# US 2021/0263409 A1 · Method for manufacturing device, and composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0263409 A1
- Document ID: US20210263409A1
- Status: Published application
- Kind: A1
- Application number: 17/317,988
- Filed: 2021-05-12
- Published: 2021-08-26
- Earliest claimed: 2015-08-24
- Assignees: Toyo Gosei Co., Ltd.
- Applicants: Toyo Gosei Co., Ltd.
- Inventors: Takeshi OSAKI
- Web page: https://patentgrep.com/patent/US20210263409A1

## CPC

- G03F 7/0002: {Lithographic processes using patterning methods other than those involving the exposure to radiation, e.g. by stamping}
- C08F 220/1807: {C7-(meth)acrylate, e.g. heptyl (meth)acrylate or benzyl (meth)acrylate}
- C08F 220/281: {and containing only one oxygen, e.g. furfuryl (meth)acrylate or 2-methoxyethyl (meth)acrylate}
- C08K 5/13: Phenols; Phenolates
- C08K 5/134: Phenols containing ester groups
- C08K 5/1345: {Carboxylic esters of phenolcarboxylic acids}
- C08K 5/1575: Six-membered rings
- C08K 5/3435: Piperidines
- C08F 220/1811: {C10or C11-(Meth)acrylate, e.g. isodecyl (meth)acrylate, isobornyl (meth)acrylate or 2-naphthyl (meth)acrylate}
- C08F 220/283: {and containing one or more carboxylic moiety in the chain, e.g. acetoacetoxyethyl(meth)acrylate}
- C08F 222/102: {of dialcohols, e.g. ethylene glycol di(meth)acrylate or 1,4-butanediol dimethacrylate}
- C08F 222/103: {of trialcohols, e.g. trimethylolpropane tri(meth)acrylate}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A method for manufacturing a device including a substrate and a second film disposed above the substrate includes: forming a first film above the substrate using a composition containing a polymerizable monomer and an oxidation inhibitor; and forming the second film by curing the first film in a state where at least one part of a mold having a convexo-concave pattern is in contact with the first film, or after at least one part of the mold is brought into contact with the first film. The oxidation inhibitor is at least one of a hindered amine compound and a hindered phenol compound having a molecular weight of 700 or more. The composition satisfies a relationship of (t0(T)−tx(T))/t0(T)×100≤13.0. (t0(T) is a height of a convex part of cured film obtained by the specific method, and tx(T) is the corresponding height after heating at 260° C.)

## Claims

### Claim 1

A method for manufacturing a device including a substrate and a second film disposed above the substrate, comprising:
forming a first film above the substrate using a composition containing a polymerizable monomer and an oxidation inhibitor; and
forming the second film by curing the first film in a state where at least one part of a mold having a convexo-concave pattern is in contact with the first film, or after at least one part of the mold is brought into contact with the first film,
wherein the oxidation inhibitor is at least one of a hindered amine compound and a hindered phenol compound having a molecular weight of 700 or more, and
the composition satisfies a relationship of (t0(T)−tx(T))/t0(T)×100≤13.0,
where t0(T) is a height of a convex part of a convexo-concave part of a cured film having the convexo-concave part obtained by forming a coating film using the composition and then by curing the coating film in a state where the coating film is in contact with a convexo-concave part in which a depth of a recess is 3 μm and a line width thereof is 5 μm, included in the mold, and
tx(T) is a height of the convex part after the cured film is heated from 25° C. to 260° C. over five minutes, then a temperature of the cured film is held at 260° C. for five minutes, and the cured film is cooled to 25° C. over 30 minutes.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the composition contains 0.05 to 10% by mass of the oxidation inhibitor.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the oxidation inhibitor is a combination of the hindered amine compound and the hindered phenol compound.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the hindered amine compound and the hindered phenol compound are blended such that the amount of the hindered phenol compound is 1 to 100 parts by mass relative to 10 parts by mass of the hindered amine compound.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the hindered amine compound has a polymerizable group selected from the group consisting of a (meth)acryloyloxy group, a vinyl group, an allyl group and a styryl group.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the hindered phenol compound has a molecular weight of 1000 or more.
