# US 2021/0265210 A1 · Processing method of wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0265210 A1
- Document ID: US20210265210A1
- Status: Published application
- Kind: A1
- Application number: 17/171,138
- Filed: 2021-02-09
- Published: 2021-08-26
- Earliest claimed: 2020-02-21
- Assignees: Disco Corporation
- Applicants: Disco Corporation
- Inventors: Yuki IKKU; Shuichiro TSUKIJI; Satoshi KOBAYASHI
- Web page: https://patentgrep.com/patent/US20210265210A1

## CPC

- H10P 54/00: Cutting or separating of wafers, substrates or parts of devices
- B23K 26/0006: {taking account of the properties of the material involved (B23K26/32, B23K26/40 take precedence)}
- B23K 26/03: Observing, e.g. monitoring, the workpiece
- B23K 26/032: {using optical means}
- B23K 26/0622: by shaping pulses
- B23K 26/083: {Devices involving movement of the workpiece in at least one axial direction}
- B23K 26/0869: {Devices involving movement of the laser head in at least one axial direction}
- B23K 26/53: for modifying or reforming the material inside the workpiece, e.g. for producing break initiation cracks
- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- B23K 2101/40: Semiconductor devices
- B23K 2103/52: {Ceramics}
- B23K 2103/54: {Glass}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A processing method of a wafer in which a modified layer is formed inside the wafer. In the processing method, irradiation with a first laser beam is executed from a back surface side of the wafer and the modified layer is formed inside the wafer. Then, irradiation with a second laser beam is executed with the focal point thereof positioned to the inside or the front surface of the wafer and reflected light is imaged by an imaging unit. Furthermore, a processing state of the wafer is determined on the basis of a taken image. The second laser beam is shaped in such a manner that a sectional shape thereof in a surface perpendicular to a traveling direction thereof becomes asymmetric across the modified layer.

## Claims

### Claim 1

A processing method of a wafer in which a modified layer is formed inside the wafer on which a plurality of planned dividing lines are set on a front surface along the planned dividing lines of the wafer, the processing method comprising:
a holding step of causing the front surface of the wafer to be opposed to a chuck table and holding the wafer by the chuck table;
a modified layer forming step of positioning a focal point of a first laser beam with a wavelength having transmissibility with respect to the wafer to inside of the wafer and executing irradiation with the first laser beam along the planned dividing lines from a side of a back surface of the wafer while relatively moving a laser beam irradiation unit and the chuck table in a direction along the planned dividing line, to form the modified layer inside the wafer;
an observation laser beam irradiation step of positioning a focal point of a second laser beam with output power that does not exceed a processing threshold of the wafer and with a wavelength having transmissibility with respect to the wafer to the inside or the front surface of the wafer and executing irradiation with the second laser beam from the side of the back surface of the wafer after the modified layer forming step;
an imaging step of imaging reflected light of the second laser beam with which the irradiation is executed in the observation laser beam irradiation step by an imaging unit; and
a determination step of determining a processing state of the wafer on a basis of an image taken in the imaging step, wherein
the second laser beam with which the wafer is irradiated in the observation laser beam irradiation step is shaped in such a manner that a sectional shape of the second laser beam in a surface perpendicular to a traveling direction of the second laser beam becomes asymmetric across the modified layer.

### Claim 2 (depends on 1)

The processing method of a wafer according to claim 1, wherein,
in the determination step,
it is determined that a crack extends from the modified layer toward a side of the front surface of the wafer when the reflected light appears in such a manner as to overlap with a region with a same shape as a region irradiated with the second laser beam with which the wafer is irradiated in the observation laser beam irradiation step in the back surface in the image taken in the imaging step, and
it is determined that the crack does not extend from the modified layer toward the side of the front surface of the wafer when the reflected light appears in such a manner as to overlap with a region with a shape obtained by inverting a shape of the region irradiated with the second laser beam with which the wafer is irradiated in the observation laser beam irradiation step in the back surface in the image taken in the imaging step.

### Claim 3

A processing method of a wafer in which a modified layer is formed inside the wafer on which a plurality of planned dividing lines are set on a front surface along the planned dividing lines of the wafer, the processing method comprising:
a holding step of causing the front surface of the wafer to be opposed to a chuck table and holding the wafer by the chuck table;
a modified layer forming step of positioning a focal point of a first laser beam with a wavelength having transmissibility with respect to the wafer to inside of the wafer and executing irradiation with the first laser beam along the planned dividing lines from a side of a back surface of the wafer while relatively moving a laser beam irradiation unit and the chuck table in a direction along the planned dividing line, to form the modified layer inside the wafer;
an observation laser beam irradiation step of positioning a focal point of a second laser beam with output power that does not exceed a processing threshold of the wafer and with a wavelength having transmissibility with respect to the wafer to the inside or the front surface of the wafer and executing irradiation with the second laser beam from the side of the back surface of the wafer after the modified layer forming step;
an imaging step of imaging reflected light of the second laser beam with which the irradiation is executed in the observation laser beam irradiation step by an imaging unit; and
a determination step of determining a processing state of the wafer on a basis of an image taken in the imaging step, wherein
the second laser beam with which the wafer is irradiated in the observation laser beam irradiation step travels to the inside of the wafer from a direction that is not perpendicular to the back surface of the wafer.

### Claim 4 (depends on 1)

The processing method of a wafer according to claim 1, wherein
the second laser beam is made incident on the wafer in a state in which aberration attributed to a lens that forms the focal point is corrected in the observation laser beam irradiation step.

### Claim 5 (depends on 1)

The processing method of a wafer according to claim 1, wherein
the first laser beam and the second laser beam have a same light source.

### Claim 6 (depends on 1)

The processing method of a wafer according to claim 1, wherein
the observation laser beam irradiation step is executed in liquid immersion.