# US 2021/0277507 A1 · Electric resistance welded steel tubes for high-strength thin hollow stabilizers, and methods for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0277507 A1
- Document ID: US20210277507A1
- Status: Published application
- Kind: A1
- Application number: 16/326,420
- Filed: 2017-10-19
- Published: 2021-09-09
- Earliest claimed: 2016-10-24
- Assignees: Jfe Steel Corporation
- Applicants: JFE Steel Corporation
- Inventors: Masatoshi Aratani; Shinsaku Kokubo; Hiromichi Hori; Yoshikazu Kawabata; Ryoji Matsui
- Web page: https://patentgrep.com/patent/US20210277507A1

## CPC

- C22C 38/32: with boron
- C22C 38/48: with niobium or tantalum
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/0226: {Hot rolling}
- C21D 8/10: during manufacturing of tubular bodies
- C21D 9/08: for tubular bodies or pipes
- C21D 9/46: for sheet metals
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/20: with copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/28: with titanium or zirconium
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/50: with titanium or zirconium
- C22C 38/54: with boron
- B23K 2101/06: Tubes
- C21D 9/085: {Cooling or quenching}
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A method for manufacturing an electric resistance welded steel tube for high-strength thin hollow stabilizers is provided. A steel with a certain chemical composition is heated to a temperature of 1000 to 1300° C., hot rolled under conditions where the rolling finish temperature is 750 to 950° C., cooled, coiled into a coil at 500 to 650° C., and skin pass rolled with a rolling reduction ratio of not less than 0.3%. The resultant hot rolled sheet is electric resistance welded into an electric resistance welded steel tube, which is then reheated to a temperature of 800 to 1100° C. and hot stretch-reducing rolled under conditions where the rolling finish temperature is not more than 850° C. and the cumulative diameter reduction is not more than 75%. Consequently, a thin electric resistance welded steel tube is produced.

## Claims

### Claim 1

A method for manufacturing an electric resistance welded steel tube for high-strength thin hollow stabilizers, comprising heating, hot rolling and skin pass rolling processes where a steel is formed into a hot rolled sheet, a tube making process by an electric resistance welding is applied to the hot rolled sheet as a steel tube material into an electric resistance welded steel tube, and a hot stretch-reducing rolling process is applied to the reheated and hot stretch-reducing rolled electric resistance welded steel tube, making a product tube having a reduced diameter, wherein
the steel has a chemical composition comprising, in mass %:
C: 0.20 to 0.40%, Si: 0.1 to 1.0%,
Mn: 0.1 to 2.0%, P: not more than 0.1%,
S: not more than 0.01%, Al: 0.01 to 0.10%,
Cr: 0.01 to 1.0%, Ti: 0.01 to 0.05%,
B: 0.0005 to 0.0050%, Ca: 0.0001 to 0.0050%, and
N: not more than 0.010%, the balance being Fe and inevitable impurities,
the heating process for the steel comprises heating the steel to a heating temperature in the range of 1000 to 1300° C.,
the hot rolling process comprises hot rolling the steel under conditions where the rolling finish temperature is 750 to 950° C., cooling the steel sheet, and coiling the steel sheet into a coil at a coiling temperature of 500 to 650° C.,
the skin pass rolling process comprises skin pass rolling the steel sheet with a rolling reduction ratio of not less than 0.3%,
the hot stretch-reducing rolling process comprises reheating the electric resistance welded steel tube to a heating temperature of 800 to 1100° C., and hot stretch-reducing rolling the electric resistance welded steel tube to a reduced diameter under conditions where the rolling finish temperature is not more than 850° C. and the cumulative diameter reduction ratio is not more than 75%,
the product tube has a depth of a decarburized layer in wall thickness direction on the tube inner surface of not more than 120 μfrom the surface,
the product tube has a surface roughness Ra of the tube inner surface of 0.01 to 5.0 μm,
the product tube has a yield ratio of not less than 65%,
the product tube has a hardness expressed in Vickers hardness of not less than 450 HV as measured after the steel tube is formed into a stabilizer and is subjected to quenching and tempering treatment, and
the product tube has a wall thickness t of not more than 6 mm and a ratio t/D of the wall thickness t (mm) to the outer diameter D (mm) of not more than 0.2 and exhibits excellent fatigue resistance after being formed into a stabilizer and subjected to quenching and tempering treatment.

### Claim 2 (depends on 1)

The method for manufacturing an electric resistance welded steel tube for high-strength thin hollow stabilizers according to claim 1, wherein the hardness expressed in Vickers hardness is less than 550 HV as measured after the steel tube is formed into a stabilizer and is subjected to quenching and tempering treatment.

### Claim 3 (depends on 1)

The method for manufacturing an electric resistance welded steel tube for high-strength thin hollow stabilizers according to claim 1, wherein the chemical composition further comprises, in mass %, at least one selected from:
Cu: not more than 1%, Ni: not more than 1%, Nb: not more than 0.05%, W: not more than 0.05%, V: not more than 0.5%, and REM: not more than 0.02%.

### Claim 4

(canceled)

### Claim 5

(canceled)

### Claim 6

An electric resistance welded steel tube for high-strength thin hollow stabilizers manufactured by hot stretch-reducing rolling an electric resistance welded steel tube of a hot rolled steel sheet, wherein
the electric resistance welded steel tube has a chemical composition comprising, in mass %:
C: 0.20 to 0.40%, Si: 0.1 to 1.0%,
Mn: 0.1 to 2.0%, P: not more than 0.1%,
S: not more than 0.01%, Al: 0.01 to 0.10%,
Cr: 0.01 to 1.0%, Ti: 0.01 to 0.05%,
B: 0.0005 to 0.0050%, Ca: 0.0001 to 0.0050%, and
N: not more than 0.010%, the balance being Fe and inevitable impurities,
the depth of a decarburized layer in wall thickness direction on the tube inner surface is not more than 120 μm from the surface,
the surface roughness Ra of the tube inner surface is 0.01 to 5.0
the yield ratio is not less than 65%,
the hardness expressed in Vickers hardness is not less than 450 HV as measured after the steel tube is formed into a stabilizer and is subjected to quenching and tempering treatment, and the electric resistance welded steel tube has a wall thickness t of not more than 6 mm and a ratio t/D of the wall thickness t (mm) to the outer diameter D (mm) of not more than 0.2 and exhibits excellent fatigue resistance after being formed into a stabilizer and subjected to quenching and tempering treatment.

### Claim 7 (depends on 6)

The electric resistance welded steel tube for high-strength thin hollow stabilizers according to claim 6, wherein the hardness expressed in Vickers hardness is less than 550 HV as measured after the steel tube is formed into a stabilizer and is subjected to quenching and tempering treatment

### Claim 8 (depends on 6)

The electric resistance welded steel tube for high-strength thin hollow stabilizers according to claim 6, wherein the chemical composition further comprises, in mass %, at least one selected from:
Cu: not more than 1%, Ni: not more than 1%, Nb: not more than 0.05%, W: not more than 0.05%, V: not more than 0.5%, and REM: not more than 0.02%.

### Claim 9

(canceled)

### Claim 10

(canceled)

### Claim 11 (depends on 2)

The method for manufacturing an electric resistance welded steel tube for high-strength thin hollow stabilizers according to claim 2, wherein the chemical composition further comprises, in mass %, at least one selected from:
Cu: not more than 1%, Ni: not more than 1%, Nb: not more than 0.05%, W: not more than 0.05%, V: not more than 0.5%, and REM: not more than 0.02%.

### Claim 12 (depends on 7)

The electric resistance welded steel tube for high-strength thin hollow stabilizers according to claim 7, wherein the chemical composition further comprises, in mass %, at least one selected from:
Cu: not more than 1%, Ni: not more than 1%, Nb: not more than 0.05%, W: not more than 0.05%, V: not more than 0.5%, and REM: not more than 0.02%.