# US 2021/0262089 A1 · Transparent Nanowire Architectures For Marine Anti-Fouling

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0262089 A1
- Document ID: US20210262089A1
- Status: Published application
- Kind: A1
- Application number: 17/182,791
- Filed: 2021-02-23
- Published: 2021-08-26
- Earliest claimed: 2020-02-25
- Assignees: The Regents of the University of Michigan
- Applicants: The Regents of the University of Michigan
- Inventors: Neil P. DASGUPTA; Jing WANG; Anish TUTEJA
- Web page: https://patentgrep.com/patent/US20210262089A1

## CPC

- C23C 16/45534: {Use of auxiliary reactants other than used for contributing to the composition of the main film, e.g. catalysts, activators or scavengers}
- B05D 1/60: {Deposition of organic layers from vapour phase (vapour phase deposition in general C23C14/00, C23C16/00)}
- B05D 5/08: to obtain an anti-friction or anti-adhesive surface (rendering particulate materials free-flowing in general, e.g. making them hydrophobic B01J2/30)
- B63B 59/04: Preventing hull fouling (anti-fouling paints C09D5/16)
- C03C 17/3417: {all coatings being oxide coatings}
- C23C 16/403: {of aluminium, magnesium or beryllium}
- C23C 16/405: {of refractory metals or yttrium}
- C23C 16/407: {of zinc, germanium, cadmium, indium, tin, thallium or bismuth}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/45555: {applied in non-semiconductor technology}
- C23C 16/56: After-treatment
- C23C 28/02: only coatings {only including layers} of metallic material
- B05D 3/067: {Curing or cross-linking the coating}
- B05D 3/142: {Pretreatment}
- B05D 7/54: {No clear coat specified}
- B05D 7/58: {No clear coat specified}
- B05D 2518/12: Ceramic precursors (polysiloxanes, polysilazanes)
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 35/00: Methods or apparatus for measurement or analysis of nanostructures
- B82Y 40/00: Manufacture or treatment of nanostructures
- C03C 2217/425: consisting of a porous layer
- C03C 2217/76: Hydrophobic and oleophobic coatings
- C03C 2217/944: Layers comprising zinc oxide
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- B63B: SHIPS OR OTHER WATERBORNE VESSELS; EQUIPMENT FOR SHIPPING (arrangements of vessel ventilation, heating, cooling, or air-conditioning B63J2/00; floating substructures as supports of dredgers or soil-shifting machines E02F9/06)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A rational design and fabrication of ZnO/Al2O3 core-shell nanowire architectures with tunable geometries (length, spacing, branching) and surface chemistry is provided. The fabricated nanowires significantly delay or even prevent marine biofouling. In some embodiments, hydrophilic nanowires can reduce the fouling coverage by up to approximately 60% after 20 days compared to planar control surfaces. The mechanism of the fouling reduction is mainly due to two geometric effects: reduced effective settlement area and mechanical cell penetration. Further, superhydrophobic nanowires can completely prevent marine algal fouling for up to 22 days. Additionally, the developed nanowire surfaces are transparent across the visible spectrum, making them applicable to windows and oceanographic sensors.

## Claims

### Claim 1

A method of forming a transparent nanowire architecture for marine anti-fouling, the method comprising:
forming a ZnO layer upon a substrate via atomic layer deposition using a precursor and an oxidizer;
hydrothermal growing of a plurality of nanowires upon the ZnO layer; and
forming a core-shell layer via atomic layer deposition.

### Claim 2 (depends on 1)

The method according to claim 1 wherein the forming a core-shell layer via atomic layer deposition comprises forming an Al2O3 layer via atomic layer deposition using a precursor and an oxidizer at a predetermined temperature.

### Claim 3 (depends on 2)

The method according to claim 2 wherein the precursor is Trimethylaluminum.

### Claim 4 (depends on 2)

The method according to claim 2 wherein the precursor is Dimethylammonium iodide.

### Claim 5 (depends on 2)

The method according to claim 2 wherein the oxidizer is water.

### Claim 6 (depends on 2)

The method according to claim 2 wherein the predetermined temperature is in the range of 60° C. to 220° C.

### Claim 7 (depends on 2)

The method according to claim 2 wherein the predetermined temperature is about 150° C.

### Claim 8 (depends on 2)

The method according to claim 2 further comprising silanizing the plurality of nanowires using heptadecafluoro-1,1,2,2-tetrahydrodecyltrichlorosilane (F-17) to achieve superhydrophobicity.

### Claim 9 (depends on 8)

The method according to claim 8 wherein the silanization comprises cleaning the plurality of nanowires in oxygen plasma and maintaining in a silane vapor environment at a predetermined temperature and time.

### Claim 10 (depends on 9)

The method according to claim 9 wherein the predetermined temperature and time are 120° C. and more than 3 hours respectively.

### Claim 11 (depends on 8)

The method according to claim 8 further comprising rising the plurality of nanowires with toluene to remove unbonded silane.

### Claim 12 (depends on 1)

The method according to claim 1 wherein the forming a core-shell layer via atomic layer deposition comprises forming an anatase TiO2 layer via atomic layer deposition using a precursor and an oxidizer at a predetermined temperature.

### Claim 13 (depends on 12)

The method according to claim 12 wherein the precursor is Tetrakis(dimethylamido)titanium.

### Claim 14 (depends on 12)

The method according to claim 12 wherein the oxidizer is water.

### Claim 15 (depends on 12)

The method according to claim 12 wherein the predetermined temperature is about 130° C. to 250° C., typically about 180° C.

### Claim 16 (depends on 12)

The method according to claim 12 wherein the predetermined temperature is about 180° C.

### Claim 17 (depends on 12)

The method according to claim 12 further comprising post annealing the anatase TiO2 layer at 350° C. for 4 hours.

### Claim 18 (depends on 12)

The method according to claim 12 further comprising functionalizing the TiO2 layer using silicone oil (polydimethylsiloxane) with viscosity ranging from 5 cSt to 100,000 cSt and polydimethylsiloxane with functional groups, and UV exposure.

### Claim 19 (depends on 18)

The method according to claim 18 wherein the polydimethylsiloxane with functional groups is chosen from the group consisting of hydroxy terminated polydimethylsiloxane and vinyl terminated polydimethylsiloxane.

### Claim 20 (depends on 12)

The method according to claim 12 further comprising functionalizing the TiO2 layer using silicone oil with viscosity ranging from 5 cSt to 100,000 cSt.