# US 2021/0242022 A1 · A method for selective incorporation of dopant atoms in a semiconductive surface

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0242022 A1
- Document ID: US20210242022A1
- Status: Published application
- Kind: A1
- Application number: 17/051,739
- Filed: 2019-05-02
- Published: 2021-08-05
- Earliest claimed: 2018-05-02
- Assignees: NewSouth Innovations Pty Limited
- Applicants: NewSouth Innovations Pty Ltd
- Inventors: Michelle SIMMONS; Joris KEIZER
- Web page: https://patentgrep.com/patent/US20210242022A1

## CPC

- H10D 30/014: {of FETs having zero-dimensional [0D] or one-dimensional [1D] channels, e.g. quantum wire FETs, single-electron transistors [SET] or Coulomb blockade transistors}
- H10P 32/12: between a solid phase and a gaseous phase
- H10D 48/3835: {Semiconductor qubit devices comprising a plurality of quantum mechanically interacting semiconductor quantum dots, e.g. Loss-DiVincenzo spin qubits}
- H10P 32/1204: {from a plasma phase}
- H10P 32/1404: {using predeposition followed by drive-in of impurities into the semiconductor surface, e.g. predeposition from a gaseous phase}
- H10P 32/171: {being group IV material}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- G01Q 80/00: Applications, other than SPM, of scanning-probe techniques (manufacture or treatment of nanostructures B82B3/00; recording or reproducing information using near-field interaction G11B9/12, G11B11/24, G11B13/08)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- G01Q: SCANNING-PROBE TECHNIQUES OR APPARATUS; APPLICATIONS OF SCANNING-PROBE TECHNIQUES, e.g. SCANNING PROBE MICROSCOPY [SPM]

## Abstract

The present disclosure is directed to a methodology for embedding a deterministic number of dopant atoms in a surface portion of a group IV semiconductor lattice. The methodology comprises the steps of: forming one or more lithographic sites on the surface portion; dosing, at a temperature below 100 K, the surface portion using a gas with molecules comprising the dopant atom and hydrogen atoms in a manner such that, a portion of the molecules bonds to the surface portion; and incorporating one or more dopant atoms in a respective lithographic site by transferring an amount of energy to the dopant atoms. The number of dopant atoms incorporated in a lithographic site is deterministic and related to the size of the lithographic site.

## Claims

### Claim 1

A method for embedding a deterministic number of dopant atoms in a surface portion of a group IV semiconductor lattice, the method comprising the steps of:
a) forming one or more lithographic sites on the surface portion;
b) dosing, at a temperature below 100 K, the surface portion using a gas with molecules comprising the dopant atom and hydrogen atoms in a manner such that, a portion of the molecules bonds to the surface portion; and
c) incorporating one or more dopant atoms in a respective lithographic site by transferring an amount of energy to the dopant atoms;
wherein the number of dopant atoms incorporated in a lithographic site is deterministic and related to the size of the lithographic site.

### Claim 2 (depends on 1)

The method of claim 1, wherein the surface portion of a group IV semiconductor lattice is a pure crystalline silicon portion or pure crystalline germanium portion.

### Claim 3 (depends on 1)

The method of claim 1, wherein, during incorporating, atoms that are not incorporated in a respective lithographic site are released from the surface portion.

### Claim 4 (depends on 1)

The method of claim 1, wherein the molecules in the dosing gas contain phosphine (PH3) and the dosing process is performed in a manner such that the surface portion is saturated with PH3 molecules.

### Claim 5 (depends on 1)

The method of claim 1, wherein the dosing process is performed in a manner such that only PH3 molecules are absorbed and bond with the surface portion at the lithographic sites.

### Claim 6 (depends on 1)

The method of claim 1, wherein the dosing process is performed at a temperature such that dissociation of PH3 into PH2 is prevented, wherein the dosing process is performed at a temperature below 40K, or at a temperature between 40K and 100K, or at a temperature of 77K.

### Claim 7

(canceled)

### Claim 8 (depends on 1)

The method of claim 1, wherein the dosing process is performed at a temperature such that dissociation of PH3 into PH2 occurs spontaneously.

### Claim 9

(canceled)

### Claim 10

(canceled)

### Claim 11 (depends on 1)

The method of claim 1, wherein the one or more lithographic sites are: 1 by 1 silicon atomic sites, 2 by 1 silicon dimer patches, 3 by 1 silicon dimer patches, 4 by 1 silicon dimer patches, or 5 by 1 silicon dimer patches.

### Claim 13 (depends on 1)

The method of claim 1, wherein the one or more lithographic sites are 3 by 1 silicon dimer patches and the step of incorporating one or more dopant atoms in a respective lithographic site comprises the step of annealing the surface portion in a manner such that single dopant atoms from a first portion of the bonded molecules are incorporated in respective lithographic sites in the surface portion; and a second portion of the bonded molecules is released from the surface portion, wherein each dimer patch bonds with six PH2 molecules.

### Claim 14

(canceled)

### Claim 15 (depends on 12)

The method of claim 12, wherein during the step of annealing the bonded PH3 molecules lose one hydrogen atom, or wherein during the step of annealing, PH2 molecules bond with an additional hydrogen atom and are released from the surface portion.

### Claim 16

(canceled)

### Claim 17 (depends on 12)

The method of claim 12, wherein the step of annealing the surface portion is performed in two phases:
i. a first phase during which the bonded PH3 molecules lose one hydrogen atom to form a plurality of PH2 molecules bonded to the surface, wherein the first annealing phase is performed by exposing the surface to room temperature;
ii. a second phase during which the bonded PH2 molecules lose their two hydrogen atoms to other PH2 molecules and a single P atom is embedded in a single 3 by 1 silicon dimer patch, wherein the second annealing phase is performed between 200° C. and 400° C.

### Claim 18

(canceled)

### Claim 19

(canceled)

### Claim 20 (depends on 1)

The method of claim 1, wherein the step of incorporating one or more dopant atoms in a respective lithographic site comprises the step of positioning a tip of a scanning tunnelling microscope above one of the molecules and transferring an amount of energy to the dopant atoms through the tip.

### Claim 21 (depends on 19)

The method of claim 19, wherein the step of transferring an amount of energy to the dopant atoms comprises applying a current to the dopant atoms and the semiconductor surface through the tip while the tip is positioned in proximity of the dopant atom, wherein in order to apply the current through the tip, a feedback control loop of the scanning tunnelling microscope is deactivated and, to increase the magnitude of the current, the tip is controlled to move closer to the dopant atom.

### Claim 22

(canceled)

### Claim 23 (depends on 20)

The method of claim 20, further comprising monitoring the magnitude of the applied current for sharp variations triggered by incorporation of a dopant atom.

### Claim 24 (depends on 20)

The method of claim 20, wherein the magnitude of the current is between 0.1 nA and 10 nA.

### Claim 25 (depends on 20)

The method of claim 20, further comprising applying a voltage between the tip and the semiconductor surface, the voltage having a magnitude between 2V and 4V.

### Claim 26 (depends on 19)

The method of claim 19, wherein the step of transferring an amount of energy to the dopant atoms comprises applying a voltage or current to the dopant atoms and the semiconductor surface through the tip while the feedback control loop of the scanning tunnelling microscope is active.

### Claim 27 (depends on 25)

The method of claim 25, comprising increasing the magnitude of the current and monitoring the distance between the tip and the dopant atom for sharp variations triggered by incorporation of a dopant atom.

### Claim 28 (depends on 26)

The method of claim 26, wherein the step of transferring an amount of energy to the dopant atoms comprises applying a voltage pulse with a duration between 0.1 s and is and a magnitude between 2V and 4V, or wherein the step of transferring an amount of energy to the dopant atoms comprises applying a current pulse with a duration between 0.1 s and is and a magnitude between 0.1 nA and 1 nA.

### Claim 29

(canceled)

### Claim 30 (depends on 25)

The method of claim 25, wherein the distance between the tip and the atom is between 0.1 nm and 10 nm.