# US 2021/0276233 A1 · Automotive molded-in-color thermoplastic polyolefin with clear coating for paint replacement and high gloss applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0276233 A1
- Document ID: US20210276233A1
- Status: Published application
- Kind: A1
- Application number: 17/193,738
- Filed: 2021-03-05
- Published: 2021-09-09
- Earliest claimed: 2020-03-06
- Assignees: LyondellBasell Advanced Polymers Inc.
- Applicants: Lyondellbasell Advanced Polymers Inc.
- Inventors: PETER J. GLENISTER; QUENTIN R. BOLL; PERRY J. BANTA; CHANGLAI YANG
- Web page: https://patentgrep.com/patent/US20210276233A1

## CPC

- B29C 45/0001: {characterised by the choice of material}
- B29C 45/0013: {using fillers dispersed in the moulding material, e.g. metal particles}
- B29C 45/0053: {combined with a final operation, e.g. shaping (injection-compression moulding B29C45/561)}
- C08L 23/12: Polypropene
- B29C 2045/0079: {applying a coating or covering}
- B29K 2023/12: {PP, i.e. polypropylene}
- B29K 2023/16: {EPM, i.e. ethylene-propylene copolymers; EPDM, i.e. ethylene-propylene-diene copolymers; EPT, i.e. ethylene-propylene terpolymers}
- B29K 2023/18: {Polymers of hydrocarbons having four or more carbon atoms, e.g. polymers of butylene, e.g. PB, i.e. polybutylene}
- B29K 2503/08: Mineral aggregates, e.g. sand, clay or the like
- B29K 2995/002: Coloured
- B29K 2995/0022: Bright, glossy or shiny surface
- B29K 2995/0063: Density
- B29K 2995/0077: Yield strength; Tensile strength
- B29K 2995/0082: Flexural strength; Flexion stiffness
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2205/08: containing additives to improve the compatibility between two polymers
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

Molded-in-color thermoplastic polyolefin (TPO) compositions useful for making automotive components, such as injection molded parts, as well as other articles of manufacture are described. The molded-in-color composition has a ΔE* value≤2.0 (compared to a painted color master), a gloss measured at 60° from about 76 to about 90 GU, a density ranging from about 0.9 to about 0.97 g/cm3, a melt mass flow rate from about 15 to about 40 g/10 min (ASTM D 1238, 230° C./2.16 kg), a flexural modulus between about 600 to about 2000 MPa, and an as-molded shrinkage between about 0.6% and about 1.4%. The compositions can be used to prepare molded-in-color components that can undergo additional clear coating steps as required by the automotive application. The clear coated molded-in-color components have a gloss measured at 20° from about 85 to about 95 GU and a gloss retention after mar between about 85% and about 93%.

## Claims

### Claim 1

A molded-in-color composition comprising:
a) a polyolefin resin composition;
b) at least one elastomer;
c) an additive package; and
d) one or more colorants,
wherein the molded-in-color composition has a ΔE* value≤2.0 (compared to a painted color master), a gloss measured at 60° from about 76 to about 90 GU, density from about 0.89 to about 0.97 g/cm3, a melt mass flow rate (MFR) from about 15 to about 40 g/10 min (ASTM D 1238, 230° C./2.16 kg), a flexural modulus between about 600 to about 2000 MPa, and an as-molded shrinkage between about 0.6% and about 1.4%.

### Claim 2 (depends on 1)

The molded-in-color composition of claim 1, wherein the polyolefin resin composition comprises a first polyolefin having a high MFR that is from about 50 to about 200 g/10 min (ASTM D 1238, 230° C./2.16 kg), and a second polyolefin has a low MFR that is from about 1 to about 5 g/10 min (ASTM D 1238, 230° C./2.16 kg).

### Claim 3 (depends on 1)

The molded-in-color composition of claim 1, further comprising a mineral filler present in an amount up to 7 weight percent of the total composition weight.

### Claim 4 (depends on 1)

The molded-in-color composition of claim 1, further comprising a compatibilizer.

### Claim 5 (depends on 1)

The molded-in-color composition of claim 1, further comprising both a mineral filler present in an amount up to 7 weight percent of the total composition weight and a compatibilizer.

### Claim 6 (depends on 1)

The molded-in-color composition of claim 1, wherein the molded-in-color composition has a tensile strength at yield from about 16 to about 26 MPa.

### Claim 7 (depends on 1)

An article formed from the molded-in-color composition of claim 1.

### Claim 8 (depends on 7)

The article of claim 7, wherein the article is a part of an automobile.

### Claim 9 (depends on 8)

The article of claim 8, further comprising a clear coat.

### Claim 10 (depends on 9)

The article of claim 9, wherein the coated article has a gloss at 20° between about 85 to about 95 GU, and a gloss retention after mar between about 85% and about 93%.

### Claim 11

A method of forming an article comprising:
a) melt blending a molded-in-color composition comprising:
i) a polyolefin composition comprising at least one polyolefin, wherein the total amount of the polyolefin composition present in the molded-in-color composition ranges from about 50 wt % to about 80 wt %, based on a total weight of the composition;
ii) at least one elastomer, wherein the total amount of elastomer present in the composition ranges from about 5 wt % to about 25 wt %, based on a total weight of the composition;
iii) an additive package present in an amount ranging from greater than 0 wt % to about 2 wt %, based on a total weight of the composition;
iv) a colorant package present in an amount ranging from greater than 0 wt % to about 5 wt %, based on a total weight of the composition;
v) wherein the composition has a ΔE* value≤2.0 (compared to a painted color master), a density ranging from about 0.9 to about 0.97 g/cm3, a melt mass flow rate (MFR) from about 15 to about 40 g/10 min (ASTM D 1238, 230° C./2.16 kg), a flexural modulus between about 600 to about 2000 MPa, and an as-molded shrinkage between about 0.6% and about 1.4%; and,
b) molding the melt blended composition into an article, wherein said article has a gloss measured at 60° from about 76 to about 90 GU.

### Claim 12 (depends on 11)

The method of claim 11, further comprising the step of priming said article and coating the primed article with a clear coat, wherein said clear coated article has a gloss measured at 20° from about 85 to about 95 GU and a gloss retention after mar between about 85% and about 93%.

### Claim 13 (depends on 11)

The method of claim 11, wherein said molded-in-color composition in step a) further comprises a filler present in an amount up to 7 wt %, based on the total weight of the composition.

### Claim 14 (depends on 11)

The method of claim 11, wherein said molded-in-color composition in step a) further comprises at least one compatibilizer, wherein the total amount of compatibilizer present in the composition ranges from about 5 wt % to about 25 wt %, based on a total weight of the composition.

### Claim 15 (depends on 11)

The method of claim 11, wherein said article is a part of an automobile.

### Claim 16 (depends on 12)

The method of claim 12, wherein said article is a part of an automobile.

### Claim 17 (depends on 11)

The method of claim 11, wherein the polyolefin composition comprises a first polyolefin having a high MFR that is from about 50 to about 200 g/10 min (ASTM D 1238, 230° C./2.16 kg), and a second polyolefin has a low MFR that is from about 1 to about 5 g/10 min (ASTM D 1238, 230° C./2.16 kg).

### Claim 18

A method of forming an article comprising:
a) melt blending a molded-in-color composition comprising:
i) a polyolefin composition comprising a first polyolefin having a high MFR that is from about 50 to about 200 g/10 min (ASTM D 1238, 230° C./2.16 kg), and a second polyolefin has a low MFR that is from about 1 to about 5 g/10 min (ASTM D 1238, 230° C./2.16 kg), wherein the total amount of thermoplastic polyolefin present in the composition ranges from about 50 wt % to about 80 wt %, based on a total weight of the composition;
ii) at least one elastomer, wherein the total amount of elastomer present in the composition ranges from about 5 wt % to about 25 wt %, based on a total weight of the composition;
iii) at least one compatibilizer, wherein the total amount of compatibilizer present in the composition ranges from about 5 wt % to about 15 wt %, based on a total weight of the composition;
iv) an additive package present in an amount ranging from greater than 0 wt % to about 2 wt %, based on a total weight of the composition; and
v) a colorant package present in an amount ranging from greater than 0 wt % to about 5 wt %, based on a total weight of the composition;
wherein the composition has a ΔE* value≤2.0 (compared to a painted color master), a density ranging from about 0.9 to about 0.97 g/cm3, a melt mass flow rate from about 15 to about 40 g/10 min (ASTM D 1238, 230° C./2.16 kg), a flexural modulus between about 600 to about 2000 MPa, and an as-molded shrinkage between about 0.6% and about 1.4%; and,
b) molding said melt blended composition into an article, wherein said article has a gloss measured at 60° from about 76 to about 90 GU.

### Claim 19 (depends on 18)

The method of claim 18, wherein said molded-in-color further comprises a filler present in an amount up to 7 wt %, based on the total weight of the composition.

### Claim 20 (depends on 18)

The method of claim 18, further comprising the step of priming said article and coating the primed article with a clear coat, wherein said clear coated article has a gloss measured at 20° from about 85 to about 95 GU and a gloss retention after mar between about 85% and about 93%.