# US 2021/0263069 A1 · Rugged, single crystal wide-band-gap-material scanning-tunneling-microscopy/lithography tips

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0263069 A1
- Document ID: US20210263069A1
- Status: Published application
- Kind: A1
- Application number: 17/237,697
- Filed: 2021-04-22
- Published: 2021-08-26
- Earliest claimed: 2016-04-25
- Assignees: UNM Rainforest Innovations
- Applicants: Unm Rainforest Innovations
- Inventors: Steven R.J. BRUECK; Daniel FEEZELL; John RANDALL; Tito BUSANI; Joshua B. BALLARD; Mahmoud BEHZADIRAD; Ashwin Krishnan RISHINARAMANGALAM
- Web page: https://patentgrep.com/patent/US20210263069A1

## CPC

- G01Q 60/16: Probes, their manufacture, or their related instrumentation, e.g. holders
- B82B 3/0004: {Apparatus specially adapted for the manufacture or treatment of nanostructural devices or systems or methods for manufacturing the same}
- G01Q 70/06: Probe tip arrays
- G01Q 70/10: Shape or taper
- G01Q 70/14: Particular materials
- G01Q 80/00: Applications, other than SPM, of scanning-probe techniques (manufacture or treatment of nanostructures B82B3/00; recording or reproducing information using near-field interaction G11B9/12, G11B11/24, G11B13/08)
- G03F 7/0002: {Lithographic processes using patterning methods other than those involving the exposure to radiation, e.g. by stamping}
- G01Q 70/12: Nanotube tips
- G01Q: SCANNING-PROBE TECHNIQUES OR APPARATUS; APPLICATIONS OF SCANNING-PROBE TECHNIQUES, e.g. SCANNING PROBE MICROSCOPY [SPM]
- B82B: NANOSTRUCTURES FORMED BY MANIPULATION OF INDIVIDUAL ATOMS, MOLECULES, OR LIMITED COLLECTIONS OF ATOMS OR MOLECULES AS DISCRETE UNITS; MANUFACTURE OR TREATMENT THEREOF
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

Provided is a composite metal-wide-bandgap semiconductor tip for scanning tunneling microscopy and/or scanning tunneling lithography, a method of forming, and a method for using the composite metal-wide-bandgap semiconductor tip.

## Claims

### Claim 1

A method of forming a composite tip for a scanning tunneling microscope (“STM”), comprising:
using a nanomanipulator to select a single crystal wide-band-gap semiconductor from an array of formed single crystal wide-band-gap semiconductors epitaxially grown selectively on a crystalline substrate;
preparing an electrically conductive wire to provide a substantially flat end surface that is substantially perpendicular to the wire length direction;
transferring the single crystal wide-band-gap semiconductor from the growth substrate to the substantially flat end surface of the electrically conductive wire; and
affixing the single crystal wide-band-gap semiconductor to the substantially flat end surface of the electrically conductive wire to form the composite tip.

### Claim 2 (depends on 1)

The method of claim 1, wherein the affixing comprises welding using a Pt ion source.

### Claim 3 (depends on 1)

The method of claim 1, wherein the single crystal wide-band-gap semiconductor comprises a group III-N nanowire wherein the group III composition comprises one or more of Ga, In, or Al.

### Claim 4 (depends on 1)

The method of claim 1, wherein the composite tip has dimensions that are from about a length of 0.5 to 4 μm, with a faceted diameter of about 0.1 to 1 μm, a tip radius of about or less than about 2 nm, and with a controlled doping to provide a resistivity of about 10−2 Ohm-cm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the electrically conductive wire comprises platinum, iridium, tungsten, and doped silicon and combinations thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein the electrically conductive wire and the tip is affixed having a common orientation within about ±1°.

### Claim 7

A method of forming an array of composite tips for use in scanning tunneling microscopy, comprising:
preparing an array of scanning tunneling microscope tip precursors on a crystalline substrate;
providing an area for selective area growth of a wide bandgap semiconducting material on each tip precursor;
growing a III-N wide bandgap material nanowire on each selective growth area wherein the nanowire has a faceted diameter of about 0.1 to 0.5 μm, a tip radius of about or less than about 2 nm, and with a controlled doping to provide a resistivity of about 10−2 Ohm-cm;
separating the array of scanning tunneling tip precursors into subarrays wherein each subarray contains at least one scanning tunneling tip; and
mounting the at least one of the subarrays of scanning tunneling microscope tip precursors for use in a scanning tunneling microscope.

### Claim 8 (depends on 7)

The method of claim 7, wherein the wide bandgap material is one of GaN, AlN, InN, or alloys thereof.

### Claim 9 (depends on 7)

The method of claim 7, wherein the growth technique is metal organic chemical vapor deposition and the growth is controlled to provide the sharp tip of the nanowire with a radius of less than about 2 nm without further processing.

### Claim 10 (depends on 7)

The method of claim 7, wherein a sub-array contains only a single scanning tunneling tip precursor.

### Claim 11 (depends on 7)

The method of claim 7, wherein a sub-array contains more than one scanning tunneling tip precursor and means is provided for relative motion between the multiple scanning tunneling tips to allow for a degree of parallel application in a scanning tunneling microscope.

### Claim 12

A method of forming a composite tip for a scanning tunneling microscope (“STM”), comprising:
using a nanomanipulator to select a single crystal wide-band-gap semiconductor from an array of formed single crystal wide-band-gap semiconductors epitaxially grown selectively on a crystalline substrate;
preparing an electrically conductive wire to provide a substantially flat end surface that is substantially perpendicular to the wire length direction;
transferring the single crystal wide-band-gap semiconductor from the growth substrate to the substantially flat end surface of the electrically conductive wire; and
affixing the single crystal wide-band-gap semiconductor to the substantially flat end surface of the electrically conductive wire to form the composite tip,
wherein the electrically conductive wire comprises a substantially cylindrical body and a distal end tapered to a diameter larger than the single crystal wide-band-gap semiconductor and terminated with a flat surface that is approximately perpendicular to a transverse axis of the electrically conductive wire.

### Claim 13 (depends on 12)

The method of claim 12, wherein the single crystal wide-band-gap semiconductor comprises a group III-N material.

### Claim 14 (depends on 13)

The method of claim 13, wherein the group III material comprises one or more of Ga, In, or Al.

### Claim 15 (depends on 12)

The method of claim 12, wherein the body of the single crystal wide-band-gap semiconductor has a substantially constant diameter and is bounded by a surface with a diameter ranging from about 0.1 to 1.0 micrometer and the surface comprising a first set of facets corresponding to natural crystal planes of the single crystal wide-band-gap semiconductor.

### Claim 16 (depends on 15)

The method of claim 15, wherein a tip of the single crystal wide-band-gap semiconductor tapers to a radius of 2 nm or less, and wherein the surface of the tip comprises additional crystal facets of the wide-band-gap semiconductor.

### Claim 17 (depends on 12)

The method of claim 12, wherein the electrically conductive wire comprises platinum, iridium, tungsten, and doped silicon and combinations thereof.

### Claim 18 (depends on 12)

The method of claim 12, wherein the electrically conductive wire and the tip is affixed having a common orientation within about ±1°.