# US 2021/0268563 A1 · Systems and methods for production of metallurgically bonded clad billet and products thereof, and metallurgically bonded clad billet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0268563 A1
- Document ID: US20210268563A1
- Status: Published application
- Kind: A1
- Application number: 17/325,586
- Filed: 2021-05-20
- Published: 2021-09-02
- Earliest claimed: 2019-03-01
- Inventors: Bhaven Chakravarti
- Web page: https://patentgrep.com/patent/US20210268563A1

## CPC

- B21C 37/06: of tubes or metal hoses; Combined procedures for making tubes, e.g. for making multi-wall tubes
- B21C 1/22: specially adapted for making tubular articles (bending sheet metal into tubular form by drawing B21D5/10)
- B21C 23/22: Making metal-coated products; Making products from two or more metals
- B21C 33/004: {Composite billet}
- B23K 20/085: {for tubes, e.g. plugging}
- B23K 20/227: with ferrous layer
- E04C 5/015: {Anti-corrosion coatings or treating compositions, e.g. containing waterglass or based on another metal (coating of discrete reinforcing elements C04B20/10)}
- B21C 29/003: {Cooling or heating of work}
- B23K 2101/06: Tubes
- B23K 2103/04: Steel {or steel} alloys
- B21C: MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES, PROFILES OR LIKE SEMI-MANUFACTURED PRODUCTS OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- E04C: STRUCTURAL ELEMENTS; BUILDING MATERIALS (for bridges E01D; specially designed for insulation or other protection E04B; elements used as building aids E04G; for mining E21; for tunnels E21D; structural elements with broader range of application than for building engineering F16, particularly F16S)

## Abstract

A method of producing a clad billet includes inserting a solid carbon or low-alloy steel (CS) material into a hollow interior of the slightly larger diameter (CRA) cylinder so that a standoff gap is provided between an outer surface of the (CS) material and the inner diameter of the (CRA) cylinder; providing an explosive material around the (CRA) cylinder; detonating the explosive material to collapse at least the inner diameter of the corrosion resistant alloy cylinder onto the outer surface of the solid carbon or low-alloy steel material and eliminate the standoff gap, creating at least a partial metallurgical bond at an interface with the outer surface and resulting in a composite billet assembly, and extruding the composite billet assembly to reduce its size and form the clad billet having a metallurgical bond between the (CS) material and the (CRA) cylinder.

## Claims

### Claim 1

A method of producing a clad billet, comprising:
providing a corrosion resistant alloy cylinder, the corrosion resistant alloy cylinder including a hollow interior, an inner diameter, and an outer diameter,
inserting a solid carbon or low-alloy steel material into the hollow interior of the corrosion resistant alloy cylinder so that an outer surface of the solid carbon or low-alloy steel material faces the inner diameter of the corrosion resistant alloy cylinder, and so that a concentric standoff gap is provided between the outer surface of the solid carbon or low-alloy steel material and the inner diameter of the corrosion resistant alloy cylinder;
providing an explosive material around the outer diameter of the corrosion resistant alloy cylinder;
detonating the explosive material to collapse at least the inner diameter of the corrosion resistant alloy cylinder onto the outer surface of the solid carbon or low-alloy steel material and eliminate the standoff gap, creating at least a partial metallurgical bond at an interface with the outer surface and resulting in a composite billet assembly; and
extruding the composite billet assembly to reduce the size of the composite billet assembly by reducing a thickness of each of the corrosion resistant alloy cylinder and the solid carbon or low-alloy steel material and form the clad billet having a metallurgical bond between the solid carbon or low-alloy steel material and the corrosion resistant alloy cylinder.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
cleaning the outer surface of the solid carbon or low-alloy steel material and the surface of the inner diameter of the corrosion resistant alloy cylinder, before inserting the solid carbon or low-alloy steel material into the hollow interior of the corrosion resistant alloy cylinder.

### Claim 3 (depends on 2)

The method of claim 2, wherein the cleaning removes at least one of oxides, oils and rust.

### Claim 4 (depends on 1)

The method of claim 1, further comprising:
providing a containment frame around the outer diameter of the corrosion resistant alloy cylinder to create an annulus between the containment frame and the outer diameter of the corrosion resistant alloy cylinder, wherein the explosive material is located in the annulus.

### Claim 5 (depends on 1)

The method of claim 1, further comprising:
welding each opposite end of the composite billet assembly at the interface, before extruding the composite billet assembly, to create a seal against oxidation of the interface.

### Claim 6 (depends on 1)

The method of claim 1, wherein the composite billet assembly comprises an outer diameter of 3 inches to 45 inches, and the clad billet comprises a cross-sectional dimension of 1 inch to 20 inches after the extruding.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
hot-rolling the clad billet to form a clad rod.

### Claim 8 (depends on 1)

The method of claim 1, wherein the composite billet assembly is drilled, machined or trepanned to form a composite pipe billet assembly for the extruding.

### Claim 9 (depends on 8)

The method of claim 8, further comprising:
at least one of cold pilgering and cold drawing the composite billet after the extruding to form a clad pipe.

### Claim 10 (depends on 1)

The method of claim 1, wherein the solid carbon or low-alloy steel material is a bar.

### Claim 11 (depends on 13)

The system of claim 13, wherein the composite billet assembly has a length of 20 feet to 60 feet, and a cross-sectional dimension of 3 inches to 10 inches.

### Claim 12 (depends on 1)

The method of claim 1, wherein the metallurgical bond is an atom-to-atom bond between the solid carbon or low-alloy steel material and the corrosion resistant alloy cylinder.

### Claim 13

A system for producing a clad billet, comprising:
a corrosion resistant alloy cylinder including a hollow interior, an inner diameter, and an outer diameter;
a solid carbon or low-alloy steel material inserted into the hollow interior of the corrosion resistant alloy cylinder so that a concentric standoff gap is provided between the outer surface of the solid carbon or low-alloy steel material and an inner diameter surface of the corrosion resistant alloy cylinder;
an explosive material for surrounding the corrosion resistant alloy cylinder;
an ignition source for detonating the explosive material to collapse at least the inner diameter of the corrosion resistant alloy cylinder onto the outer surface of the solid carbon or low-alloy steel material and eliminate the standoff gap, creating at least a partial metallurgical bond at an interface with the outer surface and resulting in a composite billet assembly; and
an extruder for extruding the composite billet assembly to reduce the size of the composite billet assembly by reducing a thickness of each of the corrosion resistant alloy cylinder and the solid carbon or low-alloy steel material and form the clad billet having a metallurgical bond between the solid carbon or low-alloy steel material and the corrosion resistant alloy cylinder.

### Claim 14 (depends on 13)

The system of claim 13, further comprising:
a containment frame around the outer diameter of the corrosion resistant alloy cylinder to create an annulus between the containment frame and the outer diameter of the corrosion resistant alloy cylinder, wherein the explosive material is located in the annulus.

### Claim 15 (depends on 13)

The system of claim 13, further comprising:
a cleaning device for cleaning at least one of oxides, oils and rust from the outer surface of the solid carbon or low-alloy steel material and the surface of the inner diameter of the corrosion resistant alloy cylinder.

### Claim 16 (depends on 13)

The system of claim 13, further comprising:
a welding device for welding each opposite end of the composite billet assembly at the interface to create a seal against oxidation of the interface.

### Claim 17 (depends on 13)

The system of claim 13, further comprising:
a hot-rolling device for hot-rolling the clad billet to form a clad rod.

### Claim 18 (depends on 13)

The system of claim 13, further comprising:
a tool for drilling, machining, or trepanning the composite billet assembly to form a composite pipe billet assembly.

### Claim 19 (depends on 18)

The system of claim 18, further comprising:
a cold pilgering/cold drawing device for at least one of cold pilgering and cold drawing the composite pipe billet assembly after extrusion to form a clad pipe.

### Claim 20 (depends on 13)

The system of claim 13, wherein the composite billet assembly has a length of 20 feet to 60 feet, and a cross-sectional dimension of 3 inches to 10 inches.