# US 2021/0262948 A1 · Method for Manufacturing Composite Material and Method for Examining Weight Unevenness of Composite Material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0262948 A1
- Document ID: US20210262948A1
- Status: Published application
- Kind: A1
- Application number: 17/253,776
- Filed: 2019-06-18
- Published: 2021-08-26
- Earliest claimed: 2018-06-19
- Assignees: Teijin Limited
- Applicants: Teijin Limited
- Inventors: Takashi Toyozumi
- Web page: https://patentgrep.com/patent/US20210262948A1

## CPC

- G01N 23/046: using tomography, e.g. computed tomography [CT]
- B29C 70/12: using fibres of short length, e.g. in the form of a mat {(non-woven fabrics per se D04H1/00)}
- G01N 21/84: Systems specially adapted for particular applications
- G01N 23/043: {using fluoroscopic examination, with visual observation or video transmission of fluoroscopic images}
- G01N 23/083: the radiation being X-rays
- B29C 70/34: and shaping or impregnating by compression {, i.e. combined with compressing after the lay-up operation}
- B29K 2307/04: Carbon
- G01N 2021/8472: {Investigation of composite materials}
- G01N 2201/06113: Coherent sources; lasers
- G01N 2223/04: and measuring absorption
- G01N 2223/406: fluoroscopic image
- G01N 2223/419: computed tomograph
- G01N 2223/615: composite materials, multilayer laminates
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

[Problem] To make it possible to perform quantitative examination of slight weight unevenness of a material, and to provide a method for manufacturing a carbon fiber composite material in which weight unevenness is suppressed through the examination step. [Solution] The above problem can be solved by a method for manufacturing a deposit containing a thermoplastic resin and carbon fibers and having a side of 300 mm or more, wherein the composite is manufactured through the following steps. Step 101: an examination step of examining the weight of an aggregate of carbon fibers or the deposit non-destructively. Step 201: a step of ascertaining weight unevenness on the basis of the result of examination in step S101. Step 301: a step of adding an aggregate of discontinuous carbon fibers and/or a thermoplastic resin to a weight-lacking area on the basis of the weight unevenness of step 201 so as to reduce the weight unevenness.

## Claims

### Claim 1

A method for manufacturing a deposit containing thermoplastic resin and discontinuous carbon fibers, wherein a length of one side of the deposit is 300 mm or more, the method manufacturing the deposit through the following steps:
Step 101: an examination step of non-destructively examining a basis weight of either an aggregate of the discontinuous carbon fibers or the deposit (hereinafter, referred to as an object to be examined 1),
Step 201: a step of ascertaining weight unevenness of the object to be examined 1 based on examination results of the step 101, and
Step 301: a step of adding the discontinuous carbon fibers to a position of the aggregate of the discontinuous carbon fibers where the basis weight is insufficient so as to reduce the weight unevenness, or a step of adding the aggregate of the discontinuous carbon fibers and/or the thermoplastic resin to a position of the deposit where the basis weight is insufficient so as to reduce the weight unevenness based on the weight unevenness of the step 201.

### Claim 2 (depends on 1)

The method for manufacturing a deposit according to claim 1, further comprising following step 202 after the step 201:
Step 202: a step of feeding back the weight unevenness of the object to be examined 1 obtained in the step 201 to a step of manufacturing the object to be examined 1.

### Claim 3 (depends on 1)

The method for manufacturing a deposit according to claim 1, wherein a variation coefficient 1 of the basis weight of the aggregate of the discontinuous carbon fibers or a variation coefficient 2 of the total basis weight of the deposit is 20% or less by the steps.

### Claim 4 (depends on 1)

The method for manufacturing a deposit according to claim 1, wherein the examination step includes
detecting infrared rays radiated from the object to be examined 1 and
using a phase analysis method.

### Claim 5 (depends on 4)

The method for manufacturing a deposit according to claim 4, further comprising heating the object to be examined 1 using a fiber laser to detect the infrared rays radiated from the object to be examined 1.

### Claim 6 (depends on 5)

The method for manufacturing a deposit according to claim 5, wherein the laser is passed through a device capable of adjusting an irradiation range of the laser, and then the object to be examined 1 is heated to detect the infrared rays.

### Claim 7 (depends on 1)

The method of manufacturing a deposit according to claim 1, wherein the examination step uses a tomographic image obtained by capturing the object to be examined 1 by X-ray CT or data of the tomographic image.

### Claim 8 (depends on 7)

The method for manufacturing a deposit according to claim 7, using X-rays having an X-ray intensity peak at a wavelength of less than 1.0×10−10 m.

### Claim 9 (depends on 1)

The method for manufacturing a deposit according to claim 1, wherein the examination step uses a fluoroscopic image obtained by capturing the object to be examined 1 by using an X-ray examination device including an X-ray area sensor or an X-ray line sensor or data derived from the fluoroscopic image.

### Claim 10 (depends on 7)

The method for manufacturing a deposit according to claim 7, wherein a spatial average of digital values in the tomographic image or the fluoroscopic image of the object to be examined 1 is 5% or more and less than 100% of a limit value of a digital value in the tomographic image.

### Claim 11 (depends on 9)

The method for manufacturing a deposit according to claim 9, using X-rays having an X-ray intensity peak at a wavelength of less than 0.5×10−10 m.

### Claim 12 (depends on 9)

The method for manufacturing a deposit according to claim 9, further comprising a step of amplifying numerical data more than 1.0 time, the numerical data being based on a relative exposure amount of X-rays received by the X-ray area sensor or the X-ray line sensor.

### Claim 13 (depends on 1)

The method for manufacturing a deposit according to claim 1, wherein a maximum value of deviation with respect to an average value of the basis weight of the object to be examined 1 examined in the examination step is 1500 g/m2 or less.

### Claim 14 (depends on 1)

A method for manufacturing a composite material, comprising:
heating the deposit of claim 1 to impregnate the aggregate of the discontinuous carbon fibers with at least a part of the thermoplastic resin.

### Claim 15

A method for examining weight unevenness of any one of an aggregate of carbon fibers, a deposit containing thermoplastic resin and an aggregate of discontinuous carbon fibers, or a composite material in which the deposit is heated to impregnate the discontinuous carbon fibers with the thermoplastic resin, the any one of the aggregate, the deposit, and the composite material (hereinafter referred to as an object to be examined 2) having a length of one side of 300 mm or more, the method examining the weight unevenness through the following steps:
Step 111: an examination step of examining a basis weight of the object to be examined 2 non-destructively, and
Step 211: a step of ascertaining the weight unevenness of the object to be examined 2 based on examination results of the step 111.

### Claim 16 (depends on 15)

The method for examining weight unevenness according to claim 15, wherein the examination step comprises
detecting infrared rays radiated from the object to be examined 2 and
using a phase analysis method.

### Claim 17 (depends on 16)

The method for examining weight unevenness according to claim 16, further comprising heating the object to be examined 2 using a fiber laser to detect the infrared rays radiated from the object to be examined 2.

### Claim 18 (depends on 16)

The method for examining weight unevenness according to claim 16, wherein the laser is passed through a device capable of adjusting an irradiation range of the laser, and then the object to be examined 2 is heated to detect the infrared rays.

### Claim 19 (depends on 15)

The method for examining weight unevenness according to claim 15, wherein the examination step uses a tomographic image obtained by capturing the object to be examined 2 by X-ray CT or data of the tomographic image.

### Claim 20 (depends on 19)

The method for examining weight unevenness according to claim 19, using X-rays having an X-ray intensity peak at a wavelength of less than 1.0×10−10 m.

### Claim 21 (depends on 15)

The method for examining weight unevenness according to claims 15, wherein the examination step uses a fluoroscopic image obtained by capturing the object to be examined 2 by using an X-ray examination device including an X-ray area sensor or an X-ray line sensor or data derived from the fluoroscopic image.

### Claim 22 (depends on 19)

The method for examining weight unevenness according to claim 19, wherein a spatial average of digital values in the tomographic image of the object to be examined 2 is 5% or more and less than 100% of a limit value of a digital value in the tomographic image.

### Claim 23 (depends on 21)

The method for examining weight unevenness according to claim 21, wherein the examination step uses X-rays having an X-ray intensity peak at a wavelength of 0.5×10−10 m or more.

### Claim 24 (depends on 21)

The method for examining weight unevenness according to claim 21, further comprising a step of amplifying numerical data more than 1.0 time and equal to or less than 5.0 times, the numerical data being based on a relative exposure amount of X-rays received by the X-ray area sensor or the X-ray line sensor.

### Claim 25 (depends on 15)

The method for examining weight unevenness according to claim 15, wherein a maximum value of deviation with respect to an average value of the basis weight of the object to be examined 2 examined in the examination step is 1500 g/m2 or less.

### Claim 26 (depends on 15)

The method for examining weight unevenness according to claim 15, further comprising detecting a void or a metal piece included in the composite material.

### Claim 27 (depends on 9)

The method for manufacturing a deposit according to claim 9, wherein a spatial average of digital values in the fluoroscopic image of the object to be examined 1 is 5% or more and less than 100% of a limit value of a digital value in the fluoroscopic image.

### Claim 28 (depends on 21)

The method for examining weight unevenness according to claim 21, wherein a spatial average of digital values in the fluoroscopic image of the object to be examined 2 is 5% or more and less than 100% of a limit value of a digital value in the fluoroscopic image.