# US 2021/0262076 A1 · Graphene copper pantograph pan material for high-speed trains and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0262076 A1
- Document ID: US20210262076A1
- Status: Published application
- Kind: A1
- Application number: 17/055,920
- Filed: 2019-06-24
- Published: 2021-08-26
- Earliest claimed: 2019-06-24
- Assignees: Northeastern University
- Applicants: Northeastern University
- Inventors: Lianwei YANG; Ruijie WANG
- Web page: https://patentgrep.com/patent/US20210262076A1

## CPC

- C22C 26/00: Alloys containing diamond {or cubic or wurtzitic boron nitride, fullerenes or carbon nanotubes}
- B22F 1/0547: {Nanofibres or nanotubes}
- B22F 3/14: simultaneously
- B22F 3/15: Hot isostatic pressing
- B22F 5/00: Manufacture of workpieces or articles from metallic powder characterised by the special shape of the product
- B22F 5/006: {of flat products, e.g. sheets (B22F3/1103 takes precedence; by using pressure rollers only see B22F3/18)}
- B60L 5/20: Details of contact bow
- B60L 5/205: {with carbon contact members}
- B60L 5/24: Pantographs
- C22C 32/0084: {carbon or graphite as the main non-metallic constituent}
- C22C 47/14: by powder metallurgy, i.e. by processing mixtures of metal powder and fibres or filaments
- C22C 49/02: characterised by the matrix material
- C22C 49/14: characterised by the fibres or filaments
- B22F 2998/10: Processes characterised by the sequence of their steps
- C22C 2026/002: {Carbon nanotubes}
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B60L: PROPULSION OF ELECTRICALLY-PROPELLED VEHICLES (arrangements or mounting of electrical propulsion units or of plural diverse prime-movers for mutual or common propulsion in vehicles B60K1/00, B60K6/20; arrangements or mounting of electrical gearing in vehicles B60K17/12, B60K17/14; preventing wheel slip by reducing power in rail vehicles B61C15/08; dynamo-electric machines H02K; control or regulation of electric motors H02P); SUPPLYING ELECTRIC POWER FOR AUXILIARY EQUIPMENT OF ELECTRICALLY-PROPELLED VEHICLES (electric coupling devices combined with mechanical couplings of vehicles B60D1/64; electric heating for vehicles B60H1/00); ELECTRODYNAMIC BRAKE SYSTEMS FOR VEHICLES IN GENERAL (control or regulation of electric motors H02P); MAGNETIC SUSPENSION OR LEVITATION FOR VEHICLES; MONITORING OPERATING VARIABLES OF ELECTRICALLY-PROPELLED VEHICLES; ELECTRIC SAFETY DEVICES FOR ELECTRICALLY-PROPELLED VEHICLES

## Abstract

The present invention provides a graphene copper pantograph pan material for high-speed trains and a preparation method thereof, and the pan uses graphene as a reinforcing material, copper and iron as base materials, coke powder and graphite fiber as self-lubricating wear-resistant materials, and titanium, tungsten and molybdenum as additives. After being uniformly mixed, all the components are directly formed by hot pressing. The pantograph pan prepared by the present invention has the advantages of favorable electrical conductivity, wear resistance, impact resistance, ablation resistance and the like, and has little wear to overhead lines. The pan not only has simple preparation process, but also has much better performance than the conventional carbon pans and metal impregnated pans. The pan material is not only suitable for pantograph pans for high-speed trains such as high-speed rails and bullet trains, but also suitable for electric contact materials for low-speed trains such as subways.

## Claims

### Claim 1

A method for preparing a graphene copper pantograph pan material for high-speed trains, wherein the method comprises the following steps:
(1) first, uniformly dispersing graphene, additive and carbon nanotube in a polyvinyl alcohol solution with the concentration of 8.5% according to the mass ratio of the components of the graphene copper pantograph pan material, wherein the mass ratio of graphene to polyvinyl alcohol is 1:10, then adding copper powder, iron powder, coke and graphite fiber to the mixed solution in sequence, and stirring uniformly;
the graphene copper pantograph pan material comprises the following components by mass ratio: wherein 2.0-11.0 wt % of graphene, 30.5-60.5 wt % of copper powder, 1.0-19.0 wt % of iron powder, 8.0-37.0 wt % of coke, 1.0-5.0 wt % of carbon nanotube, 0.4-6.2 wt % of graphite fiber and 0.06-0.25 wt % of additive; the additive is formed by mixing titanium powder of 600-800 meshes, tungsten powder of 800-1200 meshes and molybdenum powder of 900-1200 meshes, and the mass ration of titanium powder to tungsten powder to molybdenum powder is 1:3:5;
(2) drying the mixed solution prepared in step (1) in vacuum, wherein the drying temperature is 30° C.-50° C.;
(3) taking out the dried material and placing in the sample hot-pressing groove of a hot press for direct vacuum hot pressing, wherein the pressure intensity for hot pressing is 40-120 MPa, the temperature is 850° C.-1200° C., and the holding time is 8-20 min, thus obtaining a graphene copper pantograph pan material.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The method for preparing the graphene copper pantograph pan material for high-speed trains according to claim 1, wherein the particle size of the copper powder used is 400-600 meshes, and the particle size of the iron powder is 900-1200 meshes.

### Claim 4 (depends on 1)

The method for preparing the graphene copper pantograph pan material for high-speed trains according to claim 1, wherein the carbon nanotube used is single-wall or multi-wall, with the diameter of 2-10 nm and the length of 0.5-8 μm.

### Claim 5 (depends on 1)

The method for preparing the graphene copper pantograph pan material for high-speed trains according to claim 1, wherein the particle size of the coke used is 100-400 meshes, and the graphite fiber is high-strength fiber, with the diameter of 4-8 μm and the length of 0.5-3 cm.

### Claim 6

(canceled)