- Number: US 2021/0268539 A1
- Document ID: US20210268539A1
- Status: Published application
- Kind: A1
- Application number: 17/256,448
- Filed: 2019-07-01
- Published: 2021-09-02
- Earliest claimed: 2018-07-06
- Assignees: Saint-Gobain Ecophon AB
- Applicants: Saint-Gobain Ecophon AB
- Inventors: Thomas NILSSON; Roger LOVDAHL
- Web page: https://patentgrep.com/patent/US20210268539A1

## CPC

- B05D 1/26: performed by applying the liquid or other fluent material from an outlet device in contact with, or almost in contact with, the surface
- B05C 5/0204: {for applying liquid or other fluent material to the edges of essentially flat articles}
- B05D 3/0254: {After-treatment}
- B05D 3/0263: {with IR heaters}
- B05D 3/029: {with microwaves}
- B05D 3/0493: {using vacuum}
- B05D 2401/00: Form of the coating product, e.g. solution, water dispersion, powders or the like
- B05D 2401/20: Aqueous dispersion or solution
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- B05C: APPARATUS FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (spraying apparatus, atomising apparatus, nozzles B05B; plant for applying liquids or other fluent materials to objects by electrostatic spraying B05B5/08)

## Abstract

A method for coating a tile element includes providing a tile element made of a compressed fibre material having a porosity in the range of 0.92-0.99 and applying a water-based coating material to a side edge surface of the tile element extending between two opposite major surfaces of the tile element. The applying is performed by an applicator head of a continuous vacuum coating apparatus that applies the water-based coating material to the side edge surface of the tile element and removes excess through a vacuum. The water-based coating material is applied at a feeding rate of the tile element relative the applicator head in the range of 25-150 m/min. The water-based coating material forms a coating layer including an outer coating layer and an inner coating layer penetrating the side edge surface. The inner coating layer has penetration depth of at least 100 μm.

## Claims

### Claim at position 1

1-8. (canceled)

### Claim 9

A method for coating a tile element, comprising:
providing a tile element made of a compressed fibre material having a porosity in the range of 0.92-0.99, the tile element having two opposite major surfaces; and
applying a water-based coating material to a side edge surface of the tile element extending between the two opposite major surfaces,
wherein the applying the water-based coating material is performed by an applicator head of a continuous vacuum coating apparatus, the applicator head being configured to apply the water-based coating material to the side edge surface of the tile element and to remove excess of the water-based coating material through a vacuum,
wherein the water-based coating material is applied at a feeding rate of the tile element relative the applicator head of the continuous vacuum coating apparatus in the range of 25-150 m/min,
wherein the water-based coating material is applied to the side edge surface such that a coating layer is formed comprising an outer coating layer extending beyond the side edge surface and an inner coating layer penetrating the side edge surface and extending into the tile element, and
wherein the inner coating layer is given a penetration depth of at least 100 μm.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the penetration depth of the inner coating layer is in a range of 100-4000 μm.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the water-based coating material is applied to all side edge surfaces extending between the two major surfaces of the tile element.

### Claim 12 (depends on 9)

The method according to claim 9, further comprising:
drying the applied water-based coating material by means of IR-radiation and/or micro wave radiation.

### Claim 13 (depends on 9)

The method according to claim 9, wherein the outer coating layer is given a thickness of at least 100 μm.

### Claim 14 (depends on 9, 13)

The method according to claim 13, wherein the thickness of the outer coating layer is in a range of 100-1500 μm. 15 (New) The method according to claim 9, wherein the water-based coating material is applied to the side edge surface with a wet surface density in the range of 300-1,600 g/m2.

### Claim 16 (depends on 9)

The method according to claim 9, wherein the water-based coating material has an operational viscosity in the range of 50-200 Krebs unit (KU) (about 0.15-11.27 kg/m/s).

### Claim 17 (depends on 9)

The method according to claim 9, wherein the water-based coating material has an operational viscosity in the range of 80-160 KU (about 0.87-6.46 kg/m/s).

### Claim 18 (depends on 9)

The method according to claim 9, wherein the water-based coating material has an operational viscosity in the range of 105-115 KU (about 2.04-2.65 kg/m/s).

### Claim 19 (depends on 9)

The method according to claim 9, wherein the water-based coating material has a dry content of at least 60 wt. %.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the dry content of the water-based coating material is in a range of 60-80 wt. %.

### Claim 21 (depends on 9)

The method according to claim 9, wherein the compressed mineral fibre material has a density in a range of 25-200 kg/m3.