# US 2021/0239456 A1 · Liquid layer thickness measurement method, measurement device, film production method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0239456 A1
- Document ID: US20210239456A1
- Status: Published application
- Kind: A1
- Application number: 17/054,826
- Filed: 2019-05-27
- Published: 2021-08-05
- Earliest claimed: 2018-05-31
- Assignees: Toray Industries, Inc.
- Applicants: Toray Industries, Inc.
- Inventors: Kenta Nakajima; Nobuhiro Naito
- Web page: https://patentgrep.com/patent/US20210239456A1

## CPC

- B29C 55/16: simultaneously
- G01B 11/06: for measuring thickness {; e.g. of sheet material (thickness measurement by thermal means G01B21/085)}
- B29C 55/20: Edge clamps
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- G01B: MEASURING LENGTH, THICKNESS OR SIMILAR LINEAR DIMENSIONS; MEASURING ANGLES; MEASURING AREAS; MEASURING IRREGULARITIES OF SURFACES OR CONTOURS

## Abstract

A method of measuring thickness of a liquid layer includes applying a light beam to a liquid layer disposed on a surface of a member, detecting reflected light by a sensor, and analyzing the reflected light according to a spectral interference method with a curve fitting technique to determine the thickness of the liquid layer.

## Claims

### Claim at position 1

1-10. (canceled)

### Claim 11

A method of measuring thickness of a liquid layer comprising applying a light beam to a liquid layer disposed on a surface of a member, detecting reflected light by a sensor, and analyzing the reflected light according to a spectral interference method with a curve fitting technique to determine the thickness of the liquid layer.

### Claim 12 (depends on 11)

The method as set forth in claim 11, wherein the liquid layer contains a metal component.

### Claim 13 (depends on 11)

The method as set forth in claim 11, wherein the liquid layer has a thickness of 11 μm or less.

### Claim 14 (depends on 11)

The method as set forth in claim 11, wherein the member has a surface roughness of 1.0 μm or more and 2.5 μm or less.

### Claim 15 (depends on 11)

The method as set forth in claim 11, wherein the member is a rail on which bearings travel.

### Claim 16 (depends on 15)

The method as set forth in claim 15, wherein the rail is a clip rail of a tenter apparatus on which clip devices travel.

### Claim 17 (depends on 11)

The method as set forth in claim 11, wherein the sensor is a portable type sensor.

### Claim 18 (depends on 11)

An apparatus that measures thickness of a liquid layer by the method as set forth in claim 11 comprising: at least a light exposure means that emits light toward a liquid layer disposed on the surface of a member, a reflected light detection means that detects the reflected light coming from the surface of the member and a surface of the liquid layer, an analysis means that measures the reflectance spectrum based on the detected reflected light, comparing, by the curve fitting technique, the measured reflectance spectrum with a plurality of theoretical reflectance spectra corresponding to different theoretical liquid layer thicknesses set up in advance, identifying the theoretical reflectance spectrum that most closely approximates the measured reflectance spectrum, and deciding on the theoretical liquid layer thickness corresponding thereto as measured liquid layer thickness.

### Claim 19 (depends on 11)

A method of producing a film comprising a step of stretching the film with a tenter apparatus having a mechanism in which bearings travel on rails, wherein a liquid layer satisfying Equation (1) is formed on a traveling path of the bearings on each rail wherein h is the thickness of the liquid layer measured by the method as described in claim 11, h1 (μm) being the surface roughness of the rail, and h2 (μm) being the surface roughness of the bearings:
2√{square root over (h12+h22)}≤h≤10√{square root over (h12+h22)} (1)

### Claim 20 (depends on 19)

The method as set forth in claim 19, wherein the thickness h (μm) of the liquid layer is controlled by Equation (1) by adjusting a rate of liquid feeding to the traveling path of the bearings.