

### Claim 12

A method of manufacturing a palladium-coated copper bonding wire containing 50 mass ppm or less of sulfur group element in total, the palladium-coated copper bonding wire including: a core material containing copper as a main component; and a palladium layer on the core material, wherein
the sulfur group element includes at least one of:
5 mass ppm or more and 12 mass ppm or less of sulfur (S);
5 mass ppm or more and 20 mass ppm or less of selenium (Se); and
15 mass ppm or more and 50 mass ppm or less of tellurium (Te),
a concentration of palladium is 1.0 mass % or more and 4.0 mass % or less relative to the total of copper, palladium, and the sulfur group element, and
the manufacturing method comprising:
preparing a copper wire rod containing copper as a main component and forming a palladium layer containing the sulfur group element on a surface of the copper wire rod.