# US 2021/0277232 A1 · Thermoplastic polymer powder for selective laser sintering (sls)

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0277232 A1
- Document ID: US20210277232A1
- Status: Published application
- Kind: A1
- Application number: 16/330,581
- Filed: 2017-09-07
- Published: 2021-09-09
- Earliest claimed: 2016-09-08
- Assignees: Ineos Styrolution Group GmbH
- Applicants: Ineos Styrolution Group GmbH
- Inventors: Bianca WILHELMUS; Norbert NIESSNER; Viktor WIEBE; Frank EISENTRAEGER
- Web page: https://patentgrep.com/patent/US20210277232A1

## CPC

- C08L 77/02: Polyamides derived from omega-amino carboxylic acids or from lactams thereof (C08L77/10 takes precedence)
- B29C 64/153: using layers of powder being selectively joined, e.g. by selective laser sintering or melting
- B29C 64/314: Preparation
- B33Y 10/00: Processes of additive manufacturing
- B33Y 40/10: Pre-treatment
- B33Y 70/00: Materials specially adapted for additive manufacturing
- C08L 51/04: grafted on to rubbers
- C08L 55/02: ABS [Acrylonitrile-Butadiene-Styrene] polymers
- C08L 67/04: Polyesters derived from hydroxycarboxylic acids, e.g. lactones (C08L67/06 takes precedence)
- B29C 2035/0838: {using laser}
- B29K 2101/12: Thermoplastic materials
- B29K 2995/0026: Transparent
- B29K 2995/0029: Translucent
- C08L 2203/30: used for thermoforming
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

The present invention relates to a thermoplastic polymer powder and to the use thereof as material for selective laser sintering (SLS). The polymer powder contains a partially crystalline polymer, an amorphous polymer and a compatibilizing agent, and optionally additional additives and/or auxiliary substances, wherein the partially crystalline polymer, the amorphous polymer and the compatibilizing agent are in the form of a polymer blend. The invention also relates to a method for producing the thermoplastic polymer powder and to a method of selective laser sintering (SLS).

## Claims

### Claim at position 1

1-15. (canceled)

### Claim 16

A thermoplastic polymer powder P comprising
(A) from 10 to 89.9% by weight, based on the entire polymer powder P, of at least one semicrystalline polymer A;
(B) from 10 to 89.9% by weight, based on the entire polymer powder P, of at least one amorphous polymer B, where the amorphous polymer B is at least one polymer selected from the group consisting of styrene-butadiene block copolymers, acrylonitrile-butadiene-styrene copolymers, styrene-acrylonitrile copolymers, a(alpha)-methylstyrene-acrylonitrile copolymers, acrylate-styrene-acrylonitrile copolymers, methyl methacrylate-acrylonitrile-butadiene-styrene copolymers, methyl methacrylate-butadiene-styrene copolymers, styrene-methyl methacrylate copolymers, amorphous polystyrene, and impact-modified polystyrene;
(C) from 0.1 to 15% by weight, based on the entire polymer powder P, of at least one compatibilizer C, selected from the group consisting of styrene-acrylonitrile-maleic anhydride terpolymers, styrene-N-phenylmaleimide-maleic anhydride terpolymers, and methylmethacrylate-maleic anhydride copolymers;
(D) optionally from 0 to 5% by weight, based on the entire polymer powder P, of at least one additive and/or auxiliary;
where the sum of the % s by weight of components A, B, C, and optionally D is 100% by weight;
where the semicrystalline polymer A, the amorphous polymer B, and the compatibilizer C are present in the form of a polymer blend;
and where the D50 median particle diameter of the thermoplastic powder P is in the range from 5 to 200 μm.

### Claim 17 (depends on 16)

The thermoplastic polymer powder P of claim 16, wherein the semicrystalline polymer A is at least one polymer selected from the group consisting of polyamides, polyetherketones, polylactides, polybutyleneterephthalate, polyethylene, polypropylene, and syndiotactic polystryene.

### Claim 18 (depends on 16)

The thermoplastic polymer powder P of claim 16, wherein the semicrystalline polymer A is at least one polyamide selected from the group consisting of PA6 (polycaprolactam); PA6,6 (polyhexamethyleneadipamide); PA4,6 (polytetramethyleneadipamide); PA5,10 (polypentamethyleneadipamide); PA6,10 (polyhexamethylenesebacamide); PA7 (polyeneantholactam); PA11 (polyundecanolactam); and PA12 (polylaurolactam).

### Claim 19 (depends on 16)

The thermoplastic polymer powder P of claim 16, wherein the amorphous polymer B is at least one styrene polymer or styrene copolymer which has a volume melt flow index in the range from 2 to 60 cm3/10 min, measured in accordance with ISO 1133, at 220° C. and with a load of 10 kg.

### Claim 20 (depends on 16)

The thermoplastic polymer powder P of claim 16, wherein the D90 particle diameter of the polymer powder P is less than 200 μm.

### Claim 21 (depends on 16)

The thermoplastic polymer powder P of claim 16, comprising
(A) from 30 to 66% by weight, based on the entire polymer powder P, of at least one polyamide selected from the group consisting of polycaprolactam PA6; polyhexamethyleneadipamide PA6,6; polyundecanolactam PA11; and polylaurolactam PA12, as semicrystalline polymer A;
(B) from 30 to 66% by weight, based on the entire polymer powder P, of at least one polymer selected from the group consisting of styrene-butadiene block copolymers, acrylonitrile-butadiene-styrene copolymers, styrene-acrylonitrile copolymers, a(alpha)-methylstyrene-acrylonitrile copolymers, acrylate-styrene-acrylonitrile copolymers, methyl methacrylate-acrylonitrile-butadiene-styrene copolymers, methyl methacrylate-butadiene-styrene copolymers, styrene-methyl methacrylate copolymers, amorphous polystyrene, and impact-modified polystyrene, as amorphous polymer B;
(C) from 4 to 10% by weight, based on the entire polymer powder P, of a styrene-acrylonitrile-maleic anhydride terpolymer with maleic anhydride content in the range from 0.4 to 3% by weight, based on the entire terpolymer, as compatibilizer C;
(D1) from 0.1 to 3% by weight, based on the entire polymer powder P, of at least one silicon dioxide nanoparticle powder or silicone additive as powder-flow aid; and
(D2) optionally from 0 to 3% by weight, based on the entire polymer powder P, of at least one further additive and/or auxiliary as further component D.

### Claim 22 (depends on 16)

A process for the production of a thermoplastic polymer powder P of claim 16, comprising the following steps:
i) provision of a solid mixture comprising components A, B, C, and optionally D;
ii) mechanical comminution of the solid mixture, whereupon a thermoplastic polymer powder P is obtained which has a D50 median particle diameter in the range from 5 to 200 μm.

### Claim 23 (depends on 22)

The process of claim 22, wherein step i) comprises the mixing of components A, B, and C in the liquid state at a temperature in the range from 200 to 250° C.

### Claim 24 (depends on 22)

The process of claim 22, wherein the mechanical comminution of the solid mixture in step ii) is achieved by grinding, micronizing, freeze-grinding, or jet-milling.

### Claim 25 (depends on 16)

A process for the production of a three-dimensional component by selective laser sintering comprising the steps of:
x) provision of a powder layer consisting of the thermoplastic polymer powder P of claim 16 in a construction chamber;
xi) localized melting by a directed beam of electromagnetic radiation, followed by solidification of the thermoplastic polymer powder P in a defined region;
where the steps x) and xi) are repeated so that a three-dimensional component is obtained layer-by-layer via bonding of the regions of the molten and resolidified polymer.

### Claim 26 (depends on 25)

The process of claim 25, wherein the thickness of the powder layer is in the range from 100 to 200 μm.

### Claim 27 (depends on 25)

The process of claim 25, wherein the process involves the production of a transparent or translucent component.