# US 2021/0241948 A1 · Rare-earth cobalt permanent magnet, manufacturing method therefor, and device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0241948 A1
- Document ID: US20210241948A1
- Status: Published application
- Kind: A1
- Application number: 17/146,269
- Filed: 2021-01-11
- Published: 2021-08-05
- Earliest claimed: 2020-01-31
- Assignees: Tokin Corporation
- Applicants: TOKIN Corporation
- Inventors: Hirokazu MAKUTA; Hiroaki MACHIDA; Teruhiko FUJIWARA; Yu KANAMORI
- Web page: https://patentgrep.com/patent/US20210241948A1

## CPC

- H01F 1/0557: {sintered}
- H01F 41/0266: {Moulding; Pressing (H01F41/0273 takes precedence; hard magnetic particles H01F1/06, H01F1/11)}
- H01F 7/021: {Construction of PM (H01F7/0278 takes precedence; PM compositions H01F1/032)}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

A rare-earth cobalt permanent magnet having excellent magnetic characteristics, a method for manufacturing such a rare-earth cobalt permanent magnet, and a device are provided. A rare-earth cobalt permanent magnet consists of, when a rear-earth element including at least Sm is represented by R, 23 to 27 mass % of R, 1.0 to 5.0 mass % of Cu, 18 to 25 mass % of Fe, 1.5 to 3.0 mass % of Zr, and a remainder consisting of Co and unavoidable impurities, in which the rare-earth cobalt permanent magnet includes a plurality of crystal grains and grain boundary parts, and a concentration of Cu is at least two times a concentration of Zr in the grain boundary parts.

## Claims

### Claim 1

A rare-earth cobalt permanent magnet consisting of, when a rear-earth element including at least Sm is represented by R, 23 to 27 mass % of R, 1.0 to 5.0 mass % of Cu, 18 to 25 mass % of Fe, 1.5 to 3.0 mass % of Zr, and a remainder consisting of Co and unavoidable impurities, in which
the rare-earth cobalt permanent magnet includes a plurality of crystal grains and grain boundary parts, and
a concentration of Cu is at least two times a concentration of Zr in the grain boundary parts.

### Claim 2 (depends on 1)

The rare-earth cobalt permanent magnet according to claim 1, wherein a size of a cell structure constituting a crystal grain is 50 to 200 nm.

### Claim 3 (depends on 1)

The rare-earth cobalt permanent magnet according to claim 1, wherein a saturation magnetization is equal to or larger than 1.16 T and an intrinsic coercive force Hcj is 120 to 800 kA/m.

### Claim 4 (depends on 1)

The rare-earth cobalt permanent magnet according to claim 1, wherein saturation magnetization is equal to or larger than 1.16 T and an intrinsic coercive force Hcj is 240 to 800 kA/m.

### Claim 5 (depends on 1)

The rare-earth cobalt permanent magnet according to claim 1, wherein a squareness ratio expressed as a ratio (Hk/Hcj) between a magnetic field Hk at 90% of residual magnetization and an intrinsic coercive force Hcj is equal to or higher than 60% in a demagnetization curve, and
when the rare-earth cobalt permanent magnet is re-magnetized from a demagnetizing field exceeding a knickpoint in the demagnetization curve, magnetization equal to or higher than 95% of the saturation magnetization is obtained in a magnetic field equal to or weaker than five times the intrinsic coercive force Hcj.

### Claim 6 (depends on 1)

The rare-earth cobalt permanent magnet according to claim 1, wherein a squareness ratio expressed as a ratio (Hk/Hcj) between a magnetic field Hk at 90% of residual magnetization and an intrinsic coercive force Hcj is equal to or higher than 60% in a demagnetization curve, and
when the rare-earth cobalt permanent magnet is re-magnetized from a demagnetizing field exceeding a knickpoint in the demagnetization curve, magnetization equal to or higher than 95% of the saturation magnetization is obtained in a magnetic field equal to or weaker than three times the intrinsic coercive force Hcj.

### Claim 7 (depends on 1)

The rare-earth cobalt permanent magnet according to claim 1, wherein when a diffraction intensity I(006) of a plane and a diffraction intensity I of a plane are measured by a powder X-ray diffraction method, a diffraction intensity ratio I(006)/I (303) is 0.225 to 0.4.

### Claim 8

A method for manufacturing a rare-earth cobalt permanent magnet, comprising:
a step (I) of preparing an alloy consisting of, when a rear-earth element including at least Sm is represented by R, 23 to 27 mass % of R, 1.0 to 5.0 mass % of Cu, 18 to 25 mass % of Fe, 1.5 to 3.0 mass % of Zr, and a remainder consisting of Co and unavoidable impurities;
a pulverizing step (II) of pulverizing the alloy into a powder;
a pressure-molding step (III) of pressure-molding the powder into a molded body;
a step (IV) of sintering the molded body at 1,200 to 1,250° C.;
a step (V) of performing a solution treatment for a sintered molded body;
a step (VI) of heat-treating the molded body subjected to the solution treatment at 600 to 850° C.;
a step (VII) of cooling the molded body subjected to a heat treatment to 400° C. or lower at a rate of 0.2 to 10° C./min;
a step (VIII) of heat-treating the molded body at a temperature that is between 700 to 900° C. and higher than the temperature in the step (VI); and
a step (IX) of cooling the molded body subjected to the heat treatment to 400° C. or lower at a rate of 0.1 to 5° C./min.

### Claim 9

A method for manufacturing a rare-earth cobalt permanent magnet, comprising:
a step (I) of preparing an alloy consisting of, when a rear-earth element including at least Sm is represented by R, 23 to 27 mass % of R, 1.0 to 5.0 mass % of Cu, 18 to 25 mass % of Fe, 1.5 to 3.0 mass % of Zr, and a remainder consisting of Co and unavoidable impurities;
a pulverizing step (II) of pulverizing the alloy into a powder;
a pressure-molding step (III) of pressure-molding the powder into a molded body;
a step (IV) of sintering the molded body at 1,200 to 1,250° C.;
a step (V) of performing a solution treatment for the sintered molded body;
a step (VI) of heat-treating the molded body subjected to the solution treatment at 750 to 850° C.;
a step (VII) of cooling the molded body subjected to the heat treatment to 500 to 600° C. at a rate of 0.5 to 10° C./min, and then isothermally holding the molded body; and
a step (VIII) of rapidly cooling the molded body subjected to the isothermal holding.

### Claim 10 (depends on 1)

A device comprising a rare-earth cobalt permanent magnet according to claim 1.