# US 2021/0242305 A1 · Semiconductor Device and Manufacturing Method Therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0242305 A1
- Document ID: US20210242305A1
- Status: Published application
- Kind: A1
- Application number: 17/265,565
- Filed: 2019-08-09
- Published: 2021-08-05
- Earliest claimed: 2018-08-10
- Assignees: Csmc Technologies Fab2 Co., Ltd.
- Applicants: Csmc Technologies Fab2 Co., Ltd.
- Inventors: Huajun Jin; Guipeng Sun
- Web page: https://patentgrep.com/patent/US20210242305A1

## CPC

- H10D 62/109: {Reduced surface field [RESURF] PN junction structures}
- H10D 30/0281: {of lateral DMOS [LDMOS] FETs}
- H10D 30/0285: {using formation of insulating sidewall spacers}
- H10D 30/65: Lateral DMOS [LDMOS] FETs
- H10D 62/126: {Top-view geometrical layouts of the regions or the junctions}
- H10D 62/152: {Source regions of DMOS transistors}
- H10D 62/393: {Body regions of DMOS transistors or IGBTs (cell layout of DMOS H10D62/127)}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/21: {of electrically active species}
- H10P 30/22: using masks
- H10P 32/1406: {by ion implantation}
- H10P 32/171: {being group IV material}
- H10D 62/127: {of cellular field-effect devices, e.g. multicellular DMOS transistors or IGBTs}
- H10D 64/516: {the thicknesses being non-uniform}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device comprises: a substrate; a well region provided in the substrate, having a second conductivity type; source regions having a first conductivity type; body tile regions having the second conductivity type, the source regions and the body tie regions being alternately arranged in a conductive channel width direction so as to form a first region extending along the conductive channel width direction, and a boundary where the edges of the source regions and the edges of the body tie regions are alternately arranged being formed on two sides of the first region; and a conductive auxiliary region having the first conductivity type, provided on at least one side of the first region, and directly contacting the boundary, a contact part comprising the edge of at least one source region on the boundary and the edge of at least one body tie region on the boundary.

## Claims

### Claim at position 1

1-7. (canceled)

### Claim 8

A method for manufacturing a semiconductor device, comprising:
forming a well region implantation window on a substrate by photoetching; implanting ions of a first conductivity type and ions of a second conductivity type into the substrate through the well region implantation window, wherein the first conductivity type is opposite to the second conductivity type;
performing a thermal diffusion such that the implanted ions of the second conductivity type forms a well region, and the implanted ions of the first conductivity type forms a second region; and
forming a source region and a body lead-out region in the well region, wherein the source regions and the body lead-out regions are alternately arranged in a width direction of a conductive channel, so as to form a first region extending along the width direction of the conductive channel, both sides of the first region are boundaries formed by alternately arranging edges of the source regions and edges of the body lead-out regions, the first region overlaps a part of the second region, a portion of the second region located outside the first region is used as a conductive auxiliary region, a portion of the conductive auxiliary region in direct contact with the boundary comprises at least one edge of the source region on the boundary and at least one edge of the body lead-out region on the boundary.

### Claim 9 (depends on 8)

The method according to claim 8, wherein in the step of implanting ions of the first conductivity type into the substrate through the well region implantation window, an implantation energy is between 15 keV to 50 keV.

### Claim 10 (depends on 8)

The method according to claim 8, wherein in the step of implanting ions of the first conductivity type into the substrate through the well region implantation window, the implanted ions are arsenic ions.

### Claim 11 (depends on 8)

The method according to claim 8, wherein prior to the step of forming the well region implantation window on the substrate by photoetching, the method further comprises a step of forming a polysilicon layer on the substrate and etching the polysilicon layer to form a polysilicon gate.

### Claim 12 (depends on 11)

The method according to claim 11, wherein prior to the step of forming the polysilicon layer on the substrate and etching the polysilicon layer to form the polysilicon gate, the method further comprises a step of forming an insulating layer on the substrate, a part of the remaining polysilicon after completing the etching is located on the insulating layer, and a part of the remaining polysilicon extends beyond an edge on a side of the insulating layer to the substrate;
wherein the step of forming the source region and the body lead-out region in the well region comprises performing photoetching using a first photolithography mask to form an ion implantation window of the first conductivity type, and then implanting the ions of the first conductivity type into the substrate through the ion implantation window of the first conductivity type, wherein the first photolithography mask comprises a first implantation region and a second implantation region that are separated from each other, the first implantation region and the second implantation region are light-transmitting regions, the first photolithography mask further comprises a light shielding region located between the first implantation region and the second implantation region, the first implantation region is configured to form the source region, and the second implantation region is configured to form a drain region.

### Claim 13 (depends on 11)

The method according to claim 11, further comprising a step of diffusing the conductive auxiliary region along a length direction of the conductive channel by the thermal diffusion, until the conductive auxiliary region is below the polysilicon gate.

### Claim 14 (depends on 12)

The method according to claim 12, wherein in the step of performing the photoetching using the first photolithography mask, an applied photoresist forms a step above an edge on a side of the insulating layer, the light shielding region is configured to prevent exposure light from radiating the step during photolithography exposure.

### Claim 15 (depends on 12)