# US 2021/0278759 A1 · Method of manufacturing reflective mask blank, and reflective mask blank

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0278759 A1
- Document ID: US20210278759A1
- Status: Published application
- Kind: A1
- Application number: 17/181,026
- Filed: 2021-02-22
- Published: 2021-09-09
- Earliest claimed: 2020-03-03
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Applicants: Shin-Etsu Chemical Co., Ltd.
- Inventors: Yukio INAZUKI; Takuro KOSAKA; Tsuneo TERASAWA
- Web page: https://patentgrep.com/patent/US20210278759A1

## CPC

- G03F 1/24: Reflection masks; Preparation thereof
- C23C 14/0042: {Controlling partial pressure or flow rate of reactive or inert gases with feedback of measurements}
- C23C 14/185: {by cathodic sputtering}
- C23C 14/3464: {using more than one target (C23C14/56 takes precedence)}
- C23C 14/3485: {using pulsed power to the target}
- C23C 14/352: {using more than one target (C23C14/56 takes precedence)}
- G03F 1/58: having two or more different absorber layers, e.g. stacked multilayer absorbers
- G21K 1/062: {Devices having a multilayer structure}
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- H10P 76/4085: {characterised by the processes involved to create the masks}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- G21K: HANDLING OF PARTICLES OR IONISING RADIATION NOT OTHERWISE PROVIDED FOR; IRRADIATION DEVICES; GAMMA RAY OR X-RAY MICROSCOPES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A reflective mask blank including a substrate, a multilayer reflection film consisting of at least two first layers and at least two second layers that are laminated alternatively and having different optical properties each other, and an absorber film are manufactured by a sputtering method. Each layer is formed by two stages consisting of a first stage applied from when the forming of each layer is started and until a prescribed thickness is formed, and a second stage applied from when the prescribed thickness is formed and until the forming of each layer is completed, and a sputtering pressure of the first stage is set to higher than both a sputtering pressure at which the forming of the layer formed just before is completed, and a sputtering pressure of the second stage.

## Claims

### Claim 1

A method of manufacturing a reflective mask blank comprising a substrate, a multilayer reflection film formed on one main surface of the substrate, and an absorber film formed on the multilayer reflection film, the multilayer reflection film consisting of at least two first layers and at least two second layers that are laminated alternatively, the first and second layers having different optical properties each other,
the method comprising the step of forming the first and second layers constituting the multilayer reflection film alternatively by a sputtering method, wherein
in the forming step of the first and second layers constituting the multilayer reflection film, each layer is formed by two stages consisting of a first stage applied from when the forming of said each layer is started and until a prescribed thickness is formed, and a second stage applied from when the prescribed thickness is formed and until the forming of said each layer is completed, and
in forming the second layer subsequent to forming the first layer, or in forming the first layer subsequent to forming second layer, a sputtering pressure of the first stage is set to higher than both a sputtering pressure at which the forming of the layer formed just before is completed, and a sputtering pressure of the second stage.

### Claim 2 (depends on 1)

The method of claim 1 wherein the prescribed thickness formed in the first stage is at least 1/20 and less than ½ of the total thickness formed in the whole of the first and second stages.

### Claim 3 (depends on 1)

The method of claim 1 wherein the sputtering pressure of the first stage is at least 0.08 Pa, and a sputtering pressure of the second stage is less than 0.08 Pa.

### Claim 4 (depends on 1)

The method of claim 1 wherein the sputtering method is a magnetron sputtering method.

### Claim 5 (depends on 1)

The method of claim 1 wherein the sputtering pressures of the first and second stages are adjusted by argon gas.

### Claim 6 (depends on 1)

The method of claim 1 wherein the first and second layers are a Si layer and a Mo layer, respectively, and the first and second layers are laminated alternatively at least 40 layers, respectively.

### Claim 7 (depends on 1)

A reflective mask blank manufactured by the method of claim 1, comprising a substrate, a multilayer reflection film formed on one main surface of the substrate, and an absorber film formed on the multilayer reflection film, the multilayer reflection film consisting of at least two first layers and at least two second layers that are laminated alternatively, the first and second layers having different optical properties each other.

### Claim 8 (depends on 7)

The reflective mask blank of claim 7 wherein the multilayer reflection film has a reflectance of at least 66.5% with respect to extreme ultraviolet (EUV) light having a wavelength of 13 to 14 nm at an incident angle of 6°.

### Claim 9 (depends on 7)

The reflective mask blank of claim 7 wherein the first and second layers are a Si layer and a Mo layer, respectively, and the first and second layers are laminated alternatively at least 40 layers, respectively.

### Claim 10 (depends on 7)

The reflective mask blank of claim 7 wherein the main surface of the substrate on which the multilayer reflection film is formed has a surface roughness RMS of not more than 0.15 nm.