# US 2021/0277508 A1 · Aluminum alloy with additions of copper, lithium and at least one alkali or rare earth metal, and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0277508 A1
- Document ID: US20210277508A1
- Status: Published application
- Kind: A1
- Application number: 17/326,492
- Filed: 2021-05-21
- Published: 2021-09-09
- Earliest claimed: 2017-04-11
- Assignees: The Boeing Company
- Applicants: The Boeing Company
- Inventors: Austin E. Mann; Andrew H. Baker; Rajiv Mishra; Sivanesh Palanivel
- Web page: https://patentgrep.com/patent/US20210277508A1

## CPC

- C22F 1/057: of alloys with copper as the next major constituent
- B22D 7/005: {from non-ferrous metals}
- C22C 21/12: with copper as the next major constituent
- C22C 21/14: with silicon
- C22C 21/16: with magnesium
- C22C 21/18: with zinc
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A method for making an aluminum alloy includes steps of (1) weighing out starting materials to achieve a mass of material having a composition that includes aluminum, about 1.8 to about 5.6 percent by weight copper, about 0.6 to about 2.6 percent by weight lithium, and at least one of lanthanum up to about 1.5 percent by weight, strontium up to about 1.5 percent by weight, cerium up to about 1.5 percent by weight, and praseodymium up to about 1.5 percent by weight; (2) loading said starting materials into a crucible; (3) inserting said crucible into a chamber; (4) evacuating said chamber to a predetermined vacuum level; (5) melting said starting materials to form a molten mass; and (6) casting said molten mass into a mold.

## Claims

### Claim 1

A method for making an aluminum alloy comprising steps of:
weighing out starting materials to achieve a mass of material having a composition comprising:
aluminum;
about 1.8 to about 5.6 percent by weight copper;
about 0.6 to about 2.6 percent by weight lithium; and
at least one of:
lanthanum up to about 1.5 percent by weight;
strontium up to about 1.5 percent by weight;
cerium up to about 1.5 percent by weight; and
praseodymium up to about 1.5 percent by weight;
loading said starting materials into a crucible;
inserting said crucible into a chamber;
evacuating said chamber to a predetermined vacuum level;
melting said starting materials to form a molten mass; and
casting said molten mass into a mold.

### Claim 2 (depends on 1)

The method of claim 1 wherein said predetermined vacuum level is at most about 0.05 Torr, and wherein said chamber is backfilled with an inert gas.

### Claim 3 (depends on 1)

The method of claim 1 wherein:
said molten mass is cast into a mold;
said molten mass is cooled to form a solid mass;
said solid mass is homogenized and water quenched to yield an ingot;
said ingot is scalped and hot rolled;
said ingot is at least one of solution treated, cold-rolled and stretched; and
said ingot is aged.

### Claim 4 (depends on 3)

The method of claim 3 where said ingot is aged artificially at about 300 to about 320° F. for about 29 to about 35 hours.

### Claim 5 (depends on 1)

The method of claim 1 wherein said weighing comprises weighing a mischmetal as a source of said at least one of said lanthanum, said strontium, said cerium and said praseodymium.

### Claim 6 (depends on 1)

The method of claim 1 further comprising subjecting the cast aluminum alloy to a solid-state joining process.

### Claim 7

A method for manufacturing an aluminum alloy comprising steps of:
subjecting an aluminum alloy to a solid-state joining process, wherein the aluminum alloy comprises:
aluminum;
about 1.8 to about 5.6 percent by weight copper;
about 0.6 to about 2.6 percent by weight lithium; and
at least one of:
lanthanum up to about 1.5 percent by weight;
strontium up to about 1.5 percent by weight;
cerium up to about 1.5 percent by weight; and
praseodymium up to about 1.5 percent by weight.

### Claim 8 (depends on 7)

The method of claim 7 further comprising aging the aluminum alloy before the solid-state joining process.

### Claim 9

A method for joining comprising:
friction stir welding an aluminum alloy, the aluminum alloy comprising:
aluminum;
about 1.8 to about 5.6 percent by weight copper;
about 0.6 to about 2.6 percent by weight lithium; and
at least one of:
lanthanum up to about 1.5 percent by weight;
strontium up to about 1.5 percent by weight;
cerium up to about 1.5 percent by weight; and
praseodymium up to about 1.5 percent by weight.

### Claim 10 (depends on 9)

The method of claim 9 wherein the composition further comprises silicon in a non-zero quantity up to about 0.20 percent by weight.

### Claim 11 (depends on 9)

The method of claim 9 wherein the composition further comprises iron in a non-zero quantity up to about 0.30 percent by weight.

### Claim 12 (depends on 9)

The method of claim 9 wherein the composition further comprises manganese in a non-zero quantity up to about 0.6 percent by weight.

### Claim 13 (depends on 9)

The method of claim 9 wherein the composition further comprises magnesium in a non-zero quantity up to about 1.9 percent by weight.

### Claim 14 (depends on 9)

The method of claim 9 wherein the composition further comprises chromium in a non-zero quantity up to about 0.10 percent by weight.

### Claim 15 (depends on 9)

The method of claim 9 wherein the composition further comprises zinc in a non-zero quantity up to about 1.0 percent by weight.

### Claim 16 (depends on 9)

The method of claim 9 wherein the composition further comprises titanium in a non-zero quantity up to about 0.15 percent by weight.

### Claim 17 (depends on 9)

The method of claim 9 wherein the composition further comprises silver in a non-zero quantity up to about 0.7 percent by weight.

### Claim 18 (depends on 9)

The method of claim 9 wherein the composition further comprises zirconium in a non-zero quantity up to about 0.16 percent by weight.

### Claim 19 (depends on 9)

The method of claim 9 wherein the composition further comprises at least one of nickel up to about 0.05 percent by weight, gallium up to about 0.05 percent by weight and vanadium up to about 0.05 percent by weight.

### Claim 20 (depends on 9)

The method of claim 9 wherein T1 phase is precipitated during the friction stir welding.