# US 2021/0277259 A1 · Method of using water erodible marine antifouling coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0277259 A1
- Document ID: US20210277259A1
- Status: Published application
- Kind: A1
- Application number: 16/809,152
- Filed: 2020-03-04
- Published: 2021-09-09
- Earliest claimed: 2020-03-04
- Assignees: King Fahd University of Petroleum and Minerals
- Applicants: King Fahd University of Petroleum and Minerals
- Inventors: Mohammad Mizanur RAHMAN; Md. Hasan Zahir; Mohammad Abu Jafar Mazumder
- Web page: https://patentgrep.com/patent/US20210277259A1

## CPC

- C09D 5/1662: {Synthetic film-forming substance}
- B05D 1/005: {Spin coating}
- B05D 1/007: {using an electrostatic field (B05D1/02 - B05D1/16 take precedence)}
- B05D 1/02: performed by spraying
- B05D 1/04: involving the use of an electrostatic field {(B05D1/025 and B05D1/14 take precedence)}
- B05D 1/18: performed by dipping
- B05D 1/28: performed by transfer from the surfaces of elements carrying the liquid or other fluent material, e.g. brushes, pads, rollers
- C08B 37/0033: {Xanthan, i.e. D-glucose, D-mannose and D-glucuronic acid units, saubstituted with acetate and pyruvate, with a main chain of (beta-1,4)-D-glucose units; Derivatives thereof}
- C08G 18/0823: {containing carboxylate salt groups or groups forming them}
- C08G 18/10: Prepolymer processes involving reaction of isocyanates or isothiocyanates with compounds having active hydrogen in a first reaction step
- C08G 18/246: {containing also tin-carbon bonds}
- C08G 18/348: {Hydroxycarboxylic acids}
- C08G 18/4854: {Polyethers containing oxyalkylene groups having four carbon atoms in the alkylene group}
- C08G 18/6484: {Polysaccharides and derivatives thereof}
- C08G 18/6692: {with compounds of group C08G18/34}
- C08J 7/0427: {with only one layer of a composition containing a polymer binder (with more layers C08J7/042)}
- C08J 7/12: Chemical modification
- C09D 5/1625: {organic}
- C09D 175/04: Polyurethanes
- C08J 2327/06: Homopolymers or copolymers of vinyl chloride
- C08J 2405/00: Characterised by the use of polysaccharides or of their derivatives not provided for in groups C08J2401/00 or C08J2403/00
- C08J 2475/04: Polyurethanes
- C08K 5/0041: {Optical brightening agents, organic pigments}
- C08K 5/56: Organo-metallic compounds, i.e. organic compounds containing a metal-to-carbon bond
- C08L 5/02: Dextran; Derivatives thereof
- C08L 5/14: Hemicellulose; Derivatives thereof
- Y02P 20/582: Recycling of unreacted starting or intermediate materials
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C08B: POLYSACCHARIDES; DERIVATIVES THEREOF (polysaccharides containing less than six saccharide radicals attached to each other by glycosidic linkages C07H; fermentation or enzyme-using processes C12P19/00; sugar industry C13; production of cellulose D21)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method is described for inhibiting marine fouling on a surface. The surface is contacted with a composition comprising a waterborne polyurethane that is crosslinked with an acrylic acid functionalized polysaccharide, water, and a preservative. The composition is then dried to form a deposited film. The polysaccharide may be xanthan.

## Claims

### Claim 1

A method of inhibiting marine fouling of a surface, the method comprising:
contacting the surface with a composition to produce a coated surface, the composition comprising:
a waterborne polyurethane (WBPU) crosslinked with an acrylic acid functionalized polysaccharide;
water; and
a preservative dispersed in the crosslinked WBPU, and
drying the coated surface to produce a treated surface having a deposited film.

### Claim 2 (depends on 1)

The method of claim 1, wherein the acrylic acid functionalized polysaccharide is present in the deposited film at a weight percentage of 0.1-5.0 wt % relative to a total weight of the deposited film.

### Claim 3 (depends on 1)

The method of claim 1, wherein the polysaccharide is at least one selected from the group consisting of xanthan, beta-glucan, dextran, inulin, galactan, glycogen, hemicellulose, levan, lignin, mannan, pectin, amylopectin, and amylose.

### Claim 4 (depends on 1)

The method of claim 1, wherein the acrylic acid functionalized polysaccharide comprises 1-50 wt % acrylic acid functional groups relative to a total weight of the acrylic acid functionalized polysaccharide.

### Claim 5 (depends on 1)

The method of claim 1, wherein the polysaccharide is xanthan.

### Claim 6 (depends on 1)

The method of claim 1, wherein the composition comprises 50-90 wt % water relative to a total weight of the composition.

### Claim 7 (depends on 1)

The method of claim 1, wherein the preservative is present at a weight percentage of 0.01-2.0 wt % relative to a total weight of the composition.

### Claim 8 (depends on 1)

The method of claim 1, wherein the composition further comprises a pigment.

### Claim 9 (depends on 1)

The method of claim 1, wherein the composition consists of the crosslinked WBPU, the preservative, and water.

### Claim 10 (depends on 1)

The method of claim 1, wherein the contacting is done by electrocoating, spraying, electrostatic spraying, dipping, rolling, brushing, dropping, spin coating.

### Claim 11 (depends on 1)

The method of claim 1, wherein the preservative is zinc pyrithione.

### Claim 12 (depends on 1)

The method of claim 1, wherein the deposited film has a density in a range of 0.8-2.0 g/cm3.

### Claim 13 (depends on 1)

The method of claim 1, wherein the crosslinked WBPU has a number average molecular weight in a range of 26-32 kDa.

### Claim 14 (depends on 13)

The method of claim 13, wherein the number average molecular weight decreases to 22-24 kDa following at least 24 h of immersion in water, seawater, or brine.

### Claim 15 (depends on 1)

The method of claim 1, wherein the deposited film has a water contact angle in a range of 45°-67°.

### Claim 16 (depends on 1)

The method of claim 1, wherein the deposited film, when immersed in water, seawater, or brine for at least 24 hours, absorbs no more than 15 wt % water in relation to a weight of the deposited film.

### Claim 17 (depends on 1)

The method of claim 1, wherein the deposited film is in the form of a layer in direct contact with the surface, the deposited film having an average thickness in a range of 1-200 μm.

### Claim 18 (depends on 1)

The method of claim 1, wherein the deposited film, when placed in contact with water, seawater, or brine for 90 days, has a dry weight loss in a range of 1.5-8.0 wt % relative to an initial dry weight.

### Claim 19 (depends on 1)

The method of claim 1, wherein the deposited film has an adhesive strength in a range of 3.8-4.5 Kgf/cm.

### Claim 20 (depends on 1)

The method of claim 1, wherein the adhesive strength decreases to 1.8-3.5 Kgf/cm following at least 24 h of immersion in water, seawater, or brine.