# US 2021/0277290 A1 · Propylene random copolymer based hot melt adhesive composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0277290 A1
- Document ID: US20210277290A1
- Status: Published application
- Kind: A1
- Application number: 17/260,865
- Filed: 2018-08-05
- Published: 2021-09-09
- Earliest claimed: 2018-08-05
- Applicants: Borealis AG
- Inventors: Jingbo Wang; Carl-Gustaf Ek; Klaus Bernreitner; Jose Miguel Martin-Martinez; Alfonso Delucas-Freile; Monica Fuensanta-Soriano
- Web page: https://patentgrep.com/patent/US20210277290A1

## CPC

- C09J 123/14: Copolymers of propene (C09J123/16 takes precedence)
- C09J 123/20: having four to nine carbon atoms
- C09J 7/35: Heat-activated
- C09J 145/00: Adhesives based on homopolymers or copolymers of compounds having no unsaturated aliphatic radicals in a side chain, and having one or more carbon-to-carbon double bonds in a carbocyclic or in a heterocyclic system; Adhesives based on derivatives of such polymers (based on polymers of cyclic esters of polyfunctional acids C09J131/00; based on polymers of cyclic anhydrides or imides C09J135/00)
- C09J 147/00: Adhesives based on homopolymers or copolymers of compounds having one or more unsaturated aliphatic radicals, at least one having two or more carbon-to-carbon double bonds; Adhesives based on derivatives of such polymers (C09J145/00 takes precedence; based on conjugated diene rubbers C09J109/00 - C09J121/00)
- C09J 193/04: Rosin
- C08F 210/06: Propene
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2207/02: Heterophasic composition
- C09J 2423/00: Presence of polyolefin
- C09J 2423/10: Presence of homo or copolymers of propene
- C09J 2423/16: Presence of ethen-propene or ethene-propene-diene copolymers
- C09J 2493/00: Presence of natural resin
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present application relates to an adhesive composition comprising a polypropylene resin, a tackifying resin and a plasticizer resin having a superior balance of properties in regard of Brookfield viscosity and maximum probe tack. It further relates to an article comprising the adhesive composition and to a process for producing said article. The application also relates to the use of the adhesive composition in the preparation of an article.

## Claims

### Claim at position 1

1-15. (canceled)

### Claim 16

An adhesive composition comprising:
(A) a polypropylene resin comprising a multimodal propylene random copolymer (R-PP), being a multimodal random copolymer of propylene and one or more comonomer(s) selected from ethylene and C4-C10 alpha olefins, with a melt flow rate MFR2 of at least 50 g/10 min, determined according to ISO 1133 at a temperature of 230° C. and a load of 2.16 kg, and a propylene copolymer (PC) which is different from the multimodal propylene random copolymer, wherein the weight ratio of the multimodal propylene random copolymer (R-PP) and the propylene copolymer (PC) in the polypropylene resin is from 1:2 to 5:1,
(B) a tackifying resin selected from polyterpene resins, C5-C10 aliphatic hydrocarbon resins, aromatic modified aliphatic resins, or mixtures thereof, and
(C) a plasticizer resin selected from microcrystalline waxes, paraffin waxes, ionomer waxes, Fischer-Tropsch waxes, montan-based waxes, and mineral or petroleum based oils and mixtures thereof,
wherein the adhesive composition has a Brookfield viscosity at 160° C. of less than 60,000 mPa▪ as measured according to ASTM D-3236 and a maximum probe tack of at least 150 kPa as measured according to probe tack test protocol.

### Claim 17 (depends on 16)

The adhesive composition according to claim 16, having a T-peel strength of at least 5 N/m, when the adhesive composition is in direct contact with substrate that is an untreated polypropylene film.

### Claim 18 (depends on 16)

The adhesive composition according to claim 16, having a T-peel strength of at least 20 N/m when the adhesive composition is in direct contact with substrate that is an atmospheric pressure plasma jet (APPJ) surface treated polypropylene film.

### Claim 19 (depends on 16)

The adhesive composition according to claim 16, having a single-lap shear strength of from 0.05 to 0.4 MPa, when the adhesive composition is in direct contact with a substrate that is a polypropylene film with a thickness of 300 μm.

### Claim 20 (depends on 16)

The adhesive composition according to claim 16, having a single-lap shear strength of from 0.5 to 4.0 MPa, when the adhesive composition is in direct contact with a steel substrate.

### Claim 21 (depends on 16)

The adhesive composition according to claim 16, having a softening point of not more than 160° C.

### Claim 22 (depends on 16)

The adhesive composition according to claim 16, having an open time of at least 2 s.

### Claim 23 (depends on 16)

The adhesive composition according to claim 16, wherein the adhesive composition consists of:
(A) from 10 to 60% by weight of the polypropylene resin,
(B) from 20 to 90% by weight of the tackifying resin,
(C) from 1.0 to 60% by weight of the plasticizer resin,
(D) from 0 to 50% by weight of a filler, and
(E) from 0 to 5.0% by weight of additives.

### Claim 24 (depends on 16)

The adhesive composition according to claim 16, wherein the propylene copolymer (PC) has:
a) at least one comonomer selected from ethylene and C4-C12 alpha-olefins,
b) a total comonomer content in the range of 4.5 to 20.0% by weight, based on the total weight amount of monomer units in the propylene copolymer (PC),
c) a Vicat-A temperature >80° C., as measured according to ISO 306,
d) a storage modulus (G′23) in the range of from 100 to 1000 MPa, as measured at 23° C. according to ISO 6721-02 and ISO 6721-07, and
e) a melting temperature in the range of from 120° C. to 160° C., as measured according to ISO 11357-3.

### Claim 25 (depends on 11)

The adhesive composition according to claim 11, wherein the weight ratio of the propylene random copolymer (R-PP) and the propylene copolymer (PC) in the polypropylene resin is from 1:1 to 4:1.

### Claim 26 (depends on 16)

The adhesive composition according to claim 16, wherein the plasticizer resin (C) is selected from a wax, a mineral based oil, a petroleum based oil or mixtures thereof.

### Claim 27 (depends on 16)

An article comprising the adhesive composition according to claim 16, and at least one substrate, wherein the adhesive composition is in direct contact with at least one surface of said substrate.