# US 2021/0278214 A1 · Process flow for fabricating integrated photonics optical gyroscopes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0278214 A1
- Document ID: US20210278214A1
- Status: Published application
- Kind: A1
- Application number: 17/249,603
- Filed: 2021-03-05
- Published: 2021-09-09
- Earliest claimed: 2020-03-06
- Assignees: Anello Photonics, Inc.
- Applicants: Anello Photonics, Inc.
- Inventors: Mario Paniccia; Avi Feshali
- Web page: https://patentgrep.com/patent/US20210278214A1

## CPC

- G01C 19/722: {of the mechanical construction}
- G02B 6/132: by deposition of thin films
- G02B 6/126: using polarisation effects {(G02B6/1226 takes precedence)}
- G02B 6/12002: {Three-dimensional structures}
- G02B 6/136: by etching
- G02B 2006/12061: {Silicon}
- G01C: MEASURING DISTANCES, LEVELS OR BEARINGS; SURVEYING; NAVIGATION; GYROSCOPIC INSTRUMENTS; PHOTOGRAMMETRY OR VIDEOGRAMMETRY (measuring liquid level G01F; radio navigation, determining distance or velocity by use of propagation effects, e.g. Doppler effects, propagation time, of radio waves, analogous arrangements using other waves G01S)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

Aspects of the present disclosure are directed to configurations of compact ultra-low loss integrated photonics-based waveguides for optical gyroscope applications, and the methods of fabricating those waveguides for ease of large scale manufacturing. Four main process flows are described: (1) process flow based on a repeated sequence of oxide deposition and anneal; (2) chemical-mechanical polishing (CMP)-based process flow followed by wafer bonding; (3) Damascene process flow followed by oxide deposition and anneal, or wafer bonding; and (4) CMP-based process flows followed by oxide deposition. Any combination of these process flows may be adopted to meet the end goal of fabricating optical gyroscope waveguides in one or more layers on a silicon substrate using standard silicon fabrication technologies.

## Claims

### Claim 1

A method of fabricating integrated photonics optical gyroscopes, comprising:
providing a silicon substrate with a first oxide layer thereon, wherein the first oxide layer acts as a lower cladding of a waveguide;
forming a patterned silicon nitride (SiN) layer on top of the first oxide layer, the patterned SiN layer acting as a core of the waveguide;
forming a second oxide layer on top of the patterned SiN layer, wherein the second oxide layer is formed by repeating the following sequence for a predetermined number of time:
depositing a first sub-layer of the second oxide for a predetermined thickness;
annealing the deposited first sub-layer of the second oxide at a predetermined temperature for a predetermined period of time to drive impurities out;
depositing a subsequent sub-layer of the second oxide for the predetermined thickness; and
after deposition of each subsequent sub-layer of the second oxide, annealing the deposited sub-layers at the predetermined temperature for the predetermined period of time to drive impurities out.

### Claim 2 (depends on 1)

The method of claim 1, wherein the second oxide layer comprises oxide deposited using a precursor gas chosen from: TEOS, chlorinated source, or deuterated source.

### Claim 3 (depends on 2)

The method of claim 2, wherein the impurities that are driven out from the second oxide layer comprises hydrogen.

### Claim 4 (depends on 2)

The method of claim 2, wherein the predetermined temperature for annealing ranges from 1100-1300° C.

### Claim 5 (depends on 2)

The method of claim 2, wherein the predetermined period of time for annealing depends on thickness of each sub-layer.

### Claim 6 (depends on 2)

The method of claim 2, wherein each sub-layer is 0.1-0.2 μm thick.

### Claim 7 (depends on 2)

The method of claim 2, wherein the total thickness of the second oxide layer is 2-3 μm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the second oxide layer acts as an upper cladding of the waveguide.

### Claim 9 (depends on 1)

The method of claim 1, wherein the second oxide layer is polished down to a reduced thickness by chemical mechanical polishing (CMP) such that a top surface of the polished second oxide layer is substantially flush with a top surface of the core of the waveguide.

### Claim 10 (depends on 9)

The method of claim 9, wherein a wafer is bonded on top of the second oxide layer polished down to the reduced thickness by CMP.

### Claim 11 (depends on 10)

The method of claim 10, wherein the CMP causes to achieve a desired surface roughness of the SiN core of the waveguide.

### Claim 12 (depends on 10)

The method of claim 10, wherein the wafer bonded on top of the second oxide layer comprises a fused silica wafer.

### Claim 13 (depends on 10)

The method of claim 10, wherein the wafer bonded on top of the second oxide layer acts as an upper cladding of the waveguide.

### Claim 14 (depends on 1)

The method of claim 1, wherein forming a patterned silicon nitride (SiN) layer on top of the first oxide layer comprises:
depositing SiN layer for a first thickness that is higher than a desired thickness of the waveguide core;
reducing the first thickness of the SiN layer by CMP to a second thickness, wherein the second thickness is the desired thickness of the waveguide core.

### Claim 15 (depends on 14)

The method of claim 14, wherein the second oxide layer is deposited after the CMP to obtain the desired thickness.

### Claim 16 (depends on 1)

The method of claim 1, wherein forming a patterned silicon nitride (SiN) layer on top of the first oxide layer:
depositing SiN layer for a first thickness that is higher than a desired thickness of the waveguide core;
patterning the SiN layer to form waveguide core of having a desired lateral width and the first thickness that is higher than the desired thickness of the waveguide core;
depositing an additional oxide layer encompassing the patterned waveguide core, wherein the additional oxide layer forms a part of the lower cladding;
prior to forming the second oxide layer on top of the patterned SiN layer, using CMP to partially polish off the SiN layer and the additional oxide layer, thereby reducing the first thickness of the SiN layer to a second thickness, wherein the second thickness is the desired thickness of the waveguide core.

### Claim 17 (depends on 16)

The method of claim 16, wherein the CMP causes to achieve a desired surface roughness of the SiN core of the waveguide.

### Claim 18 (depends on 16)

The method of claim 16, wherein a top surface of the waveguide core is flush with a remaining portion of the additional oxide layer after CMP such that the waveguide core is effectively entrenched into the lower cladding.

### Claim 19 (depends on 1)

The method of claim 1, wherein forming a patterned silicon nitride (SiN) layer on top of the first oxide layer comprises:
creating a notch in the first oxide layer in the dimension of the waveguide core;
depositing a SiN layer on top of the first oxide layer with the etch; and
polishing the SiN layer using CMP such that SiN remains only inside the trench to form the waveguide core.

### Claim 20 (depends on 19)

The method of claim 19, wherein the CMP causes to achieve a desired surface roughness of the SiN core of the waveguide.

### Claim 21 (depends on 19)

The method of claim 19, wherein the notch is created by timed etch.

### Claim 22 (depends on 21)

The method of claim 21, wherein the second oxide layer is deposited after the CMP to leave SiN only inside the notch.

### Claim 23 (depends on 22)

The method of claim 22, wherein a cleaning step is performed after the CMP and before the deposition of the second oxide layer.