# US 2021/0262078 A1 · Monolayer-By-Monolayer Growth of MgO Layers Using Mg Sublimation and Oxidation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0262078 A1
- Document ID: US20210262078A1
- Status: Published application
- Kind: A1
- Application number: 17/316,202
- Filed: 2021-05-10
- Published: 2021-08-26
- Earliest claimed: 2018-10-16
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Sahil Patel; Guenole Jan; Yu-Jen Wang
- Web page: https://patentgrep.com/patent/US20210262078A1

## CPC

- C23C 14/0042: {Controlling partial pressure or flow rate of reactive or inert gases with feedback of measurements}
- C23C 14/165: {by cathodic sputtering}
- C23C 14/0073: {by exposing the substrates to reactive gases intermittently}
- C23C 14/081: {of aluminium, magnesium or beryllium}
- C23C 14/185: {by cathodic sputtering}
- C23C 14/5806: {Thermal treatment}
- C23C 14/5853: {Oxidation}
- C23C 14/5873: {Removal of material}
- H01F 41/307: {insulating or semiconductive spacer}
- H10N 50/01: Manufacture or treatment
- H10N 50/10: Magnetoresistive devices
- H10N 50/85: Materials of the active region
- C01F 5/04: by oxidation of metallic magnesium
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})

## Abstract

A MgO layer is formed using a process flow wherein a Mg layer is deposited at a temperature <200° C. on a substrate, and then an anneal between 200° C. and 900° C., and preferably from 200° C. and 400° C., is performed so that a Mg vapor pressure >10−6 Torr is reached and a substantial portion of the Mg layer sublimes and leaves a Mg monolayer. After an oxidation between −223° C. and 900° C., a MgO monolayer is produced where the Mg:O ratio is exactly 1:1 thereby avoiding underoxidized or overoxidized states associated with film defects. The process flow may be repeated one or more times to yield a desired thickness and resistance×area value when the MgO is a tunnel barrier or Hk enhancing layer. Moreover, a doping element (M) may be added during Mg deposition to modify the conductivity and band structure in the resulting MgMO layer.

## Claims

### Claim 1

A method comprising:
forming a first Mg monolayer by performing a first anneal at a first temperature on a first Mg layer; and
performing a first oxidation on the first Mg monolayer at a second temperature thereby forming a first MgO monolayer.

### Claim 2 (depends on 1)

The method of claim 1, wherein all Mg atoms in the first MgO monolayer are oxidized.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first MgO monolayer is a tunnel barrier layer in a magnetic tunnel junction device.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first MgO monolayer is an Hk enhancing layer in a magnetic tunnel junction device.

### Claim 5 (depends on 1)

The method of claim 1, wherein the performing of the first anneal at the first temperature on the first Mg layer results in a Mg vapor pressure of at least 10−6 Torr.

### Claim 6 (depends on 1)

The method of claim 1, further comprising:
forming a reference layer, and
forming the first Mg layer on the reference layer.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
forming a second Mg monolayer on the first MgO monolayer; and
performing a second oxidation on the second Mg monolayer thereby forming a second MgO monolayer.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first temperature ranges from about 200° C. to about 900° C., and
wherein the second temperature from about −223° C. to about 900° C.

### Claim 9

A method comprising:
forming a first doped Mg-containing layer;
treating the first doped Mg-containing layer to form a first doped Mg-containing monolayer; and
oxidizing the first doped Mg-containing monolayer to form a first oxidized doped Mg-containing monolayer.

### Claim 10 (depends on 9)

The method of claim 9, wherein the treating of the first doped Mg-containing layer to form the first doped Mg-containing monolayer includes performing an anneal process at a temperature ranging from about 200° C. to about 900° C.

### Claim 11 (depends on 9)

The method of claim 9, wherein the first doped Mg-containing layer includes a dopant selected from the group consisting of Ti, V, Cr, Mn, Fe, Ga, In, Al, Si, Ge, Sn, Zr, Mo, Nb, Hf, Ta, W and N.

### Claim 12 (depends on 9)

The method of claim 9, further comprising:
forming a second doped Mg-containing layer on the first oxidized doped Mg-containing monolayer;
treating the second doped Mg-containing layer to form a second doped Mg-containing monolayer; and
oxidizing the second doped Mg-containing monolayer to form a second oxidized doped Mg-containing monolayer.

### Claim 13 (depends on 12)

The method of claim 12, further comprising:
forming a free layer on the second oxidized doped Mg-containing monolayer; and
forming an Hk enhancing layer on the free layer.

### Claim 14 (depends on 12)

The method of claim 12, further comprising forming a reference layer on the second oxidized doped Mg-containing monolayer.

### Claim 15 (depends on 9)

The method of claim 9, wherein the treating of the first doped Mg-containing layer to form the first doped Mg-containing monolayer includes performing a first anneal process at a first temperature, and
wherein the oxidizing of the first doped Mg-containing monolayer to form the first oxidized doped Mg-containing monolayer includes performing a second anneal process at a second temperature that is different than the first temperature.

### Claim 16

A method of forming a magnetic tunnel junction device, the method comprising:
forming a first metal layer on a substrate;
performing an evaporation process on the first metal layer to remove a portion of metal atoms to thereby form a metal monolayer; and
oxidizing the metal monolayer to form an oxidized monolayer, wherein all metal atoms in the oxidized monolayer are oxidized.

### Claim 17 (depends on 16)

The method of claim 16, wherein the first metal layer includes Mg atoms.

### Claim 18 (depends on 16)

The method of claim 16, wherein the performing of the evaporation process occurs at a first temperature, and
wherein the oxidizing of the metal monolayer occurs at a second temperature that is different than the first temperature.

### Claim 19 (depends on 16)

The method of claim 16, wherein the first metal layer includes a dopant having a higher melting point than the metal atoms of the metal layer.

### Claim 20 (depends on 19)

The method of claim 19, wherein the dopant is selected from the group consisting of Ti, V, Cr, Mn, Fe, Ga, In, Al, Si, Ge, Sn, Zr, Mo, Nb, Hf, Ta, W and N, and
wherein the monolayer and the oxidized monolayer include the doping element.