# US 2021/0268485 A1 · Catalyst of platinum/zirconium dioxide/sba-15 and method for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0268485 A1
- Document ID: US20210268485A1
- Status: Published application
- Kind: A1
- Application number: 17/324,034
- Filed: 2021-05-18
- Published: 2021-09-02
- Earliest claimed: 2017-12-14
- Assignees: Xiangtan University
- Applicants: Xiangtan University
- Inventors: Jicheng ZHOU; Yanji ZHANG; Fei WANG
- Web page: https://patentgrep.com/patent/US20210268485A1

## CPC

- B01J 29/0325: {Noble metals}
- B01J 29/043: {Noble metals}
- B01J 37/0228: {in several steps}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/0242: {Coating followed by impregnation}
- B01J 37/0244: {Coatings comprising several layers}
- B01J 37/088: {Decomposition of a metal salt}
- B01J 37/343: {of ultrasonic wave energy}
- B01J 37/345: {of ultraviolet wave energy}
- C07C 209/365: {by reduction with preservation of halogen-atoms in compounds containing nitro groups and halogen atoms bound to the same carbon skeleton}
- C07C 211/52: the carbon skeleton being further substituted by halogen atoms or by nitro or nitroso groups
- B01J 2235/15: X-ray diffraction
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

A catalyst including platinum (Pt) and a composite support. The composite support includes ZrO2/mesoporous silica sieve SBA-15. The platinum accounts for 0.01-0.3 wt. % of the catalyst. ZrO2 accounts for 5-20 wt. % of the composite support.

## Claims

### Claim 1

A composition of matter, comprising:
platinum (Pt); and
a composite support, the composite support comprising ZrO2/mesoporous silica sieve SBA-15;
wherein:
the platinum accounts for 0.01-0.3 wt. % of the composition of matter; and
ZrO2 accounts for 5-20 wt. % of the composite support.

### Claim 2 (depends on 1)

The composition of matter of claim 1, wherein the platinum accounts for 0.05-0.15 wt. % of the composition of matter.

### Claim 3 (depends on 2)

The composition of matter of claim 2, wherein the platinum accounts for 0.08-0.10 wt. % of the composition of matter.

### Claim 4 (depends on 1)

The composition of matter of claim 1, wherein the ZrO2 accounts for 10-15 wt. % of the composite support.

### Claim 5 (depends on 2)

The composition of matter of claim 2, wherein the ZrO2 accounts for 10-15 wt. % of the composite support.

### Claim 6 (depends on 3)

The composition of matter of claim 3, wherein the ZrO2 accounts for 10-15 wt. % of the composite support.

### Claim 7 (depends on 1)

The composition of matter of claim 1, wherein the ZrO2 is a film structure coating the mesoporous silica sieve SBA-15, and the platinum is disposed on the film structure of ZrO2.

### Claim 8 (depends on 1)

A method for preparing the composition of matter of claim 1, the method comprising:
precipitating ZrO2 on the mesoporous silica sieve SBA-15, thereby yielding the composite support comprising ZrO2/SBA-15; and
disposing platinum on the composite support through a photocatalytic reduction method, thereby yielding Pt/ZrO2/SBA-15.

### Claim 9 (depends on 8)

The method of claim 8, wherein precipitating ZrO2 on the mesoporous silica sieve SBA-15 comprises: adding SBA-15 to a zirconium oxychloride solution, adjusting a pH of the zirconium oxychloride solution mixed with the SBA-15 to 4-6, stirring the zirconium oxychloride solution mixed with the SBA-15 for 0.5 hours, sonicating the zirconium oxychloride solution mixed with the SBA-15 for 0.5 hours, resting the zirconium oxychloride solution mixed with the SBA-15 for one night, drying the zirconium oxychloride solution mixed with the SBA-15 at 110° C. for one night, and calcinating at 500° C., thereby yielding the composite support.

### Claim 10 (depends on 8)

The method of claim 8, wherein the photocatalytic reduction method comprises: dispersing the composite support in deionized water, adding a mixture of methanol and chloroplatinic acid to the deionized water comprising the composite support, sonicating a solution of the mixture and the deionized water comprising the composite support, exposing and stirring the solution sonicated under UV irradiation, filtering the solution thereby producing a solid, collecting and washing the solid to have a pH of 7, and drying the solid, thereby yielding the Pt/ZrO2/SBA-15.

### Claim 11 (depends on 9)

The method of claim 9, wherein a mass ratio of the methanol to the deionized water is 1:5-1:15, and the solution is exposed under UV irradiation for 5-20 hours.