# US 2021/0277519 A1 · Vapor deposition of thin films comprising gold

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0277519 A1
- Document ID: US20210277519A1
- Status: Published application
- Kind: A1
- Application number: 17/330,994
- Filed: 2021-05-26
- Published: 2021-09-09
- Earliest claimed: 2017-01-26
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: Maarit Mäkelä; Timo Hatanpää; Mikko Ritala; Markku Leskelä
- Web page: https://patentgrep.com/patent/US20210277519A1

## CPC

- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/06: characterised by the deposition of metallic material
- C23C 16/18: from metallo-organic compounds
- C23C 16/45527: {characterized by the ALD cycle, e.g. different flows or temperatures during half-reactions, unusual pulsing sequence, use of precursor mixtures or auxiliary reactants or activations}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Vapor deposition processes for forming thin films comprising gold on a substrate in a reaction space are provided. The processes can be cyclical vapor deposition processes, such as atomic layer deposition (ALD) processes. The processes can include contacting the substrate with a gold precursor comprising at least one sulfur donor ligand and at least one alkyl ligand, and contacting the substrate with a second reactant comprising ozone. The deposited thin films comprising gold can be uniform, continuous, and conductive at very low thicknesses.

## Claims

### Claim 1

A process for forming a thin film comprising gold on a substrate in a reaction space, the process comprising:
sequentially contacting the substrate with a vapor phase gold precursor and a vapor phase second reactant;
wherein the vapor phase gold precursor comprises sulfur; and
wherein the gold precursor and the second reactant react to form the thin film comprising gold.

### Claim 2 (depends on 1)

The process of claim 1, wherein sequentially contacting the substrate with a vapor phase gold precursor and a vapor phase second reactant comprises a deposition cycle that is repeated two or more times.

### Claim 3 (depends on 2)

The process of claim 2, wherein the deposition cycle further comprising removing excess vapor phase gold precursor from the reaction space after contacting the substrate with the vapor phase gold precursor and prior to contacting the substrate with the vapor phase second reactant.

### Claim 4 (depends on 2)

The process of claim 2, wherein the deposition cycle further comprising removing excess second reactant and reaction byproducts, if any, from the reaction space after contacting the substrate with the second reactant.

### Claim 5 (depends on 2)

The process of claim 2, wherein the process is an atomic layer deposition (ALD) process.

### Claim 6 (depends on 2)

The process of claim 2, wherein the process is a cyclical chemical vapor deposition (CVD) process.

### Claim 7 (depends on 2)

The process of claim 2, wherein the thin film comprising gold is deposited at a growth rate of more than about 0.8 Å per deposition cycle.

### Claim 8 (depends on 2)

The process of claim 2, wherein the thin film comprising gold is continuous after 100 deposition cycles.

### Claim 9 (depends on 1)

The process of claim 1, wherein the gold of the gold precursor has an oxidation state of +III.

### Claim 10 (depends on 1)

The process of claim 1, wherein the vapor phase gold precursor comprises at least one alkyl ligand.

### Claim 11 (depends on 1)

The process of claim 1, wherein the gold precursor comprises one or more neutral adducts.

### Claim 12 (depends on 1)

The process of claim 1, wherein the gold precursor comprises a diethyldithiocarbamato ligand.

### Claim 13 (depends on 12)

The process of claim 12, wherein the gold precursor comprises Me2Au(S2CNEt2).

### Claim 14 (depends on 1)

The process of claim 1, wherein the vapor phase second reactant comprises oxygen.

### Claim 15 (depends on 14)

The process of claim 14, wherein the vapor phase second reactant comprises a reactive species of oxygen.

### Claim 16 (depends on 15)

The process of claim 15, wherein the vapor phase second reactant comprises ozone.

### Claim 17 (depends on 1)

The process of claim 1, wherein the process is carried out at a deposition temperature of from about 120° C. to about 220° C.

### Claim 18 (depends on 15)

The process of claim 15, wherein a thin film comprising gold having a thickness of from about 20 nm to about 50 nm is deposited.

### Claim 19 (depends on 16)

The process of claim 16, wherein the thin film comprising gold is continuous.

### Claim 20 (depends on 15)

The process of claim 15, wherein the thin film comprising gold has a resistivity of less than about 20 μΩcm.