# US 2021/0277192 A1 · Producing semi-crystalline pulverulent polycarbonate and use thereof in additive manufacturing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0277192 A1
- Document ID: US20210277192A1
- Status: Published application
- Kind: A1
- Application number: 17/190,030
- Filed: 2021-03-02
- Published: 2021-09-09
- Earliest claimed: 2020-03-03
- Assignees: Jabil Inc.
- Applicants: Jabil Inc.
- Inventors: Thomas Gardner; Travis Hislop; Victoria H. Pyle
- Web page: https://patentgrep.com/patent/US20210277192A1

## CPC

- C08J 3/14: by precipitation from solutions {(C08J3/122 takes precedence)}
- B29C 64/153: using layers of powder being selectively joined, e.g. by selective laser sintering or melting
- B29C 64/314: Preparation
- B33Y 10/00: Processes of additive manufacturing
- B33Y 40/10: Pre-treatment
- B33Y 70/00: Materials specially adapted for additive manufacturing
- C08G 64/40: Post-polymerisation treatment
- B29K 2069/00: Use of PC, i.e. polycarbonates {or derivatives thereof}, as moulding material
- B29K 2105/251: {Particles, powder or granules (expandable particles B29K2105/046)}
- B29K 2995/004: Semi-crystalline
- B29K 2995/0097: Thickness
- C08J 2369/00: Characterised by the use of polycarbonates; Derivatives of polycarbonates
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

Ways of preparing a partially crystalline polycarbonate powder are provided that include dissolving an amorphous polycarbonate in a polar aprotic solvent to form a first solution of solubilized polycarbonate at a first temperature. The first solution is then cooled to a second temperature, the second temperature being lower than the first temperature, where a portion of the solubilized polycarbonate precipitates from the first solution to form a second solution including the partially crystalline polycarbonate powder. Certain partially crystalline polycarbonate powders resulting from such methods are particularly useful in additive manufacturing processes, including powder bed fusion processes.

## Claims

### Claim 1

A method of preparing a partially crystalline polycarbonate powder, the method comprising:
dissolving an amorphous polycarbonate in a polar aprotic solvent to form a first solution of solubilized polycarbonate at a first temperature; and
cooling the first solution to a second temperature, the second temperature being lower than the first temperature, wherein a portion of the solubilized polycarbonate precipitates from the first solution to form a slurry comprised of the partially crystalline polycarbonate powder and a less-than-saturated or saturated solution of the polycarbonate.

### Claim 2 (depends on 1)

The method of claim 1, further comprising separating the partially crystalline polycarbonate powder from the slurry.

### Claim 3 (depends on 2)

The method of claim 2, wherein, prior to or during the separating, a low molecular weight miscible solvent that does not dissolve the polycarbonate is added to the slurry.

### Claim 4 (depends on 3)

The method of claim 3, wherein the low molecular weight miscible solvent is a C1 to C4 alcohol and the separation is performed using filtration.

### Claim 5 (depends on 1)

The method of claim 1, further comprising repeating the dissolving step using the remainder of the second solution as the polar aprotic solvent and repeating the cooling step to form the second solution including another partially crystalline polycarbonate powder, wherein at least a portion of the polycarbonate dissolved is leftover from the prior dissolving and precipitating.

### Claim 6 (depends on 1)

The method of claim 1, wherein the polar aprotic solvent is comprised of one or more of the following: dimethyl sulfoxide; diphenyl ether; or anisole.

### Claim 7 (depends on 1)

The method of claim 1, wherein the dissolving step includes heating the amorphous polycarbonate in the polar aprotic solvent to form the first solution of solubilized polycarbonate at the first temperature, the first temperature being greater than room temperature.

### Claim 8 (depends on 7)

The method of claim 7, wherein the cooling step includes cooling the first solution to the second temperature at a cooling rate, the second temperature being room temperature and the cooling rate being at most about 5° C./min.

### Claim 9 (depends on 1)

The method of claim 1, wherein the partially crystalline polycarbonate powder has one or more of: (i) a D90 particle size of less than about 150 μm, (ii) a D10 of at least 10 μm or (iii) an average particle size of about 30 μm to about 40 μm.

### Claim 10 (depends on 9)

The method of claim 9, wherein the partially crystalline polycarbonate powder has at least about 90% of the particles by number having a circularity of 0.65 or greater.

### Claim 11 (depends on 10)

The method of claim 10, wherein the partially crystalline polycarbonate powder has a crystallinity of at least about 20% to 35%.

### Claim 12

A powder composition comprising a partially crystalline polycarbonate powder having a D90 particle size of less than about 150 μm, an average particle diameter from about 30 μm to about 40 μm, and a crystallinity between about 20% and about 35%.

### Claim 13 (depends on 12)

The powder composition of claim 12, wherein the partially crystalline polycarbonate powder has a flowability of at least about 0.5 g/s as determined by Method A of ASTM D 1895 using a 15 mm nozzle.

### Claim 14 (depends on 12)

The powder composition of claim 12, wherein the partially crystalline polycarbonate powder has a circularity such that at least about 90% of the particles by number have a circularity of 0.65 or greater.

### Claim 15 (depends on 12)

An object prepared by an additive manufacturing process comprising:
fusing the powder composition of claim 12 in a powder bed fusion process to form the object.

### Claim 16 (depends on 1)

The method of claim 1, wherein the concentration of the polycarbonate in the first solution is about 5% to about 30% by weight.

### Claim 17 (depends on 12)

The powder composition of claim 12, wherein the partially crystalline polycarbonate powder has a D10 of at least 10 μm.

### Claim 18 (depends on 1)

The method of claim 1, wherein the first temperature is from about 100° C. to 150° C.

### Claim 19 (depends on 25)

The method of claim 25, wherein the first temperature is at most about 145° C.

### Claim 20 (depends on 1)

The method of claim 1, wherein the dissolving and cooling are carried out under a pressure within 1% of atmospheric pressure.